Kravchenko D.V., Kozlov I.A., Nikiforov A.A. Methods for preparing the surface of aluminum alloys for electroplating (review) // Proceedings of VIAM. 2021. No. 6 (100). Ст. 09. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-6-82-99.

Methods for preparing the surface of aluminum alloys for electroplating (review)

Kravchenko D.V., Kozlov I.A., Nikiforov A.A.
Abstract

A review of modern scientific publications in the field of methods for preparing the surface of aluminum alloys for electroplating is presented. It is shown that the most widely used methods of preparation are: zinc treatment, high-porosity anodic oxidation and immersion nickel plating. A number of combined methods for preparing the surface of aluminum alloys for electroplating are given. Methods of direct application of electroplating coatings on aluminum and its alloys without the use of a sublayer, both by electrolytic and chemical methods, are considered.

Keywords
aluminum and its alloys, zinc treatment, immersion nickel, high-porosity anodi-zing, hypophosphite sublayer, combined preparation methods, direct copper plating of aluminum, direct nickel plating of aluminum.
Reference list
  1. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  2. Duyunova V.A., Volkova E.F., Uridiya Z.P., Trapeznikov A.V. Dynamics of the development of magnesium and cast aluminum alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 225–241. DOI: 10.18577/2071-9140-2017-0-S-225-241.
  3. Kablov E.N. What to make the future of? New generation materials, technologies for their creation and processing - the basis of innovations. Krylya Rodiny, 2016. no. 5. pp. 8–18.
  4. Kablov E.N., Antipov V.V., Oglodkova Yu.S., Oglodkov M.S. Experience and prospects of using aluminum-lithium alloys in aircraft and space technology. Metallurg, 2021. no. 1. pp. 62–70.
  5. Ogorodov D.V., Trapeznikov A.V., Popov D.A., Pentuykhin S.I. The development of casting heat-resistant aluminum alloys (To the 120th anniversary since the birth of I.F. Kolobnev). Trudy VIAM, 2017, no. 2 (50), paper no. 12. Available at: http://viam-works.ru (accessed: May 30, 2021). DOI: 10.18577/2307-6046-2017-0-2-12-12.
  6. Kablov E.N., Dynin N.V., Benarieb I., Shchetinina N.D., Samokhvalov S.V., Nerush S.V. Promising aluminum alloys for brazed structures of aviation technology. Zagotovitelnye proizvodstva v mashinostroyenii, 2021, vol. 19. no. 4, pp. 179–192.
  7. Vishenkov S.A. Chemical and electrochemical methods of metal coating deposition. Moscow: Mashinostroenie, 1975, 312 p.
  8. Khmeleva K.M., Kozlov I.A., Nikitin Ya.Yu., Nikiforov A.A. Modern trends of protective galvanic coatings working at high temperatures (review). Trudy VIAM, 2020, no. 12 (94), paper no. 07. Available at: http://www.viam-works.ru (accessed: May 30, 2021). DOI: 10.18577/2307-6046-2020-0-12-75-86.
  9. Mamaev V.I., Kudryavtsev V.N. Nickel plating: textbook. Moscow: RKhTU im. D.I. Mendeleeva, 2014, 192 p.
  10. Court S.W., Barker B.D., Walsh F.C. Electrochemical Measurements of Electroless Nickel Coatings on Zincated Aluminium Substrates. Transactions of the Institute of Metal Finishing, 2000, vol. 78. no. 4. pp. 157–162. DOI: 10.1080/00202967.2000.11871330.
  11. Mamaev V.I. Functional electroplating: textbook. Kirov: VyatSU, 2013, 208 p.
  12. Vijayanand M., Elansezhian R. Effect of Different Pretreatments and Heat Treatment on Wear Properties of Electroless Ni–B Coatings on 7075-T6 Aluminum Alloy. Procedia Engineering, 2014, vol. 97. pp. 1707–1717.
  13. Monteiro F.J., Barbosa M.A. Surface pretreatments of aluminum for electroplating. Surface and coatings technology, 1988, vol. 35. pp. 321–331.
  14. Sinyavsky V.S., Valkov V.D., Kalinin V.D. Corrosion and protection of aluminum alloys. Moscow: Metallugia, 1979, 224 p.
  15. Court S., Kerr C., Ponce de León C. et al. Monitoring of zincate pre-treatment of aluminium prior to electroless nickel plating. Transactions of the Institute of Metal Finishing, 2017, vol. 95. no. 2. pp. 97–105. DOI: 10.1080/00202967.2016.1236573.
  16. Pearson T., Wake S.J. Improvements in the Pretreatment of Aluminium as a Substrate for Electrodeposition. Transactions of the Institute of Metal Finishing, 1997, vol. 75. no. 3. pp. 93–97. DOI: 10.1080/00202967.1997.11871150.
  17. Pearson T. Pretreatment of aluminium for electrodeposition. Transactions of the Institute of Metal Finishing, 2006, vol. 84. no. 3. pp. 121–123.
  18. Electroplated aluminum parts and process for production: pat. US 6692630B2; filed 09.08.01; publ. 17.02.04.
  19. Vernik S., Pinner R. Chemical and electrolytic treatment of aluminum and its alloys. Leningrad: State union publishing house of shipbuilding industry, 1960, 389 p.
