Aleksandrov D.A., Budinovskiy S.A., Gorlov D.S. Development of functional ion-plasma coatings based on multilayer heterogeneous structures of metal nitrides // Proceedings of VIAM. 2021. No. 8 (102). Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-8-34-42.

Development of functional ion-plasma coatings based on multilayer heterogeneous structures of metal nitrides

Aleksandrov D.A., Budinovskiy S.A., Gorlov D.S.
Abstract

The article deals with the development of ion-plasma coating systems based on multilayer heterogeneous structures of the type (Me1)N/(Me2)N, (Me1–Me2)N/(Me3)N, (Me1–Me2–Me3)N/(Me4)N, where Me: Ti, Al, Cr, Mo. Tests for heat resistance and wear resistance, gas-abrasive resistance, metallographic and x-ray structural studies were carried out. It is shown that the ion-plasma coating (Ti–Al–Cr)N/CrN can be used to increase the heat resistance, wear resistance (including abrasive) of steel and titanium intermetallic parts of aircraft gas turbine engines operating in the temperature range up to 800 °C.

Keywords
heat resistance, wear resistance, ion-plasma coatings, wear-resistant coatings, titanium nitride, GTE blades.
Reference list
  1. Kablov E.N., Kashapov O.S., Pavlova T.V., Nochovnaya N.A. Development of a pilot industrial technology for the manufacture of semi-finished products from pseudo-alpha titanium alloy VT41. Titan, 2016, no. 2 (52). S. 33–42.
  2. Kablov E.N., Muboyadzhyan S.A. Erosion-resistant coatings for gas turbine engine compressor blades. Russian metallurgy (Metally), 2017, vol. 2017, no. 6, pp. 494–504.
  3. Kablov E.N., Bondarenko Yu.A., Kolodyazhny M.Yu., Surova V.A., Narskiy A.R. Prospects for the creation of high-temperature heat-resistant alloys based on refractory matrices and natural composites. Voprosy materialovedeniya, 2020, no. 4 (104). S. 64–78.
  4. Aleksandrov D.A. The research of wear-resistant coatings based on multicomponent titanium nitrides Trudy VIAM, 2020, no. 4-5 (88), paper no. 07 Available at: http://www.viam-works.ru (accessed: June 10, 2021). DOI: 10.18577 / 2307-6046-2020-0-45-62-69.
  5. Gorlov D.S., Zaklyakova O.V., Aleksan- drov D.A., Budinovskii S.A. Improving of fretting resistance intermetallic Ti2AlNb alloy. Trudy VIAM, 2021, no. 2 (96), paper no. 07. Available at: http://www.viam-works.ru (accessed: June 10, 2021). DOI: 10.18577/2307-6046-2021-0-2-62-70.
  6. Zhang M., Cheng Y., Xin L. et al. Cyclic oxidation behaviour of Ti/TiAlN composite multilayer coatings deposited on titanium alloy. Corrosion Science, 2020, no. 166, pp. 108476–108486. Available at: http://www.elsevier.com/locate/corsci (accessed: June 10, 2021). DOI: 10.1016/j.corsci.2020.108476.
  7. Alexandrov D.A., Gorlov D.S., Budinovskii S.A. Application of a complex of ion-plasma technologies to protect the compressor blades of a helicopter gas-turbine engine from erosion wear and fretting. Trudy VIAM, 2021, no. 2 (96), paper no. 08. Available at: http://www.viam-works.ru (accessed: June 10, 2021). DOI: 10.18577/2307-6046-2021-0-2-71-80.
  8. Grzesik W., Malecka J., Kwasny W. Identification of oxidation process of TiAlN coatings versus heat resistant aerospace alloys based on diffusion couples and tool wear tests. CIRP Annals – Manufacturing Technology, 2020, no. 69, pp. 41–44.
  9. Gromov V.I., Yakusheva N.A., Vostrikov A.V., Cherkashneva N.N. High strength structural steels for gas-turbine engine shafts (review). Aviation materials and technology, 2021. no. 1 (62). paper no. 01 Available at: http://www.journal.viam.ru (accessed: March 29, 2021). DOI: 10.18577/2713-0193-2021-0-1-3-12.
  10. Muboyadzhyan S.A. Erozionnostoykiye pokrytiya dlya lopatok kompressora GTD. Metally, 2009, no. 3, pp. 3–20.
  11. Vereschaka A.A., Grigoriev S.N. Study of cracking mechanisms in multi-layered composite nano-structured coatings. Wear, 2017, no. 378–379, pp. 43–57. Available at: http://www.elsevier.com/locate/wear (accessed: June 10, 2021). DOI: 10.1016/j.wear.2017.01.101.
  12. Xu Y.X., Riedl H., Holec D. et al. Thermal stability and oxidation resistance of sputtered Ti–Al–Cr–N hard coatings. Surface & Coatings Technology. 2017, no. 324, pp. 48–56. Available at: http://www.elsevier.com/locate/surfcoat (accessed: June 10, 2021). DOI: 10.1016/j.surfcoat.2017.05.053.
  13. Asanuma H., Polcik P., Kolozsvari S. et al. Cerium doping of Ti–Al–N coatings for excellent thermal stability and oxidation resistance. Surface & Coatings Technology, 2017, no. 326, pp. 165–172. Available at: http://www.elsevier.com/locate/surfcoat (accessed: June 10, 2021). DOI: 10.1016/j.surfcoat.2017.07.037.
  14. Sui X., Li G., Zhou H. et al. Evolution behavior of oxide scales of TiAlCrN coatings at high temperature. Surface & Coatings Technology, 2019, no. 360, pp. 133–139. Available at: http://www.elsevier.com/ locate/surfcoat (accessed: June 10, 2021). DOI: 10.1016/j.surfcoat.2019.01.016.
  15. Tillmann W., Grisales D., Stangier D. et al. Residual stresses and tribomechanical behaviour of TiAlN and TiAlCN monolayer and multilayer coatings by DCMS and HiPIMS. Surface & Coatings Technology, 2021, no. 406, pp. 126664–126675. Available at: http://www.elsevier.com/locate/surfcoat (accessed: June 10, 2021). DOI: 10.1016/j.surfcoat.2020.126664.
  16. Pilemalm R., Sjögren A. High pressure and high temperature behaviour of TiAlN coatings deposited on c-BN based substrates. Processing and Application of Ceramics, 2020, vol. 3, no. 14, pp. 210–217. DOI: 10.2298/PAC2003210P.
  17. Özkan D., Erarslan Y., Sulukan E. et al. Tribological behavior of TiAlN, AlTiN, and AlCrN coatings at boundary lubricating condition. Tribology Letters, 2018, no. 66, pp. 152–167. DOI: 10.1007/s11249-018-1111-1.
  18. Lin J., Zhang X., Ge F. et al. Thick CrN/AlN superlattice coatings deposited by hot filament assisted HiPIMS for solid particle erosion and high temperature wear resistance. Surface & Coatings Technology, 2019, no. 377, pp. 124922–124933. Available at: http:// www.elsevier.com/locate/surfcoat (accessed: June 10, 2021). DOI: 10.1016/j.surfcoat.2019.124922.