Krivushina A.A., Startsev V.O. Micromycetes-destructors of polymeric materials among extremophilic microorganisms (review) // Proceedings of VIAM. 2022. No. 1 (107). Ст. 12. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2022-0-1-123-134.

Micromycetes-destructors of polymeric materials among extremophilic microorganisms (review)

Krivushina A.A., Startsev V.O.
Abstract

Extremophilic microorganisms are able to survive under extreme environmental conditions. The article is devoted to a review of research works on the study of extremophilic micromycetes, as well as the search among them for species known as destructors of polymeric materials. Such groups of extremophilic micromycetes as thermophiles, xerophiles, and oligotrophs, capable of surviving at high ambient temperatures, low humidity and lack of nutrients, are considered.In each group of extremophilic microorganisms, species of micromycetes were found, which were repeatedly noted as destructors of polymer materials.

Keywords
extremophilic microorganisms, extremophiles, micromycetes-destructors, biodeterioration, thermophiles, xerophiles, oligotrophs, ecological niche
Reference list
  1. Kablov E.N. The key problem is materials. Trends and guidelines for innovative development in Russia. Moscow: VIAM, 2015, pp. 458–464.
  2. Kablov E.N., Erofeev V.T., Svetlov D.A., Smirnov V.F., Bogatov A.D. Biodamage in space vehicles. Int. scientific and technical conf. “Composite materials. Theory and practice". Penza: Privolzhsky House of Knowledge, 2015, pp. 40–46.
  3. Krivushina A.A., Goryashnik Yu.S. Ways of protection of materials and products from microbiological damage (review). Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 80–86. DOI: 10.18577/2071-9140-2017-0-2-80-86.
  4. Krivushina A.A., Bobyreva T.V., Yakovenko T.V., Nikolaev E.V. Methods of microorganisms-destructors storage in FSUE «VIAM» collection (review). Aviacionnye materialy i tehnologii, 2019, No. 3 (56), pp. 89–94. DOI: 10.18577 / 2071-9140-2019-0-3-89-94.
  5. Kablov E.N., Erofeev V.T., Dergunova A.V., Deraeva E.V., Svetlov D.A. Influence of environmental factors on the processes of biodegradation of vinylester composites. Journal of Physics: Conference Series. International Conference on Engineering Systems. 2020, vol. 1687, art. 012029. DOI: 10.1088/1742-6596/1687/1/012029.
  6. Sevastyanov D.V., Sutubalov I.V., Daskovskij M.I., Shein E.A. Polymer biocomposites based on biodegradable binders reinforced by natural fibers (review). Aviacionnye materialy i tehnologii, 2017, no. 4 (49), pp. 42–50. DOI: 10.18577/2071-9140-2017-0-4-42-50.
  7. Morozkina E.V., Slutskaya E.S., Fedorova T.V. et al. Extremophilic microorganisms: biochemical adaptation and biotechnological application (review). Prikladnaya biokhimiya i mikrobiologiya, 2010, vol. 46, no. 1, pp. 5–20.
  8. Marteinsson V.T., Birrien J.L., Reysenbach A.L. et al. Thermococcus barophilus sp.now., a new barophilic and hyperthermophilic archaeon isolated under high hydrostatic pressure from a deep-sea hydrothermal vent. International Journal of Systematic Bacteriology, 1999, vol. 49, no. 2, pp. 351–359. DOI: 10.1099/00207713-49-2-351.
  9. Cooney D. G., Emerson R. Thermophilic fungi. An account of their biology, activities and classification. San Francisco ; London: W.H. Freeman & Co, 1964, no. 15, pp. 25–35.
  10. Kuzyakina T.I. Ecology and geochemical activity of microorganisms on active volcanoes and in hydrothermal waters. Vladivostok: Dalnauka, 2004, 251 p.
  11. Kalinina A.E., Sokolyanskaya L.O., Glukhova L., Karnachuk O.V. Isolation of thermophilic micromycetes from coal combustion sites. Start in science: materials LXVII scientific. stud. conf. Biological Institute. Tomsk, 2019, p. 77.
  12. Kartavtseva Z.M., Koval E.Z., Kalaganov V.A., Lyapunov N.A. Destruction of diesel fuel by microorganisms in circulation systems. Mikrobiologicheskiy zhurnal, 1989, vol. 51, no. 4, pp. 87–94.
