Minibaev M.I., Usacheva M.N., Dyshenko V.S., Goncharov V.A. A device and tool for making sample from polymer composite materials on a CNC machine (review) // Proceedings of VIAM. 2021. No. 4 (98). Ст. 08. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-4-100-109.

A device and tool for making sample from polymer composite materials on a CNC machine (review)

Minibaev M.I., Usacheva M.N., Dyshenko V.S., Goncharov V.A.
Abstract

The article discusses devices for fixing sheet metal blanks from PCM: a perforated vacuum table, its design features, advantages and disadvantages. Based on these data, the upper part of the vacuum table was made for cutting samples for Iosipescu tests and dielectric tests. The article describes various types of tools for PCM processing and an experiment on the wear resistance of a diamond-like coated rasp cutter when milling carbon fiber reinforced plastic, carried out by foreign researchers.

Keywords
machining, milling, polymer composite material, vacuum table, cutting tool, numerical control machine, defects.
Reference list
  1. Onishchenko G.G., Kablov E.N., Ivanov V.V. Scientific and technological development of Russia in the context of achieving national goals: problems and solutions. Innovatsii, 2020, no. 6 (260), pp. 3–16.
  2. Kablov E.N. New Generation Materials and Technologies for their Digital Processing. Herald of the Russian Academy of Sciences, 2020, vol. 90, no. 2, pp. 225–228.
  3. Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7-8, pp. 54–58.
  4. Kablov E.N. New generation materials and digital technologies for their processing. Bulletin of the Russian Academy of Sciences, 2020, vol. 90, no. 4, pp. 331–334.
  5. Draft order of the Government of the Russian Federation «On approval of the Strategy for the development of the aviation industry of the Russian Federation for the period up to 2030». Available at: https://www.minpromtorg.gov.ru (accessed: December 1, 2020).
  6. Minibaev M.I., Raskutin A.E, Goncharov V.A. Peculiarities of technology production specimens of PCM on CNC machines (review). Trudy VIAM, 2019, no. 1 (73), paper no. 11. Available at: http://www.viam-works.ru (accessed: December 2, 2020). DOI: 10.18577/2307-6046-2019-0-1-105-114.
  7. Ozkan D., Sabri Gok M., Oge M., Cahit Karaoglanli A. Milling Behavior Analysis of Carbon Fiber-Reinforced Polymer (CFRP) Composites. Materials Today: Proceedings, 2019, vol. 11, pp. 526–533.
  8. Kondrashov S.V., Shashkeev K.A., Petrova G.N., Mekalina I.V. Constructional polymer composites with functional properties. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 405–419. DOI: 10.18577/2071-9140-2017-0-S-405-419.
  9. Kutsevich K.E., Tyumeneva T.Yu., Petrova A.P. Influence of fillers on properties of adhesive prepregs and PCM on their basis. Aviacionnye materialy i tehnologii, 2017, no. 4 (49), pp. 51–55. DOI: 10.18577/2071-9140-2017-0-4-51-55.
  10. Ilichev A.V., Gubin A.M., Akmeev A.R., Ivanov N.V. Definition of area of the maxi-mum shear deformations for CFRP samples on Iosipescu method, with use of optical system of measurements. Trudy VIAM, 2018, no. 6 (66), paper no. 10. Available at: http://www.viam-works.ru (accessed: December 1, 2020). DOI: 10.18577/2307-6046-2018-0-6-99-109.
  11. Zastrogina O.B., Serkova E.А., Sarychev I.A., Vavilova M.I. Influence of Russian and Chinese vinyflex on the properties of the VFT binder and fiberglass based on it. Aviacionnye materialy i tehnologii, 2020, no. 3 (60), pp. 3–9. DOI: 10.18577/2071-9140-2020-0-3-3-9.
  12. ASTM D5379/D5379M-19. Standard Test Method for Shear Properties of Composite Materials by the V-Notched Beam Method. ASTM International, West Conshohocken, 2019. Available at: http://astm.org (accessed: accessed: December 1, 2020). DOI: 10.1520/D5379_D5379M-19.
  13. Thakur R.K., Singh K.K., Karumesh K. Investigation of milling characteristics in grapheme-embedded epoxy/carbon fiber reinforced composite. Materials Today: Proceedings, 2020, vol. 33, pp. 5643–5648.
  14. Aristova Е.Yu., Denisova V.А., Drozhzhin V.S. et al. Composite materials using hollow microspheres. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 52–57. DOI: 10.18577/2071-9140-2018-0-1-52-57.
  15. Gao C., Xiao J., Xu J., Ke Y. Factor analysis of machining parameters of fiber-reinforced polymer composites based on finite element simulation with experimental investigation. International Journal of Advanced Manufacturing Technology, 2016, vol. 83, is. 5-8, pp. 1113–1125. DOI: 10.1007/s00170-015-7592-2.
  16. Vorobyov V.V. Manufacturing technology of structures from composite materials. Moscow: MAI Publishing House, 1996, 178 p.