Solovyanchik L.V., Kondrashov S.V. The prospects of using carbon nanotubes to impart functional properties to the surface of polymer materials (review) // Proceedings of VIAM. 2021. No. 9 (103). Ст. 02. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-9-11-21.

The prospects of using carbon nanotubes to impart functional properties to the surface of polymer materials (review)

Solovyanchik L.V., Kondrashov S.V.
Abstract

Presents a review of the scientific literature on various methods for producing electrically conductive polymer materials and coatings. The prospects of using carbon nanotubes (CNT) to impart high electrical properties to the surface of materials are shown. The mechanism of formation of the structured surface of polymer materials with CNT is described. It is shown that the use of CNT is a promising way to impart electrically conductive and superhydrophobic properties to the surface.

Keywords
electrically conductive material, electrically conductive coating, superhydrophobic properties, electric conductivity, carbon nanotubes.
Reference list
  1. Kablov E.N. Aviation and Space Materials Science. Vse materialy. Entsiklopedicheskiy spravochnik, 2008, no. 3, pp. 2–14.
  2. Kablov E.N. Chemistry in aviation materials science. Russian Journal of General Chemistry, 2011, vol. 81, no. 5, pp. 967–969.
  3. Fedusiv I.N., Chermoshentsev S.F. Propulsion electrification of an unmanned aerial vehicle. XXII Tupolev Readings (School of Young Scientists). Kazan: KNITU-KAI, 2015, pp. 150–153.
  4. Horvat T., Berta I. Neutralization of static electricity. Trans. from Engl. Moscow: Energoatomizdat, 1987, 104 p.
  5. Gainutdinov R.R., Chermoshentsev S.F. Methodology for ensuring the intersystem electromagnetic compatibility of the onboard equipment of unmanned aerial vehicles. Izvestiya vysshikh uchebnykh zavedeniy. Aviatsionnaya tekhnika, 2016, no. 4, pp. 155–160.
  6. Gorlov M.I., Emelyanov A.V., Plebanovich V.I. Electrostatic charges in electronics. Minsk: Belarusian Science, 2006, 295 p.
  7. Hirano Y., Yoshimura A. Coupled thermal-electrical analysis for carbon fiber/epoxy composites exposed to simulated lightning current. Composites, Part A. 2010, no. 41, pp. 973–981.
  8. Tkachenko A.N., Vishnyakov L.R., Gogaev K.A. et al. Copper microwires for lightning protection meshes of knitted structure. Tekhnologicheskie sistemy, 2009, no. 4, pp. 16–20.
  9. Polozkov V.T., Goncharyuk V.A., Linetskiy V.A., Sultanovich A.I. Labor protection at oil refineries and petrochemical plants. Moscow: Khimiya, 1973, 296 p.
  10. Khalilov F.Kh. Electromagnetic compatibility of electric power industry, technosphere and biosphere: textbook. Saint Petersburg: Center for training energy personnel, 2014, 190 p.
  11. Melnikov A.A., Shchur P.A. Transparent conductive antireflective coatings based on ITO, SiO2, TiO2. Trudy VIAM, 2019, No. 8 (80), paper no. 07. Available at: http://www.viam-works.ru (accessed: June 1, 2021). DOI: 10.18577 / 2307-6046-2019-0-8-56-66.
  12. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  13. Knyazheva O.A., Baklanova O.N., Zhansakova K.S. et al. Physical and mechanical properties and electrical conductivity of polypropylene ‒ carbon black compositions. 9 Int. Sc. & Tech. Conf. «Technics and technology of petrochemical and oil and gas production». Omsk, 2019, pp. 165–165.
  14. Low-resistivity polymer positive temperature coefficient material and preparation method thereof: pat. CN 102167859; filed 20.01.11; publ. 31.08.11.
  15. Improved thermal conductive polymeric PTC compositions: pat. US 2008039575; filed 03.08.07; publ. 02.14.08.
  16. Polyolefin/carbon black PTC conductive composite material and preparing method thereof: pat. CN 1528817; filed 30.09.03; publ. 15.09.04.
  17. PTC conductive composition containing a low molecular weight polyethylene processing aid: pat. US 6620343; filed 19.03.02; publ. 16.09.03.
  18. Ragushina M.D., Evseeva K.A., Kalugina E.V., Ushakova O.B. Polymer composite materials with antistatic and electrically conductive properties. Plasticheskie massy, 2021, no. 3-4, pp. 6–9.
  19. Stepashkina A.S., Tsobkallo E.S., Aleshin A.N. Modeling the electrical conductivity of composite materials based on polypropylene and carbon black. Izvestiya vysshikh uchebnykh zavedeniy. Tekhnologiya legkoy promyshlennosti, 2014, vol. 25, pp. 51–54.
  20. Matkovsky P.E., Sedov I.V., Saratovskikh S.L., Yarullin R.S. Thermoplastic composite materials. Vse materialy. Entsiklopedicheskiy spravochnik, 2011, no. 2, pp. 2–16.