  13. Gaylarde C.C., Bento F.M., Kelley J. Microbial contamination of stored hydrocarbon fuels and its control. Revista de Microbiologia, 1999, vol. 30, no. 1, pp. 1–10.
  14. Bento F.M., Beech I.B., Gaylarde C.C. et al. Degradation and corrosive activities of fungi in a diesel – mild steel – aqueous system. World journal of microbiology and biotechnology, 2005, vol. 21, no. 2, pp. 135-142.
  15. McNamara C. J., Perry T.D., Leard R. et al. Corrosion of aluminum alloy 2024 by microorganisms isolated from aircraft fuel tanks. Biofouling, 2005, vol. 21, no. 5, pp. 257–265.
  16. Chertishchev V.Yu., Ospennikova O.G., Boichuk A.S., Dikov I.A., Generalov A.S. Determina-tion of the size and depth of defects in multilayer PCM honeycomb structures based on the mechanical impedance value. Aviaсionnye materialy i tehnologii, 2020, no. 3 (60), pp. 72–94. DOI: 10.18577/2071-9140-2020-0-3-72-94.
  17. Lugauskas A.Yu., Mikulskene A.I., Shlyauzhene D.Yu. Catalog of micromycetes-biodegradants of polymeric materials. Moscow: Nauka, 1987, pp. 258–259.
  18. Zlochevskaya I.V. Ecological groups of fungi damaging materials and their features. Biologicheskiye nauki, 1987, no. 8, pp. 81–87.
  19. Scott J.A., Forsyth T.J. Thermophilic microorganisms in aircraft fuel. International Biodeterioration Bulletin, 1976, vol. 12.No. 1, pp. 1-4.
  20. Thomas A.R., Hill E.C. Aspergillus fumigatus and supersonic aviation. International Biodeterioration Bulletin, 1977, vol. 13.No. 1, pp. 1-4.
  21. Kanevskaya I.G. Biological damage to industrial materials. Leningrad: Nauka, 1984, 232 p.
  22. Moretti M.M.S., Martins D.A.B., Silva R.D., Rodrigues A. Selection of thermophilic and thermotolerant fungi for the production of cellulases and xylanases under solid-state fermentation. Brazillian Journal of Microbiology, 2012, vol. 43 (3), pp. 1062–1071. DOI: 10.1590/S1517-838220120003000032.
  23. Brink J.V.D., Harman-van Muiswinkel G.C.J., Theelen B.J.F. Efficient plant biomass degradation by thermophilic fungus Myceliophthora heterothallica. Applied and Environmental microbiology, 2012, vol. 79 (4). DOI: 10.1128/AEM.02865-12.
  24. McClendon S.D., Batth T., Petzold C.J. et al. Thermoascus aurantiacus is a promising source of enzymes for biomass deconstruction under thermophilic conditions. Biotechnology for biofuels, 2012, no. 5 (54), pp. 1–9.
  25. Berka R. M., Grigoriev I. V., Otillar R. et al. Comparative genomic analysis of the thermophilic biomass-degrading fungi Myceliophthora thermophila and Thielavia terrestris. Nature Biotechnology, 2011, vol. 29, no. 10, pp. 922–927. DOI: 10.1038/nbt. 1976.
  26. Balabanova L.A., Bakunina I.Yu., Slepchenko L.V. and other Polysaccharide-degrading activity of marine and terrestrial strains of filamentous fungi. Bioorganicheskaya khimiya, 2018, vol. 44, no. 4, pp. 425–432.
  27. Goryaeva A.G., Velikova T.D., Dobrusina S.A. Mycobiota of air and composites of paper with polymer coatings in the Russian National Library. Mikologiya i fitopatologiya, 2010, vol. 44, no. 1, pp. 10–18.
  28. Smolyanitskaya OL Micromycetes as potential agents of biological damage to cultural property and a strategy of protection against them in the State Hermitage: thesis abstracts, Cand. Sc. (Bio). St Petersburg, 2007, 26 p.
  29. Goncharova I.A., Sabadakha E.N., Trigubovich A.M., Black N.V. Mycological analysis of industrial materials contaminated with microscopic fungi. Trudy BGTU, Ser. 2, 2020, no. 2, pp. 163–168.
  30. Rebrikova NL, Ponizovskaya VB Extremely xerophilic fungi found in museum funds. Modern mycology in Russia: abstracts reports. Ser. 6, 2015, vol. 5, pp. 298–300.
