Kulagina G.S., Zhelezina G.F., Shuldeshova P.M., Kurshev E.V. Structure and physical-mechanical properties of a new generation organoplastic based on Rusar-NT brand aramid fiber fabric and melt binder // Proceedings of VIAM. 2022. No. 10 (116). Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2022-0-10-55-65.

Structure and physical-mechanical properties of a new generation organoplastic based on Rusar-NT brand aramid fiber fabric and melt binder

Kulagina G.S., Zhelezina G.F., Shuldeshova P.M., Kurshev E.V.
Abstract

Considered and analyzes the microstructure of an organoplastic (organotextolite) based on an aramid fabric, made from a third-generation fiber of the Rusar-NT brand, and a melted epoxy binder modified with a thermoplastic – polysulfone. The physico-mechanical properties of organoplastics are determined. It has been established that the studied organoplastic in terms of its strength characteristics and water resistance surpasses its predecessors – organoplastics based on aramid fibers of the first and second generation.

Keywords
aramid fiber Rusar-NT, aramid fabric, melt binder, microstructure, physical and mechanical properties
Reference list
  1. Aviation materials: reference book in 13 vols. Ed. E.N. Kablov. 7th ed., add. and rev. Moscow: VIAM, 2015, vol. 7: Polymer composite materials, 209 p.
  2. Zhang S., Zhao D. Advances in materials science and engineering. Aerospace materials handbook. CRC Press. Taylor & Francis Group, 2012, 781 p.
  3. Singh A.K., Wanhill R.J.H., Prasad N.E. Lightweight ballistic armours for aero-vehicle protection. Aerospace materials and material technologies, 2017, vol. 2: Aerospace material technologies. pp. 541–567.
  4. Reference book on composite materials. Ed. J. Lubin. Moscow: Mashinostroitel, 1988, book 1, 448 p.
  5. Kablov E.N. Modern materials – the basis of innovative modernization of Russia. Metally Evrazii, 2012, no. 3, pp. 10–15.
  6. Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  7. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  8. Kolobkov A.S. Polymer composite materials for various aircraft structures (review). Trudy VIAM, 2020, no. 6–7 (89), paper no. 05. Available at: http://www.viam-works.ru (accessed: May 18, 2022). DOI: 10.18577/2307-6046-2020-0-67-38-44.
  9. Mikhailin Yu.A. Structural polymeric composite materials. 2nd ed. St. Petersburg: Nauchnye osnovy i tekhnologii, 2013, 822 p.
  10. Zhelezina G.F., Gulyaev I.N., Soloveva N.A. Aramide organic plastics of new generation for aviation designs. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 368–378. DOI: 10.18577/2071-9140-2017-0-S-368-378.
  11. Roberts G.D., Revilock D.M., Binienda W.K. et al. Impact Testing and Analysis of Composites for Aircraft Engine Fan Cases. Journal of Aerospace Engineering, 2002, no. 15, pp. 104–110.
  12. Zhelezina G.F., Solovieva N.A., Kulagina G.S., Shuldeshova P.M. Study of the possibility of increasing the impact resistance of thin-sheeted carbon fiber-reinforced plastics due to clading with aramid organoplastics. Aviation materials and technologies, 2021, no. 4 (65), paper no. 04. Available at: http://www.journal.viam.ru (accessed: May 18, 2022). DOI: 10.18577/2713-0193-2021-0-4-35-42.
  13. Laurens B.V. Development of a new hybrid material (ARALL) for aircraft structures. Industrial & Engineering Chemistry, 1983, no. 22 (3), pp. 492–496.
  14. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymeric composite materials. Ed. E.N. Kablov. Mosocow: NRC "Kurchatov Institute" – VIAM, 2021, 528 p.
  15. Petrova A.P., Mukhametov R.R., Shishimirov M.V., Pavlyuk B.Ph., Starostina I.V. Test methods and researches thermosetting binding for polymeric composite materials (review). Trudy VIAM, 2018, no. 12 (72), paper no. 07. Available at: http://viam-works.ru (accessed: May 11, 2022). DOI: 10.18577/2307-6046-2018-0-12-62-70.
  16. Zhelezina G.F., Voinov S.I., Chernykh T.E., Chernykh K.Yu. New aramid fibers Rusar-NT for reinforcing structural organoplastics. Voprosy materialovedeniya, 2015, no. 1 (81), pp. 60–70.
  17. Kablov E.N., Kulagina G.S., Zhelezina G.F., Lons-kii S.L., Kurshev E.V. Microstructure research of the unidirectional organoplastic based on Rusar-NT aramid fibers and epoxy-polysulfone binder. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 19–26. DOI: 10.18577/2071-9140-2020-0-4-19-26.
  18. Deev I.S., Kobets L.P. Study of the microstructure and microfields of deformations in polymer composites by scanning electron microscopy. Zavodskaya laboratory. Material diagnostics, 1999, vol. 65, no. 4, pp. 27–34.
  19. Deev I.S., Kablov E.N., Kobets L.P., Chursova L.V. Research of the scanning electron microscopy method deformation of microphase structure of polymeric matrix at mechanical loading. Trudy VIAM, 2014, no. 7, paper no. 06. Available at: http://www.viam-works.ru (accessed: May 22, 2022). DOI: 10.18577/2307-6046-2014-0-7-6-6.
  20. Pakhomov K.S., Antipov Yu.V., Chalykh A.E., Budylin N.Yu., Stoyanov O.V., Simonov-Emelyanov I.D. Energy parameters of the surface of aramid fibers. Vestnik tekhnologicheskogo universiteta, 2016, vol. 19, no. 1, pp. 100–103.
  21. Chalykh, A.E., Gerasimov, V.K., Bukhteev, A.E. et al. Compatibility and evolution of the phase structure of mixtures of polysulfone–curing epoxy oligomers, Vysokomolekulyarnye soyedineniya, Ser. A, 2003, vol. 45, no. 7, pp. 1148–1159.
  22. Budylin N.Yu., Shapagin A.V., Chalykh A.E. Comparative studies of mutual diffusion and phase states in mixtures of epoxy oligomers with polysulfones and polyethersulfones. Articles of XIX All-Rus. conf. "Structure and Dynamics of Molecular Systems". Moscow: IFCHE RAN, 2012, vol. 2, pp. 192–195.
  23. Min H.S., Kim S.Ch. Fracture toughness of polysulfone/epoxysemi-IPN with morphology spectrum. Polymer Bulletin, 2003, vol. 42, pp. 221–227.
  24. Woo E.M., Hseih H.K. Morphology development in epoxy/polymer systems: thermosetting epoxy micro particles with a thermoplastic shell. Polymer, 1998, vol. 39, no. 1, pp. 7–13.
  25. Kim B.S., Chiba T., Inoue T. Phase separation and apparent phase dissolution during cure process of thermoset/thermoplastic blend. Polymer, 1995, vol. 36, no. 1, pp. 67–71.
  26. Shapagin A.V. Structure formation in systems epoxy oligomers–thermoplastics: thesis, Cand. Sc. (Chem.). Moscow, 2004, 163 p.