Konokotin S.P., Nazarkin R.M. The influence of interstitial impurities in the Zr–Y target alloys on the heat resisting ceramic coating quality // Proceedings of VIAM. 2021. No. 2 (96). Ст. 06. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-2-52-61.

The influence of interstitial impurities in the Zr–Y target alloys on the heat resisting ceramic coating quality

Konokotin S.P., Nazarkin R.M.
Abstract

The influence of interstitial impurities in the Zr–Y target alloys (manufactured by two different techniques) on the quality of thermal barrier ceramic layers of heat resisting coating are studied in this work. The heat resisting ceramic coating manufactured in the UOKS-2 devices by magnetron medium-feculence plasma–chemical deposition on the surface of components that are used at the high temperatures (above 1150 °C). It was found that when the content of interstitial impurities in the target alloy is more than 0,1% (1000 ppm), the rate of the coating process decreases and has to be maintained by increasing the energy of argon ions. This leads to overheating of the target alloy and the surface of the parts (substrate) which impairs the adhesion of the deposited atoms.

Keywords
Zr–Y alloy, heat resisting ceramic coatings, interstitial impurities, x-ray diffraction analysis, phase analysis, metallography, crystal lattice periods.
Reference list
  1. Kablov E.N., Muboyadzhyan S.A. Ion-plasma protective coatings for gas turbine engine blades. Litye lopatki gazoturbinnykh dvigateley: splavy, tekhnologii, pokrytiya. Moscow: Nauka, 2006, pp. 531–608.
  2. Sudhangshu B. High Temperature Coatings. Oxford: Butterworth-Heinemann, 2018, 416 p.
  3. Kablov E.N., Muboyadzhyan S.A., Budinovsky S.A., Galoyan A.G., Lutsenko A.N. Protective and hardening coatings of blades and GTE parts. 75 years. Aviation materials. Moscow: VIAM, 2007, pp. 107–124.
  4. Bakan E., Vassen R. Ceramic Top Coats of Plasma – Sprayed Thermal Barrier Coatings: Materials, Processes, and Properties. Journal of Thermal Spray Technology, 2017, vol. 26, pp. 992–1010.
  5. Sergeev V.P., Neifeld V.V., Sungatulin A.R. et al. Increase in thermal cycling resistance of coatings based on Zr–Y–O obtained by magnetron deposition. Izvestiya Tomskogo politekhnicheskogo universiteta, 2010, vol. 317, no. 3, pp. 111–115.
  6. Chubarov D.A., Budinovskij S.A., Smirnov A.A. Magnetron sputtering method for applying ceramic layers for thermal barrier coatings. Aviacionnye materialy i tehnologii, 2016, No. 4 (45), pp. 23–30. DOI: 10.18577/2107-9140-2016-0-4-23-30.
  7. Chubarov D.A., Budinovskij S.A. Choosing ceramic materials for thermal barrier coating of GTE turbine blades on working temperatures up to 1400°С. Trudy VIAM, 2015, no. 4, paper no. 7. Available at: http://viam-works.ru (accessed: September 17, 2020). DOI: 10.18577/2307-6046-2015-0-4-7-7.
  8. Muboyadzhyan S.A., Budinovskij S.A. Ion-plasma technology: prospective processes, coatings, equipment. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 39–54. DOI: 10.18577/2071-9140-2017-0-S-39-54.
  9. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  10. Muboyadzhyan S.A., Lesnikov V.P., Kuznetsov V.P. Complex protective coatings for turbine blades of aircraft gas turbine engines. Ekaterinburg: Kvist, 2008, 208 p.
  11. Gorelik S.S., Skakov Yu.A., Rastorguev L.N. X-ray and electron-optical analysis: textbook. manual for universities. 4th ed., add. and rev. Moscow: MISiS, 2002, 360 p.
  12. Nolze G. PowderCell: instruction manual. Berlin: Federal Institute for Materials Research and Testing, 2017, 45 p.
  13. Dukhopelnikov D.V. Magnetron spray systems: textbook in 2 parts. Moscow: Publ. house of Bauman MSTU, 2014. Part 1: Device, principles of operation, application, pp. 31–35.
  14. Samsonov G.V., Borisova A.L., Zhidkova T.G. et al. Physico-chemical properties of oxides: handbook. Moscow: Metallurgiya, 1978, 472 p.
  15. Budinovsky S.A., Stekhov P.A., Doronin O.N., Artemenko N.I. Main mechanisms of destruction of the ceramic layer of thermal barrier coatings (review). Trudy VIAM, 2019, no. 2 (74), paper no. 11. Available at: http://www.viam-works.ru (accessed: August 11, 2020). DOI: 10.18577/2307-6046-2019-0-2-105-112.