Barbotko S.L., Bochenkov M.M., Volnyj O.S., Korobeinichev O.P., Shmakov A.G. Evaluation of the effectiveness of the fire retardants, promising for the creation of new polymer composite materials intended for aviation techniques // Proceedings of VIAM. 2021. No. 2 (96). Ст. 03. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-2-20-29.

Evaluation of the effectiveness of the fire retardants, promising for the creation of new polymer composite materials intended for aviation techniques

Barbotko S.L., Bochenkov M.M., Volnyj O.S., Korobeinichev O.P., Shmakov A.G.
Abstract

Studies have been carried out on the effectiveness of the action of two types of fire retardants – graphene and an organic phosphorus-containing compound DOPO-THPO, introduced into an epoxy resin. The amount of fire retardants introduced was 0; 2 and 4% of the amount of epoxy resin. The efficiency was assessed by the oxygen index method (LOI). It was shown that for this epoxy resin, the introduction of graphene provided an increase in the oxygen index from 21 to 27%, and the introduction of the phosphorus-containing fire retardant DOPO-THPO – from 21 to 23%. With the simultaneous introduction of graphene (3%) and DOPO-THPO (1%), it was possible to achieve an increase in the oxygen index up to 28%.

Keywords
fire safety, flammability, limited oxygen index, polymeric material, aircraft material, epoxy resin, fire test.
Reference list
  1. Airworthiness standards for transport category aircraft: AP-25: approved. 5th ed. Moscow: Aviaizdat, 2015, 288 p.
  2. Airworthiness Standards: Transport Category Airplanes: Part 25. Electronic Code of Federal Regulation. Title 14: Aeronautic and Space. Chapter 1. Subchapter C. Available at: https://www.ecfr.gov/cgi-bin/text-idx?SID=9091f0ebbfbf1539cdb87015908ad369&mc=true&node=pt14.1.25&rgn=div5 (дата обращения: 01.12.2020).
  3. Barbotko S.L., Volny O.S., Kirienko O.A., Shurkova E.N. Assessment of fire safety of polymer materials for aviation purposes: state analysis, test methods, development prospects, methodological features. Ed. E.N. Kablov. Moscow: VIAM, 2018, 424 p.
  4. Raskutin A.E. Development strategy of polymer composite materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
  5. Kondrashov S.V., Shashkeev K.A., Petrova G.N., Mekalina I.V. Constructional polymer composites with functional properties. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 405–419. DOI: 10.18577/2071-9140-2017-0-S-405-419.
  6. Kablov E.N. Marketing of materials science, aircraft construction and industry: present and future. Direktor po marketingu i sbytu, 2017, no. 5-6, pp. 40–44.
  7. Korobeinichev O.P., Gonchikzhapov M.B., Paletsky A.A. et al. Structure of counterflow flame of ultrahigh-molecular-weight polyethylene with and without triphenylphosphate. Proceedings of the Combustion Institute, 2017, vol. 36 (2), p. 3279–3286. DOI: 10.1016/j.proci.2016.06.117.
  8. Korobeinichev O.P., Gonchikzhapov M.B., Paletsky A.A. et al. Counterflow flames of ultrahigh-molecular-weight polyethylene with and without triphenylphosphate. Combustion and Flame, 2016, vol. 169, pp. 261–271. DOI: 10.1016/j.combustflame.2016.04.019.
  9. Korobeinichev O.P., Trubachev S.A., Joshi A.K. et al. Experimental and numerical studies of downward flame spread over PMMA with and without addition of tri phenyl phosphate. Proceedings of the Combustion Institute. 2020. Available at: https://www.sciencedirect.com/science/article/abs/pii/S1540748920305320 (accessed: December 14, 2020). DOI: 10.1016/j.proci.2020.07.082.
  10. Trubachev S.A., Korobeinichev O.P., Karpov A.I. et al. The effect of triphenyl phosphate inhibition on flame propagation over cast PMMA slabs. Proceedings of the Combustion Institute. 2020. Available at: https://www.sciencedirect.com/science/article/abs/pii/S1540748920300912 (accessed: December 14, 2020). DOI: 10.1016/j.proci.2020.05.043.
  11. Ma S., Xiao Y., Zhou F. et al. Effects of novel phosphorus-nitrogen-containing DOPO derivative salts on mechanical properties, thermal stability and flame retardancy of flexible polyurethane foam. Polymer Degradation and Stability. 2020, vol. 177, art. No. 109160. DOI: 10.1016/j.polymdegradstab.2020.106160.
  12. Jayarama Krishna J.V., Srivatsa Kumar S., Korobeinichev O.P., Vinu R. Detailed kinetic analysis of slow and fast pyrolysis of poly(methyl methacrylate)-Flame retardant mixtures. Thermochimica Acta, 2020, vol. 687. Art. No. 178545. DOI: 10.1016/j.tca.2020.178545.
  13. Interior Parts and Components Fire Protection for Transport Category Airplanes. Federal Register, 2019, vol. 84, no. 128, p. 31747–31769. Available at: https://www.federalregister.gov/documents/2019/07/03/2019-13646/interior-parts-and-components-fire-protection-for-transportcategory-airplanes (accessed: December 1, 2020).
  14. Barbotko S.L., Volny O.S., Bochenkov M.M. Analysis of the US Federal Aviation Administration proposals for the reform of aviation standards regarding the fire safety of used materials (review). Trudy VIAM, 2020, no. 6–7 (89), paper no. 11. Available at: http://www.viam-works.ru (accessed: December 1, 2020). DOI: 10.18577/2307-6046-2020-0-67-101-117.
  15. Flame Retardant Chemicals: Technologies and Global Markets / BCC Research. 2015. 164 p.
  16. Polymer Green Flame Retardant. Ed. C.D. Papaspyrides, P. Kiliaris. Elsevier, 2014. 943 p.
  17. Organization for the Prohibition of Chemical Weapons. Chemical Weapons Convention. Available at: http://www.opcw.org/ru (accessed: December 1, 2020).
  18. Serkova EA, Zastrogina O. B., Barbotko S. L. Study of the possibility of use of new environmentally friendly organophosphorus flame retardants in the composition of binders for interior fire safety materials . Trudy VIAM, 2019, no. 2 (74), paper no. 03. Available at: http://www.viam-works.ru (accessed: December 01, 2020). DOI: 10.18577/2307-6046-2019-0-2-24-34.
  19. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  20. Kablov E.N. What to make the future of? New generation materials, technologies for their creation and processing – the basis of innovations. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  21. Krutikova A. Functionalized graphene oxide improves the fire resistance of composites. Available at: https://ogneportal.ru/news/2401 (accessed: December 01, 2020).
  22. Graphene in the form of microparticles in powder. Available at: https://rusgraphene.ru/product-page/graphene-powder (accessed: December 01, 2020).
  23. Wang J., Ma C., Wang P., Qiu S. et al. Ultra-low phosphorus loading to achieve the superior flame retardancy of epoxy resin. Polymer Degradation and Stability, 2018, no. 149, pp. 119–128. DOI: 10.1016/j.polymdegradstab.2018.01.024.
  24. Yan W., Zhang M.-Q., Yu J. et al. Synergistic Flame-retardant Effect of Epoxy Resin Combined with Phenethyl-bridged DOPO Derivative and Graphene Nanosheets. Chinese Journal of Polymer Science, 2019, no. 37, pp. 79–88. DOI: 10.1007/s10118-019-2175-6.