Lomberg B.S., Bazyleva O.A., Karashaev M.M., Letnikov M.N. Study of a high-temperature intermetallide matrix of the Ni–Al–Co system for producing structural alloys with increased plasticity (review) // Proceedings of VIAM. 2021. No. 9 (103). Ст. 01. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-9-3-10.

Study of a high-temperature intermetallide matrix of the Ni–Al–Co system for producing structural alloys with increased plasticity (review)

Lomberg B.S., Bazyleva O.A., Karashaev M.M., Letnikov M.N.
Abstract

A generalization of the results of scientific and technical publications is presented, the analysis of which will allow to develop scientific foundations for the creation of a new class of heat-resistant structural materials based on intermetallic matrices with increased plasticity at room temperature and high specific strength at temperatures up to 950 °C in the Ni–Al–Co system. It is shown that alloys of the Ni–Al–Co system can be used in the manufacture of rotary parts in the form of gas turbine engine discs (GTE), working at temperatures up to 950 °C, as well as materials for GTE blades due to heat resistance at temperatures up to 1200 °C.

Keywords
alloys of the Ni–Al–Co system, intermetallic high-temperature alloy, gas turbine engine, specific structural strength, thermomechanical treatment, metallurgy of granules.
Reference list
  1. Kablov E.N., Ospennikova O.G., Lomberg B.S. Strategic directions of development of structural materials and technologies for their processing for aircraft engines. Avtomaticheskaya svarka, 2013, no. 10, pp. 23–32.
  2. Ospennikova O.G. Strategy of development of hot strength alloys and steels special purpose, protective and heat-protective coverings Aviacionnye materialy i tehnologii, 2012, no. S, pp. 19–36.
  3. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  4. Bratukhin A.G., Shalin R.E., Kablov E.N., Toloraya V.N., Orekhov N.G. Cast monocrystalline turbine blades. Liteynoye proizvodstvo, 1993, no. 6, pp. 3–6.
  5. Bratukhin A.G., Kablov E.N., Toloraya V.N. Comparative analysis of materials and technological processes for obtaining monocrystalline turbine blades. Aviatsionnaya promyshlennost, 1995, no. 3, pp. 20–31.
  6. Kablov E.N. The main directions of development of materials for aerospace technology of the XXI century. Perspektivnye materialy, 2000, no. 3, pp. 27–36.
  7. Kablov E.N., Svetlov I.L., Petrushin N.V. Nickel heat-resistant alloys for casting blades with directional and single-crystal structure (Part II). Materialovedenie, 1997, no. 5, pp. 14–17.
  8. Kablov E.N., Svetlov I.L., Petrushin N.V. Nickel heat-resistant alloys for casting blades with directional and single-crystal structure (Part I). Materialovedenie, 1997, no. 4, pp. 32–39.
  9. Kablov E.N. Ways of increasing the heat resistance of nickel alloys. Metallurg, 2000, no. 4, pp. 26–28.
  10. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Casting heat-resistant nickel alloys for promising aircraft gas turbine engines. Tekhnologiya legkikh splavov, 2007, no. 2, pp. 6–16.
  11. Kablov E.N., Petrushin N.V., Elyutin E.S. Monocrystalline heat-resistant alloys for gas turbine engines. Vestnik MGTU im. N.E. Bauman, ser.: Mechanical engineering, 2011, no. SP2, pp. 38–52.
  12. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nickel foundry heat resisting alloys of new generation. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 36–52.
  13. Kornilov I.I. Physicochemical foundations of heat resistance of alloys. Moscow: AN SSSR, 1961, 561 p.
  14. Petrushin N.V., Ospennikova O.G., Elyutin E.S. Rhenium in single crystal nickel-based superalloys for gas turbine engine blades. Aviacionnye materialy i tehnologii, 2014, no. S5, pp. 5–16. DOI: 10.18577/2071-9140-2014-0-s5-5-16.
  15. Kablov E.N. VIAM: new generation materials for PD-14. Krylya rodiny, 2019, no. 7-8, pp. 54–58. 16. Kablov E.N. New generation materials – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  16. Kishkin S.T. Creation, research and application of heat-resistant alloys. Moscow: Nauka, 2006, 408 p.
  17. Kablov E.N., Bronfin M.B. The effect of S.T. Kishkina, or why the structure of heat-resistant alloys should be heterophase. Foundry heat-resistant alloys. The effect of S.T. Kishkina: On the occasion of the 100th anniversary of the birth of S.T. Kishkina: scientific and technical collection. Moscow: Nauka, 2006, 272 p.