  21. Lubineau G., Rahaman A. A review of strategies for improving the degradation properties of laminated continuous-fiber/epoxy composites with carbon-based nanoreinforcements. Carbon, 2012, vol. 50, pp. 2377–2395.
  22. Lukina E.A., Zaitsev D.V., Romanenko V.A. Structure and properties of a composite material based on aluminum alloy with the addition of carbon nanotubes. Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 27–34. DOI: 10.18577/2071-9140-2019-0-4-27-34.
  23. Garcia E.J., Wardle B.L., Hart J.A., Yamamoto N. Fabrication and multifunctional properties of a hybrid laminate with aligned carbon nanotubes grown In Situ. Composites Science and Technology, 2008, vol. 68, pp. 2034–2041.
  24. Gunyaev G.M., Kablov E.N., Aleksashin V.M. Modification of structural carbon plastics with carbon nanoparticles. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, no. 1, pp. 5–11.
  25. Dushin M.I., Donetskiу K.I., Timoshkov P.N., Karavaev R.Yu. Research of process of out-of-autoclave formation semi-pregs on the basis of carbon fillers (rеview). Trudy VIAM, 2018, no. 9 (69), paper no. 03. Available at: http://www.viam-works.ru (accessed: June 1, 2021). DOI: 10.18577/2307-6046-2018-0-9-21-31.
  26. Popkov O.V., Yurkov G.Y., Fionov A.S. Stabilization of nanoparticles on the surface of detonation nanodiamond. Physics, chemistry and application of nanostructures. Singapore: World Scientific, 2009, pp. 369–372.
  27. Gul V.E., Shenfil L.Z. Electrically Conductive Polymer Compositions, Moscow: Knimiya, 1984, 240 p.
  28. Ivanovsky V.I. Carbon black. Processes and devices: textbook. Omsk: Tekhuglerod, 2004, 228 p.
  29. Donnet J.B., Bansal R.C., Wang M.J. Carbon Black: Sceince and Technology. 2nd ed. New York: Marcel Dekker Inc., 1993, 461 p.
  30. Klochko B.N., Zachateyskiy E.E., Biider V.Ya. Influence of the dispersity and structure of soot on its electrical resistance. Kauchuk i rezina, 1969, no. 8, pp. 22–24.
  31. Sommers D.J. Carbon black for electrically conductive plastics. Polymer Plastics Technology and Engineering, 1984, vol. 23 (1), pp. 83–98.
  32. Safronov V.A., Klochkova D.A., Seleznev A.A. Electrically conductive thermoplastic elastomers based on polyolefins. XXII Regional Conf. young scientists of the Volgograd region. Volgograd, 2017, pp. 26–27.
  33. Bauhofer W., Kovacs J.Z. A review and analysis of electrical percolation in carbon nanotube polymer composites. Composites Science and Technology, 2009, vol. 69, pp. 1486–1498.
  34. Polymer – carbon nanotube composites. Preparation, properties and applications. Ed. T. McNally, P. Pötschke. Woodhead Publishing Ltd., 2011, 820 p.
  35. Carbon Nanotubes – Polymer Nanocomposites. Ed. S. Yellampalli. Published by InTech, 2011, 396 p.
  36. Irzhak V.I. Epoxy composite materials with carbon nanotubes. Uspekhi khimii, 2011, no. 8, pp. 821–839.
  37. Rakov E.G. Carbon nanotubes in new materials. Uspekhi khimii, 2013, vol. 82, no. 1, pp. 227–247.
  38. Reia da Costa E.F., Skordos A.A., Partridge I.K., Rezai A. RTM processing and electrical performance of carbon nanotube modified epoxy/fiber Composites. Composites. Part A: Applied Science and Manufacturing, 2012, vol. 43, no. 4, pp. 593–602.
  39. Badamshina E.R., Gafurova M.P., Estrin Ya.I. Modification of nanotubes and synthesis of polymer composites with their participation. Uspekhi khimii, 2010, vol. 79, no. 11, pp. 1027–1063.
  40. Grady B.P. Carbon Nanotube-Polymer Composites: Manufacture, Properties, and Applications. Wiley, 2011, 352 p.
  41. Troung V.T., Tsang K.M.C., Keough S.J., St John N.G. Effect of Sonication on the Mechanical Properties of Poly Vinyl Alcohol. Carbon Nanotube Composites, 2006, no. 6415, pp. 641–503.
  42. 42. Kondrashov S.V., Shashkeev K.A., Petrova G.N., Mekalina I.V. Constructional polymer composites with functional properties. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 405–419. DOI: 10.18577/2071-9140-2017-0-S-405-419.
  43. Akatenkov R.V., Aleksashin V.M., Anoshkin I.V., Babin A.N., Bogatov V.A., Grachev V.P., Kondrashov S.V., Minakov V.T., Rakov E.G. Criterion of the application efficiency of functionalized carbon nanotubes for improving the physico-mechanical properties of epoxy resins. Aviacionnye materialy i tehnologii, 2010, no. 3, pp. 22–27.