  20. Electroplated aluminium parts and process of production thereof: pat. CN 1498288A; filed 17.08.01; publ. 19.05.04.
  21. Robertson S.G., Ritchie I.M. The role of iron (III) and tartrate in the zincate immersion process for plating aluminium. Journal of Applied Electrochemistry, 1997, vol. 27 (7). pp. 799–804.
  22. Takács D., Sziráki L., Török T.I. et al. Effects of pre-treatments on the corrosion properties of electroless Ni–P layers deposited on AlMg2 alloy. Surface and Coatings Technology, 2007, vol. 201. pp. 4526–4535.
  23. Delaunois F., Petitjean J.P., Lienard P., Jacob-Duliere M. Autocatalytic electroless nickel-boron plating on light alloys. Surface and Coatings Technology, 2000, vol. 124. pp. 201–209.
  24. Thurlow K.P. Electroless nickel plating on aluminium connectors. Transactions of the Institute of Metal Finishing, 1989, vol. 67. no. 1. pp. 82–86. DOI: 10.1080/00202967.1989.11870847.
  25. Sharma A.K. Gold plating on aluminium alloys for space applications. Transactions of the Institute of Metal Finishing, 1989, vol. 67. no. pp. 87–88. DOI: 10.1080/00202967.1989.11870848.
  26. Electroplating on aluminium and its alloys: pat. GB 1007252A; filed 12.09.61; publ. 13.10.65.
  27. Wyszynski A.E. An Immersion Alloy Pretreatment for Electroplating on Aluminium. Transactions of the Institute of Metal Finishing, 1967, vol. 45. no. 1. pp. 147–154. DOI: 10.1080/00202967.1967.11870032.
  28. Burgess J. Electroplating onto aluminium and its alloys. Transactions of the Institute of Metal Finishing, 2019, vol. 97. no. 6. pp. 285–288. DOI: 10.1080/00202967.2019.1675280.
  29. Yin Z., Chen F. Effect of nickel immersion pretreatment on the corrosion performance of electroless deposited Ni–P alloys on aluminum. Surface and Coatings Technology, 2013, vol. 228. pp. 34–40.
  30. Laughton R.W. Recent Developments for Electroless Nickel Plating onto Aluminium, their Basis and Implications. Transactions of the Institute of Metal Finishing, 1992, vol. 70. no. 3, pp. 120–122. DOI: 10.1080/00202967.1992.11870957.
  31. State Standart 9.305–84. Unified system of protection against corrosion and aging. Metallic and non-metallic inorganic coatings. Operations of technological processes for obtaining coatings (with Amendments No. 1, 2, with Amendment). Moscow: Publishing house of standards, 2003. 105 p.
  32. Arrowsmith D.J., Clifford A.W., Moth D.A. Phosphoric acid anodizing of aluminium. Transactions of the Institute of Metal Finishing, 1985, vol. 63. no. 1. pp. 41–46. DOI: 10.1080/00202967.1985.11870704.
  33. Devyatkina T.I., Luchneva S.I., Vasin E.N. et al. Surface preparation of aluminum alloys for electroplating. Journal of Applied Chemistry, 2020, vol. 93, is. 9, pp. 1323–1331.
  34. Digby R.P., Paekham D.E. Pretreatment of aluminium: topography, surface chemistry and adhesive bond durability. International Journal Adhesion and Adhesives, 1995, vol. 15. pp. 61–71.
  35. Spooner R.C., Seraphim D.P. Phosphoric Acid Anodizing of Aluminium and its Application to Electroplating. Transactions of the Institute of Metal Finishing, 1954, vol. 31. no. 1. pp. 29–51. DOI: 10.1080/00202967.1954.11869627.
  36. Yazdi S.S., Ashrafizadeh F., Hakimizad A. Improving the grain structure and adhesion of Ni–P coating to 3004 aluminum substrate by nanostructured anodic film interlayer. Surface and Coatings Technology, 2013, vol. 232. pp. 561–566.
  37. Ali H.O., Christie I.R.A. Electroplating on Aluminium Wire. Transactions of the Institute of Metal Finishing, 1983, vol. 61. no. 1. pp. 67–71. DOI: 10.1080/00202967.1983.11870641.
  38. Latha N., Raj V., Selvam M. Effect of plating time on growth of nanocrystalline Ni–P from sulphate/glycine bath by electroless deposition method. Bulletin Materials Science, 2013, vol. 36. no. 4. pp. 719–727.
  39. Kocabaşa M., Örnekd C., Curionie M., Canseverc N. Nickel fluoride as a surface activation agent for electroless nickel coating of anodized AA1050 aluminum alloy. Surface and Coatings Technology, 2019, vol. 364. pp. 231–238.
  40. Skopintsev V.D., Vinokurov E.G. Theoretical and applied aspects of autocatalytic formation of coatings based on nickel-phosphorus alloy. Moscow: VINITI RAN: RKhTU im. D.I. Mendeleeva, 2018, 228 p.
  41. Sallee N., Cromer M., Vittori O. Electroplating of Copper on Aluminium with Direct and Pulsed Currents. Canadian Metallurgical Quarterly, 1994, vol. 33. no. 2. pp. 155–162. DOI: 10.1179/cmq.1994.33.2.155.
  42. ASTM B253-11. Preparation of Aluminum Alloys for Electroplating. ASTM, 2007. Available at: http://www.ru.scribd.com (accessed: May 17, 2021).