Valeev R.A., Korolev D.V., Morgunov R.B., Piskorsky V.P. The effect of high concentrations of cobalt on the properties of magnets Pr–Dy–Fe–Co–B and Nd–Dy–Fe–Co–B // Proceedings of VIAM. 2022. No. 10 (116). Ст. 06. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2022-0-10-66-75.

The effect of high concentrations of cobalt on the properties of magnets Pr–Dy–Fe–Co–B and Nd–Dy–Fe–Co–B

Valeev R.A., Korolev D.V., Morgunov R.B., Piskorsky V.P.
Abstract

Analysis of the magnetic hysteresis loops of permanent magnets Pr–Dy–Fe–Co–B and Nd–Dy–Fe–Co–B with a high Co content allows us to conclude that with an increase in the cobalt content in the alloy, the coercive force HcI value decreases significantly. The replacement of Nd with Pr in the alloy composition leads to a decrease in the volume fraction of the main magnetic phase R2–(FeCo)14B in the composition of sintered permanent magnets, which proportionally affects the dependence of the HcI on the Co content in the permanent magnet material. This effect is presumably related to the difference in the diffusion rate in the materials under consideration.

Keywords
rare earth magnets, main magnetic phase, residual induction, coercive force, diffusion rate, rare earth metals
Reference list
  1. Rodewald W., Katter M., Uestuener K. Top Nd–Fe–B magnets: >56 MGOe, energy density, 9,8 kOe Coercitiviy. IEEE Transitions on Magnetics, 2002, vol. 38, pp. 2955–2957.
  2. Martynenko Yu.G. Trends in the development of modern gyroscopy. Sorosovskiy obrazovatelnyj zhurnal, 1997, no. 11, pp. 120–127.
  3. Topilskaya S.V., Borodulin D.S., Kornyukhin A.V. Experimental evaluation of allowable mechanical impacts on a dynamically adjustable gyroscope. Vestnik MGTU im. N.E. Baumana. Ser.: Priborostroyenie, 2018, no. 4, pp. 69–79. DOI: 10.18698/0236-3933-2018-4-69-79.
  4. Peshekhonov V.G. Prospects for the development of gyroscopy. Giroskopiya i navigatsiya, 2020, vol. 28, no. 2, pp. 3–10. DOI: 10.1785/0869-7035-0028.
  5. Morgunov R.B., Piskorskiy V.P., Valeev R.A., Korolev D.V. The thermal stability of rare-earth magnets supported by means of the magnetocaloric effect. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 88–94. DOI: 10.18577/2071-9140-2019-0-1-88-94.
  6. Piskorsky V.P., Valeev R.A., Korolev D.V., Morgunov R.B., Rezchikova I.I. Terbium and gadolinium dopin g influence on thermal stability and magnetic properties of sintered magnets Pr–Tb–Gd–Fe–Co–B. Trudy VIAM, 2019, no. 7 (79), paper no. 07. Available at: http://www.viam-works.ru (accessed: May 5, 2022). DOI: 10.18577/2307-6046-2019-0-7-59-66.
  7. Koplak O.V., Kunitsyna E.I., Valeev R.A., Korolev D.V., Piskorskii V.P., Morgunov R.B. Ferromagnetic microwires α-Fe/(PrDy)(FeCo)B for micromanipulators and polymer composites. Trudy VIAM, 2019, no. 11 (83), paper no. 7. Available at: http://www.viam-works.ru (accessed: May 5, 2022). DOI: 10.18577/2307-6046-2019-0-11-60-67.
  8. Morgunov R.B., Koplak O.V., Talantsev A.D., Korolev D.V., Piskorskij V.P., Valeev R.A. The phenomenology of the magnetic hysteresis loops in multilayer microwires α-Fe/DyPrFeCoB. Trudy VIAM, 2019, no. 7 (79), paper no. 08. Available at: http://www.viam-works.ru (accessed: May 5, 2022). DOI: 10.18577/2307-6046-2019-0-7-67-75.
  9. Haavisto M., Tuominen S., Santa-Nokki T. et al. Magnetic behavior of sintered NdFeB mag-nets on a long-term timescale. Advances in Materials Science and Engineering, 2014, art. ID 760584. DOI: 10.1155/2014/760584.
  10. Wang Y., Yu B., Feng M. et al. Magnetic properties оf Nd–Fe–Co–B permanent magnetic alloys. Journal of Applied Physics, 1987, vol. 61, pp. 3448–3450.
  11. Bolzoni F., Leccabue F., Moze O. et al. 3d and 4f magnetismin Nd2Fe14–xCoxB and Y2Fe14–xCoxB compounds. Journal of Applied Physics, 1987, vol. 61, no. 12, pp. 5369–5373.
  12. Niihara K., Shishido T., Yajima S. The crystal data of ternary rare earth borides RCo2B2. Bulletin of the chemical society of Japan, 1973, vol. 46, pp. 1137–1140.
  13. Belov K.P., Nikitin S.A., Savitsky E.M. Magnetic and Magnetostrictive Properties of Intermetallic Compounds of Rare Earth Metals with Iron Type RFe2 and RFe3. Rare Earth Metals, Alloys and Compounds. Moscow: Nauka, 1973, pp. 89–91.
  14. Herbst J.F. R2Fe14B materials: intrinsic properties and technological properties and technological aspects. Reviews of Modern Physics, 1991, vol. 63, no. 4, pp. 819–898.
  15. Kablov E.N., Petrakov A.F., Piskorsky V.P., Valeev R.A., Nazarova N.V. Influence of dysprosium and cobalt on the temperature dependence of magnetization and phase composition of the material of the Nd–Dy–Fe–Co–B system. Metallovedenie i termicheskaya obrabotka metallov, 2007, no. 4, pp. 3–10.
  16. Bala H., Szymura S., Sergeev V.V. et al. Properties of terbium-doped (Nd, Dy)–(Fe, Co)–B sintered magnets. Journal of Magnetism and Magnetic Materials, 1992, vol. 103, pp. 58–64.
  17. Deryagin A.V. Rare-earth magnetically hard materials. Uspekhi fizicheskikh nauk, 1976, vol. 120, is. 3, pp. 393–437.
  18. Szytula A. Magnetic properties of the RT2X2, RTX2 and RTX compounds in high magnetic field. Acta Physica Polonica A, 1994, vol. 85, no. 2, pp. 293–296.
  19. Faria R.N., Davies B.E., Brown D.N., Harris I.R. Microstructural and magnetic studies of cast and annealed Nd and PrFeCoBZr alloys and HDDR materials. Journal of Alloys and Compounds, 2000, vol. 296, pp. 223–228.
  20. Bolzoni F., Coey J.M., Gavigan J. et al. Magnetic properties of Pr2(Fe1–xCox)14B compounds. Journal of Magnetism and Magnetic Materials, 1987, vol. 65, pp. 123–127.