  44. Solovyanchik L.V., Shashkeev K.A., Soldatov M.A. A method for controlling the electrical conductive properties of a polymer composition. Bulletin of the Moscow Aviation Institute. Vestnik Moskovskogo aviatsionnogo instituta, 2017, vol. 24, no. 4, pp. 184–194.
  45. Yakovlev A.D. Chemistry and technology of paints and varnishes: textbook. Saint Petersburg: Khimizdat, 2010.448 p.
  46. Matkovsky P.E., Sedov I.V., Saratovskikh S.L., Yarullin R.S. Thermoplastic composite materials. Entsiklopediya inzhenera-khimika, 2011, no. 6, pp. 49–57.
  47. Richardson M. Industrial polymer composite materials. Moscow: Chemistry, 1980, p. 472.
  48. Compositions for electrically conductive coatings and a method of making solid electrically conductive coatings: pat. 2460750 Rus. Federation, no. 2011115573/05; declared 21.04.11; publ. 10.09.12.
  49. Kats G.S., Milevski D.V. Fillers for polymer composite materials: a reference guide. Moscow: Khimiya, 1981, p. 736.
  50. Electrically conductive paint for radio-absorbing aggregates: pat. 2472825 Rus. Federation, no. 2011145154/05; declared 09.11.11; publ. 20.01.13.
  51. Shchibrya N.G. Powder-based antistatic decorative coatings. Lakokrasochnyye materialy i ikh primeneniye, 1996, no. 12, pp. 19–20.
  52. Tolmacheva D. Powder paints with metallic effect. Features of production. Promyshlennaya okraska, 2011, no. 2, pp. 33–34.
  53. Yazykov S.Yu., Dammer V.Kh., Panin S.V., Vechkin B.B. Antistatic composite coatings for the protection of magnesium alloys based on powder paints processed in a planetary ball mill. Izvestiya Tomskogo politekhnicheskogo universiteta. Inzhiniring georesursov, 2014, vol. 325, no. 2, pp. 105–111.
  54. Kondrashov E.K. Paints and varnishes for special purposes. Lakokrasochnyye materialy i ikh primeneniye, 1994, no. 11–12, pp. 23–24.
  55. Guldi D.M., Nazario M. Carbon Nanotubes and Related Structures: Synthesis, Characterization, Functionalization, and Applications. Wiley-VCH Verlag GmbH & Co., 2010, p. 562.
  56. Lordi V., Yao N. Molecular mechanics of binding in carbon-nanotube-polymer composites. Journal of Materials Research, 2000, vol. 15, no. 12, pp. 2770–2779.
  57. Fritzsche J., Lorenz H., Kluppel M. et al. Elastomer – carbon nanotube composites in Polymer – carbon nanotube composites. Preparation, properties and applications. Woodhead Publishing Ltd, 2011, 820 p.
  58. Boynovich LB, Emelianenko A.M. Hydrophobic materials and coatings: principles of creation, properties and application. Uspekhi khimii, 2008, vol. 77, no. 7, pp. 619–638.
  59. Zou J., Chen H., Chunder A. Et al. Preparation of a Superhydrophobic and Conductive Nanocomposite Coating from a Carbon-Nanotube-Conjugated Block Copolymer Dispersion. Advanced Materials, 2008, vol. 20, no. 17, pp. 3337–3341.
  60. Peng M., Liao Z., Qi J., Zhou Z. Nonaligned carbon nanotubes partially embedded in polymer matrixes: a novel route to superhydrophobic conductive surfaces. Langmuir, 2010, vol. 26, no. 16, pp. 13572–13578.
  61. Kablov E.N., Solovyanchik L.V., Kondrashov S.V., Yurkov G.Yu., Buznik V.M., Kushch P.P., Kichigina G.A., Kiryukhin D.P., Dyachkova T.P. Electrically conductive hydrophobic polymer composite materials based on oxidized carbon nanotubes modified with tetrafluoroethylene telomers. Rossiyskiye nanotekhnologii, 2016, vol. 11, no. 12, pp. 91–97.
  62. Das A., Hayvaci H. T., Tiwari M. K. et al. Superhydrophobic and conductive carbon nanofiber / PTFE composite coatings for EMI shielding. Journal of colloid and interface science, 2011, vol. 353, no. 1, pp. 311–315.
  63. Han J.T., Kim S.Y., Woo J.S., Lee G.W. Transparent, conductive, and superhydrophobic films from stabilized carbon nanotube/silane sol mixture solution. Advanced Materials, 2008, vol. 20, no. 19, pp. 3724–3727.
  64. Asthana A., Maitra T., Büchel R., Tiwari M. K., Poulikakos D. Multifunctional superhydrophobic polymer/carbon nanocomposites: graphene, carbon nanotubes, or carbon black? ACS applied materials & interfaces. 2014, vol. 6, no. 11, pp. 8859–8867.
  65. Solovyanchik L.V., Kondrashov S.V., Nagornaya V.S., Volkov I.A., Dyachkova T.P., Borisov K.M. Electrically conductive, highly hydrophobic nanocomposites based on fluoropolymer with carbon nanotubes. Zhurnal prikladnoy khimii, 2018, vol. 91, no. 10, pp. 1462–1467.