  31. Kuvshinova N.M., Svistova I.D., Gulieva D.Z. The composition and structure of the mycomycete complex of leached chernozem. Razvitiye sovremennoy nauki: teoreticheskiye i prikladnyye aspekty, 2016, no. 3, pp. 173–175.
  32. Zheltikova T.M., Antropova A.B., Bilanenko E.N. et al. Molds for living quarters. RET-info, 2006, no. 1, pp. 31–36.
  33. Antropova A.B., Mokeeva V.L., Bilanenko E.N. and other Aeromikota living quarters in Moscow. Mikologiya i fitopatologiya, 2003, vol. 37, is. 6, pp. 1–11.
  34. Sizonenko T.A., Khabibullina F.M., Zagirova S.V. Soil microbiota of the meso-oligotrophic bog of the middle taiga. Mikologiya i fitopatologiya, 2016, vol. 50. 2, pp. 115–123.
  35. Mitkovskaya T.I., Koval E.Z. Assessment of the role of micromycetes isolated from works of art. Abstracts of the II congress of mycologists of Russia "Modern mycology in Russia". Moscow: Nat. Academy of Mycology, 2008, vol. 2, pp. 374–375.
  36. Kataev A.D., Kurakov A.V. Microbial colonization and destruction of biodegradable synthetic materials based on polyhydroxybutyrate and polyhydroxyvalerate in soils. Abstracts of the III congress of mycologists of Russia "Modern mycology in Russia". Moscow: Nat. Academy of Mycology, 2012, vol. 3, pp. 218–219.
  37. Baluta A.A., Vazhinskaya I.S. Resistance of modern building materials to mold damage. Abstracts of the III congress of mycologists of Russia "Modern mycology in Russia". Moscow: Nat. Academy of Mycology, 2012, vol. 3, p. 210.
  38. Ogarkova G.R., Bukovskaya N.E., Samusenok L.V., Ogarkov B.N. Biodamage of porous building materials by associations of specific microorganisms. Abstracts of the III congress of mycologists of Russia "Modern mycology in Russia". Moscow: Nat. Academy of Mycology, 2012, vol. 3, pp. 224–225.
  39. Mamaeva N.Yu., Velikova T.D., Goryaeva A.G. Biodamage of paper by micromycetes under conditions of different illumination. Abstracts of the IV congress of mycologists of Russia "Modern mycology in Russia". Moscow: Nat. Academy of Mycology, 2017, vol. 6, pp. 418–420.
  40. Popikhina E.A., Trepova E.S. Microdestructors of building materials. Tez. reports of the IV congress of mycologists of Russia "Modern mycology in Russia". Moscow: Nat. Academy of Mycology, 2017, vol. 6, pp. 424–426.
  41. Khalmuradova P.A., Mezitova L.D., Alatbi A.Kh. et al. Micromycetes-destructors of old buildings in Kazan: analysis of metabolites and selection of biocides. Abstracts of the IV congress of mycologists of Russia "Modern mycology in Russia". Moscow: Nat. Academy of Mycology, 2017, vol. 6, pp. 415.
  42. Georgieva M.L., Grum-Grzhimailo A.A., Yamnova I.A., Bilanenko E.N. Filamentous fungi in the soils of sulfate-soda salinization of the Gobi Desert (Mongolia). Mikologiya i fitopatologiya, 2012, vol. 46. 1, pp. 27–32.
  43. Redkina V.V. Biological activity of primary soils on nepheline sands of tailing dumps of JSC "Apatit" (Murmansk region). Biological monitoring of natural-technogenic systems: materials of All-Russian. scientific-practical conf. with Int. participation. Kirovsk: Loban, 2011, part 1, pp. 148–152.
  44. Evdokimova G.A., Korneikova M.V., Lebedeva E.V., Kalmykova V.V. Micromycetes in sands and sandy soils of natural and technogenic genesis. Mikologiya i fitopatologiya, 2009, vol. 43, is. 2, pp. 84–92.
  45. Rojas T. I., Aira M. J., Batista A. et al. Fungal biodeterioration in historic buildings of Havana (Cuba). Grana, 2012, vol. 51, is. 1, pp. 44–51.
  46. Sumina O.I., Vlasov D.Yu., Dolgova L.L., Safronova E.V. Features of the formation of communities of micromycetes in overgrown sand pits in the north of Western Siberia. Vestnik Sankt-Peterburgskogo universiteta, Ser. 3, 2010, is. 2, pp. 84–90.