Nikiforov A.A., Dyomin S.A., Khmeleva K.M. Electrochemical treatment of parts obtained by selective laser fusion // Proceedings of VIAM. 2021. No. 7 (101). Ст. 01. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-7-3-12.

Electrochemical treatment of parts obtained by selective laser fusion

Nikiforov A.A., Dyomin S.A., Khmeleva K.M.
Abstract

The use of additive technologies for the production of parts is one of the main trends in recent years in the field of industrial production. Application of the technology of «layer-by-layer growing» provides savings in materials, a significant reduction in labor intensity, and allows you to create parts of any complexity and configuration.

To reduce the surface roughness values of parts manufactured using additive technology, the authors proposed a method of electrochemical treatment in acid electrolytes, which makes it possible to achieve a decrease in surface roughness values by more than 5 times compared to the original one, and to process parts of any complexity and configuration.

Keywords
additive manufacturing, electrochemical machining, polishing, high-temperature nickel alloy, surface treatment, surface roughness.
Reference list
  1. Kablov E.N. Powders get rid of unnecessary things. Ekspert, 2014, no. 49 (926), pp. 46–51.
  2. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Kablov E.N., Evgenov A.G., Mazalov I.S., Shurtakov S.V., Zaitsev D.V., Prager S.M. Evolution of structure and properties of high-chromium heat-resistant alloy VZh159, obtained by selective laser alloying. Part I. Materialovedenie, 2019, no. 3, pp. 9–17. DOI: 10.31044/1684-579X-2019-0-3-9-17.
  4. Kablov E.N. Present and future of additive technologies. Metally Evrazii, 2017, no. 1, pp. 2–6.
  5. Grilikhes S.Ya. Electrochemical and Chemical Polishing: Theory and Practice. Influence on the property of metals. 2nd ed., Rev. Leningrad: Mashinostroyenie, 1987, pp. 17–19.
  6. Shluger M.A., Azhogin F.F., Efimov E.A. Corrosion and protection of metals. Moscow: Metallurgy, 1981, p. 216.
  7. Suslov A.G. The surface quality of the layer of machine parts. Moscow: Mashinostroenie, 2000, p. 320.
  8. Amirkhanova N.A., Khamzina A.R. Electrochemical polishing of heat-resistant nickel-chromium alloys KhN45MVTYuBR and KhN50VMTYuB. Metalloobrabotka, 2008, no. 1 (43), pp. 17–21.
  9. Grilikhes S.Ya. Electrochemical and chemical polishing. Moscow: Mashinostroenie, 1987, p. 27.
  10. Engineering of the surface of the part. Ed. A.G. Suslova. Moscow: Mashinostroenie, 2008, p. 42.
  11. Farafonov D.P., Leshchev N.E., Afanasiev-Khody- kin A.N., Artemenko N.I. Abrasive wear-resistant seal materials of the gas turbine engine flow section. Aviacionnye materialy i tehnologii, 2019, No. 3 (56), pp. 67–74. DOI: 10.18577/2071-9140-2019-0-3-67-74.
  12. Rassokhina L.I., Bityutskaya O.N., Gamazina M.V., Echin A.B. Technological process de-velopment of casting details «diffuser» for gas turbine engines from VZh159 superalloy in the conditions of the machine-building enterprise. Trudy VIAM, 2019, no. 12 (84), paper no. 03. Available at: http://www.viam-works.ru (accessed: July 11, 2021). DOI: 10.18577 / 2307-6046-2019-0-12-20-28.
  13. Bondarenko Yu.A. Trends in the development of high-temperature metal materials and technologies in the production of modern aircraft gas turbine engines. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 3–11. DOI: 10.18577/2071-9140-2019-0-2-3-11.
  14. Kablov E.N., Sidorov V.V., Kablov D.E., Min P.G., Rigin V.E. Resource-saving technologies for the smelting of promising casting and wrought superheat-resistant alloys taking into account the processing of all types of waste. Electrometallurgiya, 2016, no. 9, pp. 30–41.
  15. Gorbovets M.A., Belyayev M.S., Ryzhkov P.V. Fatigue strength of heat-resistant nickel alloys produced by selective laser melting. Aviaсionnye materialy i tehnologii, 2018, no. 3, pp. 50–55. DOI: 10.18577/2071-9140-2018-0-3-50-55.
  16. Loshchinin Yu.V., Pakhomkin S.I., Razmakhov M.G. Phase transformation temperatures and calorimetric analysis of powder compositions of nickel-based superalloys. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 79–85. DOI: 10.18577/2071-9140-2020-0-1-79-85.
  17. Kogaev V.P., Makhutov N.A., Gusenkov A.P. Calculations of machine parts and structures for strength and durability. Moscow: Mashinostroenie, 1983, p. 224.
  18. Shibaev B.A., Balmasov A.V. Electrochemical polishing of structural alloyed steels. Galvanotekhnika i obrabotka poverkhnosti, 2019, no. 2, pp. 24–25.
  19. Dontsov M.G., Balmasov A.V., Semenova N.V. Chemical and electrochemical copper polishing - similarities and differences. II. Influence of the surface of layers. Izvestiya vuzov, ser.: Khimiya i khimicheskaya tekhnologiya, 2008, vol. 51, no. 12, pp. 54–58.