Gulyaev I.N., Zelenina I.V., Valevin E.O., Khaskov M.A. Influence of climatic ageing on the properties of high-temperature carbon fiber reinforced plastics // Proceedings of VIAM. 2021. No. 2 (96). Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-2-39-51.

Influence of climatic ageing on the properties of high-temperature carbon fiber reinforced plastics

Gulyaev I.N., Zelenina I.V., Valevin E.O., Khaskov M.A.
Abstract

Presentsthe  results of of research of the properties of a series of high-temperature carbon plastics based on phthalonitrile resin after long-term exposure in various climatic zones: temperate climate, moderately warm climate with mild winters, warm humid climate, very cold climate are presented. The state of the surface of carbon fiber reinforced plastics has been investigated, their thermal stability and water absorption have been determined. After exposure, CFRPs showed high retention of properties from the level of the initial values: 80–90% at room temperature of tests and 60–75% at a temperature of 300 °С.

Keywords
high-temperature carbon plastics, phthalonitrile resin, climatic zones, strength characteristics, water absorption.
Reference list
  1. Kablov E.N. New generation materials – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  2. Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  3. Kablov EN, Kirillov VN, Zhirnov AD, Startsev OV, Vapirov Yu.M. Centers for climatic testing of aviation PCM. Aviatsionnaya promyshlennost, 2009, no. 4, pp. 36–46.
  4. Aviation materials: reference book: in 13 vols. Ed. E.N. Kablov. 7th ed., rev. and add. Moscow: VIAM, 2015, vol. 13: Climatic and microbiological resistance of non-metallic materials, 270 p.
  5. Kablov E.N., Startsev O.V. The basic and applied research in the field of corrosion and ageing of materials in natural environments (review). Aviacionnye materialy i tehnologii, 2015, no. 4 (37), pp. 38–52. DOI: 10.18577/2071-9140-2015-0-4-38-52.
  6. Kablov E.N., Startsev V.O. Climatic aging of polymer composite materials for aviation purposes. I. Assessment of the influence of significant factors of influence. Deformatsiya i razrusheniye materialov, 2019, no. 12, pp. 7–16.
  7. Kablov E.N., Startsev V.O. Climatic aging of polymer composite materials for aviation purposes. II. Development of research methods for the early stages of aging. Deformatsiya i razrusheniye materialov, 2020, no. 1, pp. 15–21.
  8. Kablov E.N., Startsev V.O., Inozemtsev A.A. The moisture absorption of structurally similar samples from polymer composite materials in open climatic conditions with application of thermal spikes. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 56–68. DOI: 10.18577/2071-9140-2017-0-2-56-68.
  9. Laptev A.B., Barbotko S.L., Nikolaev E.V. The main research areas of the persistence properties of materials under the influence of climatic and operational factors. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 547–561. DOI: 10.18577/2071-9140-2017-0-S-547-561.
  10. Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7-8, pp. 54–58.
  11. Kablov E.N., Skibin V.A., Abuzin Yu.A., Kochetov V.N., Shavnev A.A., Karimbaev T.D., Luppov A.A. Wide-chord fan blades for turbofan engines of 5–6 generations. Konversiya v mashinostroyenii, 2006, no. 5, pp. 5–16.
  12. Mekham M. Snecma and her partner AEC create a new technology for the manufacture of composite blades. Aviatransportnoe obozrenie, 2012, no. 131. Available at: http://www.ato.ru/content/ snecma-i-ee-partner-aec-sozdayut-novuyu-tehnologiyu-izgotovleniya-kompozitnyh-lopatok (accessed: November 17, 2020).
  13. Novikov A.S., Karimbaev T.D., Luppov A.A., Afanasyev D.V., Mezentsev M.A. Innovations in the use of composite materials in aircraft engines. Dvigatel, 2015, no. 2 (98), pp. 6–9.
  14. Novikov A.S., Karimbaev T.D. Rotor blades of high bypass fans for promising turbojet engines. Dvigatel, 2015, no. 5 (101), pp. 6–11.