  18. Kablov E.N., Ospennikova O.G., Bazyleva O.A. Materials for highly loaded parts of gas turbine engines. Vestnik MGTU im. N.E. Bauman, ser.: Mechanical engineering, 2011, no. SP2, pp. 13–19.
  19. History of aviation materials science. VIAM-80 years: years and people. Ed. E.N. Kablov. Moscow: VIAM, 2012, 520 p.
  20. Kablov E.N., Tolorajya V.N. VIAM – the founder of domestic casting technology of single-crystal turbine blades of GTE and GTU. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 105–117.
  21. Galieva E.V., Povarova K.B., Drozdov A.A., Valitov V.A. Structure and properties of solid-phase joints of wrought nickel alloy EP975 and monocrystalline intermetallic alloy VKNA-25, obtained by pressure welding with a degree of deformation of 24% under conditions of superplasticity of alloy EP975. Metally, 2018, no. 6, pp. 64–72.
  22. Garibov G.S. Scientific and technical groundwork in the field of granular metallurgy for the creation of advanced aircraft engines. Tekhnologiya legkikh splavov, 2018, no. 2, pp. 63–71.
  23. Gessinger G.Kh. Powder metallurgy of heat-resistant alloys. Chelyabinsk: Metallurgiya, 1988, 320 p.
  24. Garibov G.S. IN AND. Dobatkin and metallurgy of high-temperature nickel alloy granules. Tekhnologiya legkikh splavov, 2015, no. 2, pp. 34–39.
  25. Garibov G.S. Crystallization theory and technology of granulated heat-resistant nickel alloys. Tekhnologiya legkikh splavov, 2016, no. 1, pp. 107–118.
  26. Letnikov M.N., Lomberg B.S., Ovsepyan S.V. Investigation experimental alloys based on Ni–Al–Co ternary system for development a new high-temperature intermetallic alloy for disk application. Trudy VIAM, 2013, no. 10, paper no. 01. Available at: http://www.viam-works.ru (accessed: July 5, 2021).
  27. Kablov E.N., Bondarenko Yu.A., Echin A.B. Development of technology of cast superalloys directional solidification with variable controlled temperature gradient. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 24–38. DOI: 10.18577/2071-9140-2017-0-S-24-38.
  28. Kablov E.N., Petrushin N.V., Sidorov V.V. Rhenium in Nickel-Base Superalloys for Single Crystal gas turbine blades. 7th International Symposium on Technetium and Rhenium – Science and Utilization book of proceedings, 2011, p. 17.
  29. Kablov E.N., Ospennikova O.G., Sidorov V.V., Rigin V.E. Production of cast rod (charge) billets from modern high-heat-resistant nickel alloys foundry. Problems and prospects for the development of metallurgy and mechanical engineering with the use of completed fundamental research and R&D: Proceedings of Vseros. scientific and technical conf. Ekaterinburg, 2011, pp. 31–38.
  30. Kucheryaev V.V., Mironova N.A., Shishkov S.U. Research of technological features of Ni–Al–Co system ingots deformation. Trudy VIAM, 2016, no. 3 (39), paper no. 01. Available at: http://viam-works.ru (accessed: July 05, 2021). DOI: 10.18557/2307-6046-2016-0-3-1-1.
  31. Lomberg B.S., Ovsepjan S.V., Bakradze M.M., Letnikov M.N., Mazalov I.S. The application of new wrought nickel alloys for advanced gas turbine engines. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 116–129. DOI: 10.18577/2071-9140-2017-0-S-116-129.
  32. Povarova KB, Kazanskaya NK, Lomberg BS, Bondarenko Yu.A., Shkolnikov D.Yu. High-temperature structural (β + γ)-alloys based on NiAl with increased low-temperature plasticity. Metallurg, 1996, no. 5, pp. 13–20.
  33. Bannykh O.A., Povarova K.B. Intermetallic compounds – a new class of light heat-resistant and heat-resistant materials. Tekhnologiya legkikh splavov, 1992, no. 5, pp. 26–32.
  34. Povarova K.B., Lomberg B.S., Filin S.A., Kazanskaya N.K., Shkolnikov D.Yu., Bespalova M.D. Structure and properties of (β + γ)-alloys of the Ni – Al – Co system. Metally, 1994, no. 3, p. 77.
  35. Povarova K.B., Kazanskaya N.K., Lomberg B.S., Shkolnikov D.Yu., Filin S.A., Bespalova M.D. Phase composition and structure of alloys based on NiAl systems Ni – Al – Co – Me, where Me –Ti, Zr, Hf, V, Nb, Ta, Cr, Mo. Metally, 1996, no. 3, pp. 33.
