Malinina G.A., Denisova V.S., Solntsev St.S., Vaganova M.L. Investigation of the effect of oxide additives on the properties of heat-resistant glass-crystal coating // Proceedings of VIAM. 2021. No. 5 (99). Ст. 09. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-5-87-95.

Investigation of the effect of oxide additives on the properties of heat-resistant glass-crystal coating

Malinina G.A., Denisova V.S., Solntsev St.S., Vaganova M.L.
Abstract

Experimental compositions of coatings based on SiO2–Al2O3–MgO matrix glass and modifying additives are considered. A number of refractory metal oxides were selected as modifying additives. The influence of these additives on the properties of the coating melt, such as the spreadability and the wetting edge angle, as well as the oxidability of the resulting compositions, is studied. It was found that the experimental coating modified with aluminum oxide has the best protective properties. The introduction of modifying additives in quantities of more than 5 % is considered inappropriate.

Keywords
glass-crystal coatings, aluminum oxide, heat resistance, melt, spreadability, wettability.
Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Ospennikova O.G., Podieiachev V.N., Stoliankov Yu.V. Refractory alloys for innovative equipment. Trudy VIAM, 2016, no. 10, paper no. 5. Available at: http://www.viam-works.ru (accessed: February 18, 2021). DOI: 10.18577/2307-6046-2016-0-10-5-5.
  3. Kablov E.N. The role of chemistry in the creation of new generation materials for complex technical systems. Reports of XX Mendeleev Congress on General and Applied Chemistry. Ekaterinburg: Ural Branch of the Russian Academy of Sciences, 2016, pp. 25–26.
  4. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  5. Kashin D.S., Dergacheva P.E., Stekhov P.A. Heat resistant slurry coatings (review). Trudy VIAM, 2018, no. 5 (65), paper no. 08. Available at: http://www.viam-works.ru (accessed: February 18, 2021). DOI: 10.18577/2307-6046-2018-0-5-64-75.
  6. Kablov E.N., Grashchenkov D.V., Isaeva N.V., Solntsev S.S. Promising high-temperature ceramic composite materials. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, no. 1, pp. 20–24.
  7. Solntsev S.S. Protective technological coatings and refractory enamels. Moscow: Mashinostroenie, 1984, 256 p.
  8. Kablov E.N., Evgenov A.G., Ospennikova O.G., Semenov B.I., Semenov A.B., Korolev V.A. Metal-powder compositions of EP648 heat-resistant alloy produced by FSUE «VIAM» State Scientific Center of the Russian Federation in technologies of selective laser alloying, laser gas-powder surfacing and high-precision casting of polymers filled with metal powders. Izvestiya vysshikh uchebnykh zavedeniy, ser.: Mashinostroyenie, 2016, no. 9, pp. 62–80. DOI: 10.18698/0536-1044-2016-9-62-80.
  9. Evgenov A.G., Gorbovec M.A., Prager S.M. Structure and mechanical properties of heat resistant alloys VZh159 and EP648, prepared by selective laser fusing. Aviacionnye materialy i tehnologii, 2016, no. S1, pp. 8–15. DOI: 10.18577/2071-9140-2016-0-S1-8-15.
  10. Zhitnyuk S.V. Effect of sintering additives on the properties of silicon carbide-based ceramics (review). Trudy VIAM, 2019, no. 3 (75), paper no. 09. Available at: http://www.viam-works.ru (accessed: February 18, 2021). DOI: 10.18577/2307-6046-2019-0-3-79-86.
  11. Biryukova A.A., Dzhienalyev T.D., Boronina A.V. et al. Influence of modifying additives on the synthesis and properties of cordierite-mullite ceramics from raw materials of Kazakhstan. Nauchnye issledovaniya i razrabotki, 2017, no. 3, pp. 148–152.
  12. Lysenko V. Ceramics from magnesium oxide nanopowder: creation and properties. Nanoindustriya, 2016, no. 4, pp. 94–97. DOI: 10.22184/1993-8578.2016.66.4.94.97.
  13. Vitkalova I.A., Torlova A.S., Pikalov E.S. Influence of lanthanum oxide on the properties of chemically resistant ceramics obtained using galvanic sludge. Mezhdunarodniy nauchno-issledovatelskiy zhurnal, 2019, no. 10 (88), pp. 35–39.
  14. Alekseev R.O., Savinkov V.I., Sigaev V.N. Optical glasses with high values of refractive index and dispersion. Uspekhi v khimii i khimicheskoy tekhnologii, 2018, vol. XXXII, no. 2, pp. 34–36.
  15. Chakraborty I.N., Shelby J.E., Condrate R.A. Properties and structure of lanthanum borate glasses. Journal of the American Ceramic Society, 1984, vol. 67, no. 12, pp. 782–785.
  16. Betekhin A.G. Mineralogy course. Moscow: Book House «Universitet», 2007. 721 p.
  17. Baraz V.R., Levchenko V.P., Povzner A.A. The structure and physical properties of crystals: textbook. Ekaterinburg: USTU-UPI, 2009, 164 p.