Vorobev N.N., Barinov D.Y., Zuev A.V., Pahomkin S.I. Computational and experimental study of the effective thermal conductivity of fibrous materials // Proceedings of VIAM. 2021. No. 7 (101). Ст. 10. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-7-95-102.

Computational and experimental study of the effective thermal conductivity of fibrous materials

Vorobev N.N., Barinov D.Y., Zuev A.V., Pahomkin S.I.
Abstract

The article is devoted to the evaluation of the effect of porosity on the effective thermal conductivity of thermal insulation materials. The main factors influencing the thermal conductivity of the material, such as density, the type of porous structure of the material and humidity, are considered. The method of measuring the thermal conductivity by the stationary heat flow method and the hot zone method is described. A method for calculating the effective thermal conductivity of fibrous materials is presented. A computational and experimental study of the effective thermal conductivity is carried out and the results are analyzed.

Keywords
thermal insulation materials, fibrous materials, porosity, thermal conductivity, heat transfer, heat flow.
Reference list
  1. Varrik N.M. Heat-resistant fibers and heat and sound insulating fireproof materials. Trudy VIAM, 2014, no. 6, paper no. 7. Available at: http://viam-works.ru (accessed: April 17, 2021). DOI: 10.18577/2307-6046-2014-0-6-7-7.
  2. Kablov E.N. New generation materials – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  3. Kablov E.N. Formation of domestic space materials science. Vestnik RFFI, 2017, no. 3, pp. 97–105.
  4. Raskutin A.E. Development strategy of polymer composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
  5. Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7-8, pp. 54–58.
  6. Aristova Е.Yu., Denisova V.А., Drozhzhin V.S. et al. Composite materials using hollow microspheres. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 52–57. DOI: 10.18577/2071-9140-2018-0-1-52-57.
  7. Kondrashov S.V., Shashkeev K.A., Petrova G.N., Mekalina I.V. Constructional polymer composites with functional properties. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 405–419. DOI: 10.18577/2071-9140-2017-0-S-405-419.
  8. Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
  9. Tikhonov V.B., Kolesnichenko M.P. Features of the use of modern polymer-based thermal insulation materials. Energobezopasnost i energosberezhenie, 2011, no. 1, pp. 24–27.
  10. Treshchalin M.Yu., Tyumenev Yu.Ya., Treshchalin A.V., Puzanova N.V. Design of nonwovens that reduce the technogenic impact on the environment (for example, geotextile fabrics). Moscow: PAIMS, 2001, 132 p.
  11. Tarasov V.A., Timofeev M.P., Ermakova Yu.V., Boyarskaya R.V. Analysis of the properties and features of the functioning of highly porous heat-insulating materials based on basalt fiber. Vestnik MGTU im. N.E. Bauman. Ser.: Mechanical engineering, 2013, no. 4, pp. 129.
  12. Yu.P. Gorlov Heat-insulating materials technology. Moscow: Stroyizdat, 1980, 396 p.
  13. Bolshakova N.V., Kostenok O.M. Thermal conductivity of basalt fiber materials. Refractories, 1995, vol. 36, pp. 331–332. DOI: 10.1007/BF02227481.
  14. Dulnev G.N., Zarichnyak Yu.P. Thermal conductivity of mixtures and composite materials. Leningrad: Energiya, 1974, 264 p.
  15. Timrot D.L. Determination of thermal conductivity of building and insulation materials. Moscow: Energoizdat, 1932, 120 p.
  16. Kaufman B.N. Thermal conductivity of building materials. Moscow: GILSA, 1955, 82 p.
  17. Chudnovsky A.F. Heat transfer in dispersed media. Moscow: GITSL, 1954, 444 p.
  18. Zhang B.-M., Zhao S.-Y., He X.-D. Experimental and theoretical studies on high-temperature thermal properties of fibrous insulation. Journal of Quantitative Spectroscopy and Radiative Transfer, 2008, vol. 109, pp. 1309–1324.
  19. Daryabeigi K. Heat Transfer in High-Temperature Fibrous Insulation. 8th AIAA/ASME Joint Thermophysics and Heat Transfer Conference. St. Louis, 2002. DOI: 10.2514/6.2002-3332.
  20. Wang M., Pan N. Predictions of effective physical properties of complex multiphase materials. Materials Science and Engineering, 2008, vol. 63, pp. 1–30.
  21. Zhou H., Zhang S., Yang M. The effect of heat-transfer passages on the effective thermal conductivity of high filler loading composite materials. Composites Science and Technology, 2007, vol. 67, pp. 1035–1040. DOI: 10.1016/j.compscitech.2006.06.004.
  22. MDS 41-7.2004. Methodology for assessing the effect of humidity on the efficiency of thermal insulation of equipment and pipelines. Moscow: Teploproekt., 2004. Available at: http://base1.gostedu.ru/44/44607 (accessed: April 17, 2021).
  23. Wang Q.L., Not J.H., Li Z.B. Fractional Model for Heat Conduction in Polar Bear Hairs. Thermal Science, 2021, vol. 16, is. 2, pp. 339–342.
  24. He J.-H. A New Fractal Derivation. Thermal Science, 2011, vol. 15, is. suppl. 1, pp. S145–S147. DOI: 10.2298/TSCI11S1145H.