  15. High temperature plastics market by type (polysulfones, polyimides, polyphenylene sulfide, fluoropolymers, and others), by end-use industries (electrical & electronic, transportation, industrial, medical, and others) – Global trends & forecast to 2019. Available at: https://www.marketsandmarkets.com/Market-Reports/high-temperature-plastics-market-1192.html (accessed: November 17, 2020).
  16. Kurnosov A.O., Raskutin A.E., Mukhametov R.R., Melnikov D.A. Polymer composite materials based on thermosetting polyimide binders. Voprosy materialovedeniya, 2016, no. 4, pp. 50–62.
  17. Kuznetsov A.A., Semenova G.K. Promising high-temperature thermosetting binders for polymer composite materials. Rossiyskiy khimicheskiy zhurnal, 2010, vol. 53, no. 4, pp. 86–96.
  18. Zelenina I.V., Gulyayev I.N., Kucherovskiy A.I., Mukhametov R.R. Heat-resistant CFRP for the impulse wheel of the centrifugal compressor. Trudy VIAM, 2016, no. 2 (38), paper no. 08. Available at: http://www.viam-works.ru (accessed: November 6, 2020). DOI: 10.18577/2307-6046-2016-0-2-8-8.
  19. Nikolaev E.V., Barbotko S.L., Andreeva N.P., Pavlov M.R., Grashchenkov D.V. Complex research of influence of climatic and operational factors on new generation epoxy binding and polymeric composite materials on its basis. Part 4. Natural climatic tests of polymeric composite materials on the basis of epoxy matrix. Trudy VIAM, 2016. no. 6, paper no. 11. Available at: http://www.viam-works.ru (accessed: November 6, 2020). DOI: 10.18577/2307-6046-2016-0-6-11-11.
  20. Gladkikh A.V., Kurs I.S., Kurs M.G. Analysis of the data of full-scale climatic tests combined with the application of operational factors of nonmetallic materials (review). Trudy VIAM, 2018, no. 10 (70), paper no. 09. Available at: http://www.viam-works.ru (accessed: November 06, 2020). DOI: 10.18577/2307-6046-2018-0-10-74-82.
  21. Deev I.S., Kurshev E.V., Lonsky S.L., Zhelezina G.F. The influence of long-term climatic aging on the surface microstructure of epoxy organoplastics and the nature of its destruction under bending conditions. Voprosy materialovedeniya, 2016, no. 3 (87), pp. 104–114.
  22. Startsev V.O. Climatic resistance of polymer composite materials and protective coatings in a moderately warm climate: thesis, Dr. Sc. (Tech.). Moscow: VIAM, 2018, 308 p.
  23. Valevin E.O. Influence of heat and humidity impact on the properties of heat-resistant polymer composite materials based on phthalonitrile matrix: thesis, Cand. Sc. (Tech.). Moscow: MAI, 2018. 130 p.
  24. Valevin E.O., Zelenina I.V., Shvedkova A.K., Gulyaev I.N. Thermal aging of heat-resistant carbon plastics. Voprosy materialovedeniya, 2015, no. 4 (84), pp. 91–99.
  25. Gulyaev I.N., Zelenina I.V., Valevin E.O., Shvedkova A.K. Investigation of the influence of increased temperature and humidity on the properties of heat-resistant carbon plastics. Konstruktsii iz kompozitsionnykh materialov, 2015, no. 3 (139), pp. 55–61.
  26. Valevin E.O., Startsev V.O., Zelenina I.V. Thermal aging, surface degradation and water transfer in carbon fiber reinforced plastic VKU-38TR. Trudy VIAM, 2020, no. 6–7 (89), paper no. 12. Available at: http://www.viam-works.ru (accessed: November 06, 2020). DOI: 10.18577/2307-6046-2020-0-67-118-128.
  27. Panin P.V. Investigation of changes in surface relief and moisture transfer in polymer composite materials in the process of climatic aging: thesis, Cand. Sc. (Tech.). Moscow: VIAM, 2015, 131 p.
  28. Nikolaev E.V., Kirillov V.N., Skirta A.A., Grashhenkov D.V. Study of moisture transport rules and development of a standard on measurement of the diffusion coefficient and moisture content limit to evaluate mechanical properties of carbon fiber reinforced plastics. Aviacionnye materialy i tehnologii, 2013, no. 3, pp. 44–48.
  29. Laptev A.B., Barbotko S.L., Nikolaev E.V., Skirta A.A. Statistical processing of the results of climatic tests of fiberglass. Plasticheskiye massy, 2016, no. 3–4, pp. 58–64.