Serpova V.M., Nyafkin A.N., Kurbatkina E.I. Hybrid metal matrix composites based on copper (review) // Proceedings of VIAM. 2022. No. 1 (107). Ст. 08. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2022-0-1-76-87.

Hybrid metal matrix composites based on copper (review)

Serpova V.M., Nyafkin A.N., Kurbatkina E.I.
Abstract

The article presents a scientific and technical literature review of copper-based hybrid composite materials (CM). Common combinations of reinforcing components for the manufacture of hybrid composite materials are presented. The main methods for fabricating copper-based hybrid CMs are briefly mentioned. The influence of a combination of various types of reinforcing components and their volume or mass content on the mechanical, thermophysical and tribological properties of hybrid CMs based on copper is considered. A comparison of the characteristics of hybrid CMs with matrix alloys or metallic CMs of similar systems is given.

Keywords
composite material, hybrid composite material, reinforcing component, whiskers, particles, silicon carbide, graphite oxide, titanium boride, graphene, aluminum nitride
Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. What is the future to be made of? Materials of a new generation, technologies for their creation and processing - the basis of innovation. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  3. Kablov E.N., Valueva M.I., I.V. Zelenina, Khmelnitskiy V.V., Aleksashin V.M. Carbon plastics based on benzoxazine oligomers – perspective materials. Trudy VIAM, 2020, no. 1, paper no. 07. Available at: http://www.viam-works.ru (accessed: June 2, 2021). DOI: 10.18577/2307-6046-2020-0-1-68-77.
  4. Imametdinov E.S., Valueva M.I. Сomposites for piston engines (rеview). Aviacionnye materialy i tehnologii, 2020, no. 3 (60), pp. 19–28. DOI: 10.18577/2071-9140-2020-0-3-19-28.
  5. Karashaev M.M., Bazyleva O.A., Shesta- kov A.V., Ovsepyan S.V. Technological princi-ples for the development of metal composite materials reinforced with oxide and intermetallic particles. Aviacionnye materialy i tehnologii, 2020, no. 3 (60), pp. 29–36. DOI:10.18577/2071-9140-2020-0-3-29-36.
  6. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  7. Serpova V.M., Sidorov D.V., Nyafkin A.N., Kurbatkina E.I. Hybrid metal matrix compo-sites based on aluminum alloys (review). Trudy VIAM, 2021, no. 3 (97), paper no. 06. Available at: http://www.viam-works.ru (accessed: June 2, 2021). DOI: 10.18577/2307-6046-2021-0-3-68-77.
  8. Chawla N., Chawla K.K. Metal Matrix Composites. New York: Springer Sience + Business Media, Inc., 2006, pp. 351–379.
  9. Chu K., Jia C.C., Jiang L.K., Li W.S. Thermal conductivity enhancement in carbon nanotube/Cu–Ti composites. Applied Physics A, 2013, vol. 110, pp. 269–273. DOI: 10.1007/s00339-012-7450-0.
  10. Dong S.J., Zhou Y., Shi Y.W., Chang B.H. Formation of a TiB2-Reinforced Copper-Based Composite by Mechanical Alloying and Hot Pressing. Metallurgical and materials transactions A, 2002, vol. 33A, pp. 1275–1280. DOI: 10.1007/s11661-002-0228-9.
  11. Jia L., Yang M., Lu Z. et al. Microstructure evolution and reaction behavior of Cu–Ni alloy and B4C powder system. Progress in Natural Science: Materials International, 2021, vol. 31, pp. 55–62. DOI: 10.1016/j.pnsc.2020.12.002.
  12. Zhang X., Shi C., Liu E. In-situ space-confined synthesis of well-dispersed three-dimensional graphene/carbon nanotube hybrid reinforced copper nanocomposites with balanced strength and ductility. Composites. Part A: Applied Science and Manufacturing, 2017, vol. 103, pp. 178–187. DOI: 10.1016/j.compositesa.2017.
  13. Thankachan T., Prakash K., Kavimani S. Investigating the effects of hybrid reinforcement particles on the microstructural, mechanical and tribological properties of friction stir processed copper surface composites. Composites, Part B: Engineering, 2019, vol. 174. DOI: 10.1016/j.compositesb.2019.107057.
  14. Liang S., Li W., Jiang Y. et al. Microstructures and properties of hybrid copper matrix composites reinforced by TiB whiskers and TiB2 particles. Journal of Alloys and Compounds, 2019, vol. 797, pp. 589–594. DOI: 10.1016/j.jallcom.2019.05.1.
  15. Akbarpour M.R., Salahi E., Alikhani H.F. et al. Fabrication, characterization and mechanical properties of hybrid composites of copper using the nanoparticulates of SiC and carbon nanotubes. Materials Science and Engineering: A, 2013, vol. 572, pp. 83–90. DOI: 10.1016/j.msea.2013.02.039.
  16. Chen X., Tao J., Liu Y. et al. Interface interaction and synergistic strengthening behavior in pure copper matrix composites reinforced with functionalized carbon nanotube-graphene hybrids. Carbon, 2019, vol. 146, pp. 736–755. DOI: 10.1016/j.carbon.2019.02.048.
  17. Chu K., Wang F., Li Y. et al. Interface and mechanical/thermal properties of graphene/copper composite with Mo2C nanoparticles grown on grapheme. Composites, Part A: Applied Science and Manufacturing, 2018, vol. 109, pp. 267–279. DOI: 10.1016/j.compositesa.2018.
  18. Luo H., Sui Y., Qi J. et al. Copper matrix composites enhanced by silver/reduced graphene oxide hybrids. Materials Letters, 2017, vol. 196, pp. 354–357. DOI: 10.1016/j.matlet.2017.03.08.
  19. Zhang X., Dong P., Zhang B. et al. Preparation and characterization of reduced graphene oxide/copper composites incorporated with nano-SiO2 particles. Journal of Alloys and Compounds, 2016, vol. 671, pp. 465–472. DOI: 10.1016/j.jallcom.2016.02.06.