Nikolaev E.V., Slavin A.V., Startsev V.O., Laptev A.B. Modern approaches to assessing the impact of external factors on materials and complex technical systems (to the 120th anniversary of G.V. Akimov) // Proceedings of VIAM. 2021. No. 9 (103). Ст. 12. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-9-117-130.
Modern approaches to assessing the impact of external factors on materials and complex technical systems (to the 120th anniversary of G.V. Akimov)
Abstract
The founder of the science of protecting materials from corrosion, aging and bio-damage in Soviet Russia is Georgy Vladimirovich Akimov, who created the infrastructure for climate testing of materials and products. Currently, his students and followers have discovered new directions for the development of climatic and microbiological tests – these are studies of the preservation of the properties of materials in complex technical systems under the influence of climatic factors, mold fungi, bacteria and operational loads using the most modern methods at the sites of the created network of climate test stations, as well as using modern regulatory documentation.
Keywords
corrosion of metals and concrete, aging of polymer materials, bio-damage of materials, climatic tests, bacteria, micromycetes, sequencing, prediction of material properties.
Reference list
- Akimov G.V. Theory and methods of metal corrosion research. Moscow; Leningrad: Publishing house of the Academy of Sciences of the USSR, 1945, 414 p.
- Investigation of corrosion of metals under tension. Ed. G.V. Akimov. Moscow: Mashgiz, 1953, 140 p.
- Akimov G.V., Rosenfeld I.L. Influence of the concentration of hydrogen ions on corrosion and electrode potential of metals. Research in the field of electrochemical and corrosion behavior of metals and alloys. Moscow: Oborongiz, 1950, pp. 201–233.
- Paleologue E.N., Akimov G.V., Tomashov N.D., Korotkova K.S. Influence of protective films on corrosion and electrochemical behavior of magnesium. Problem of corrosion and protection of metals. Moscow: Publishing House of the Academy of Sciences of the USSR, 1956, pp. 237–254.
- Clark G.B., Akimov G.V. Electrode potentials of magnesium-based solid solutions. Research in the field of electrochemical and corrosion behavior of metals and alloys. Moscow: Oborongiz, 1950, pp. 121–137.
- Kablov E.N., Startsev V.O. Climatic aging of polymer composite materials for aviation purposes. I. Assessment of the influence of significant influencing factors. Deformatsiya i razrusheniye materialov, 2019, no. 12, pp. 7–16.
- Kablov E.N., Erasov V.S., Panin S.V., Course M.G., Gladkikh A.V., Avtaev V.V., Sorokina N.I., Lukyanychev D.A. Investigation of the combined effect of mechanical loads and climatic factors on the properties of materials in the composition of a large-sized structure of the experimental wing compartment after 4 years of testing. Reports of the II Intern. scientific and technical conf. "Corrosion, aging and biostability of materials in a maritime climate". Moscow: VIAM, 2016. Art. 6.
- Kablov E.N., Startsev V.O. Climatic aging of polymer composite materials for aviation purposes. II. Development of research methods for the early stages of aging. Deformatsiya i razrusheniye materialov, 2020, no. 1, pp. 15–21.
- Laptev A.B., Nikolaev E.V., Kurshev E.V., Goryashnik Yu.S. Features of biodegradation of thermoplastics based on polyesters in different climatic zones. Trudy VIAM, 2019, no. 7 (79), paper no. 10. Available at: http://www.viam-works.ru (accessed: June 15, 2020). DOI: 10.18577/2307-6046-2019-0-7-84-91.
- Krasnoyarsk V.V., Frenkel G.V., Nosov R.P. Corrosion and protection of metals. Moscow: Metallurgy, 1969, p. 9.
- Polyakov K.A., Slomyanskaya F.B., Polyakova K.K. Corrosion and chemical resistant materials. Moscow: State sc. and tech. publ. house chem. literature, 1953, p. 10.
- Kablov E.N., Petrova A.P., Narsky A.R. G.V. Akimov – the creator of the national science of corrosion. Istoriya nauki i tekhniki, 2009, no. 11, pp. 12–15.
- Castañeda A., Corvo F., Fernández D., Valdés C. Outdoor-Indoor Atmospheric Corrosion in a Coastal Wind Farm Located in a Tropical Island. Engineering journal, 2016, vol. 21, is. 2, pp. 44–62.
- Morcillo M., Chico B., de la Fuente D., Simancas J. Looking back on contributions in the field atmospheric corrosion offered by the MICAT Ibero-American testing network. International journal of corrosion, 2012, vol. 2012, art. ID 824365.
- Dong J., Han E., Ke W. Introduction to atmospheric corrosion research in China. Science and Technology of Advanced Materials, 2007, no. 8, pp. 559–565.
- Perevedentsev Yu.P., Zandi R., Aukhadaev T.R. Dynamics of dust storms on the territory of Khuzenstan (south-west of Iran) at the beginning of the XXI century. Rossiyskiy zhurnal prikladnoy ekologii, 2015, no. 1, pp. 10–14.
- Khristoforov D.A., Klyushnichenko A.B., Startsev V.O., Suranov A.Ya., Fizulov B.G., Startsev O.V. Linear dilatometry of polymers and polymer composite materials. Experimental methods in the physics of structurally inhomogeneous condensed media: proceedings of the Second Intern. scientific and technical conf. EFM-2001. Barnaul: Altaysk. state un-t, 2001, pp. 186–194.
- Nizina T.A., Startsev V.O., Selyaev V.P., Startsev O.V., Nizin D.R. Analysis of the influence of actinometric parameters on the intensity of changes in the color characteristics of epoxy composites in a marine climate. Vestnik Belgorodskogo gosudarstvennogo tekhnologicheskogo universiteta imeni I.I. V.G. Shukhova, 2015, no. 5, pp. 95–101.
- Kurs M.G., Kutyrev A.E., Fomina M.A. Research of corrosion damage of wrought aluminium alloys at laboratory and full-scale tests. Trudy VIAM, 2016, no. 8 (44), paper no. 10. Available at: http://www.viam-works.ru (accessed: June 18, 2021). DOI: 10.18577/2307-6046-2016-0-8-10-10.
- Abramova M.G. Revisiting the confirmation of the identity of the corrosion destruction mechanism of aluminum alloys (review). Part 1. Atmospheric corrosion. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 86–94. DOI: 10.18577/2071-9140-2020-0-4-86-94.
- Abramova M.G. Revisiting the confirmation of the identity of the corrosion destruction mechanism of aluminum alloys (review). Part 2. Corrosion in sea water. Aviation materials and technology, 2021. no. 1 (62). paper no. 09. Available at: http://www.journal.viam.ru (accessed: July 7, 2021). DOI: 10.18577/2713-0193-2021-0-1-95-103.
- Tourova T., Sokolova D., Nazina T., Grouzdev D., Kurshev E., Laptev A. Biodiversity of microorganisms colonizing the surface of polystyrene samples exposed to different aqueous environments. Sustainability, 2020, vol. 12, art. 3624. DOI: 10.3390/su12093624.
- Yang Y., Yang J., Wu W.-M. et al. Biodegradation and mineralization of polystyrene by plastic-eating mealworms: part 2. Role of gut microorganisms. Environmental Science & Technology, 2015, vol. 49, pp. 12087–12093. DOI: 10.1021/acs.est.5b02663.