  36. Povarova K.B., Lomberg B.S., Kazanskaya N.K., Drozdov A.A. Principles of creating structural alloys based on NiAl for high-temperature service. Problems of creating new materials for the aerospace industry in the XXI century: abstracts of interdisciplinary scientific and practical conf. (Moscow, June 25–26, 2002). Moscow: VIAM, 2002, p. 32.
  37. Kablov E.N. Formation of domestic space materials science. Vestnik RFFI, 2017, no. 3, pp. 97–105.
  38. Letnikov M.N., Lomberg B.S., Ospennikova O.G., Bakradze M.M. The influence of quench rate on microstructure and mechanical properties of nickel-based wrought superalloy VZh175-ID. Aviacionnye materialy i tehnologii, 2019, No. 2 (55), pp. 21–30. DOI: 10.18577/2071-9140-2019-0-2-21-30.
  39. Bazyleva O.A., Ospennikova O.G., Arginbaeva E.G., Letnikova E.Yu., Shestakov A.V. Development trends of nickel-based intermetallic alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 104–115. DOI: 10.18577/2071-9140-2017-0-S-104-115.
  40. Povarova K.B., Drozdov A.A., Bazyleva O.A., Morozov A.E., Antonova A.V., Bondarenko Yu.A., Bulakhtina M.A., Ashmarin A.A., Arginbaeva E.G., Aladiev N.A. Structural heat-resistant (NiAl + Ni3Al) alloys of the Ni – Al – Co system. I. Features of crystallization and structure of alloys. Metally, 2017, no. 5, pp. 20–30.
  41. Povarova K.B., Drozdov A.A., Bazyleva O.A., Morozov A.E., Antonova A.V., Bondarenko Yu.A., Bulakhtina M.A., Arginbaeva E.G., A.V. Amezhnov Influence of cobalt concentration and chromium alloying on the structure of heat-resistant (NiAl + Ni3Al + Ni) alloys of the Ni – Al – Co system. Metally, 2018, no. 4, pp. 50–55.
  42. Povarova K.B., Drozdov A.A., Bazyleva O.A., Morozov A.E., Antonova A.V., Arginbaeva E.G., Aladev N.A., Sirotinkin V.P. Structural heat-resistant (NiAl + Ni3Al) alloys of the Ni – Al – Co system. II. Oxidation. Metally, 2017, no. 5, pp. 31–36.
  43. Povarova K.B., Skachkov O.A., Drozdov A.A. and others. Powder alloys Fe – Cr – Al and NiAl. I. Obtaining powders. Zagotovitelnye proizvodstva v mashinostroyenii, 2017, vol. 15, no. 8, pp. 13–20.
  44. Logacheva A.I., Gusakov M.S., Sentyurina Zh.A. et al. Production of NiAl-based rod blanks for plasma centrifugal spraying using the method of mechanochemical synthesis. Metally, 2017, no. 3, pp. 84–93.
  45. Razuvaev E.I., Kapitanenko D.V., Sidorov S.A. Influence of structure and temperature-rate parameters during hot deformation of EP742 (KhN62BMKTYu) alloy. Kuznechno-shtampovochnoye proizvodstvo. Obrabotka materialov davleniyem, 2019, no. 2, pp. 22–30.
  46. Izakov I.A., Kapitanenko D.V., Sidorov S.A., Chebotareva E.S. Heating units for isothermal deformation. Part 1. Types of installations. Kuznechno-shtampovochnoye proizvodstvo. Obrabotka materialov davleniyem, 2019, no. 3, pp. 23–32.
  47. Izakov I.A., Kapitanenko D.V., Bubnov M.V., Bazhenov A.R. Investigation of the parameters of technological processes of isothermal deformation. Novosti materialovedeniya. Nauka i tekhnika, 2016, no. 5 (23), paper no. 4. Available at: http://materialsnews.ru (accessed: May 28, 2021).
  48. Izakov I.A., Kapitanenko D.V., Bubnov M.V., Nekrasov B.R. Thermomechanical foundations of isothermal deformation of metals under conditions of dynamic softening. Kuznechno-shtampovochnoye proizvodstvo. Obrabotka materialov davleniyem, 2015, no. 8, pp. 38–45.
  49. Razuvaev E.I., Moiseev N.V., Kapitanenko D.V., Skugorev A.V. Modern technologies of metal forming by pressure. Tekhnologiya legkikh splavov, 2015, no. 1, pp. 37–43.