Petrov A.A., Speransky K.A. Magnesium alloys: prospective industries of application, advantages and disadvantages (review). Part 2. Mechanism of deformation and anisotropy of mechanical properties of magnesium alloys // Proceedings of VIAM. 2021. No. 11 (105). Ст. 02. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-11-12-24.

Magnesium alloys: prospective industries of application, advantages and disadvantages (review)

Part 2. Mechanism of deformation and anisotropy of mechanical properties of magnesium alloys
Petrov A.A., Speransky K.A.
Abstract

Magnesium alloys are the lightest of metallic structural materials with a number of advantages, such as low density, manufacturability and high damping capacity. In this part of the review, the article deals with the anisotropy of the mechanical properties of magnesium alloys associated with the texture of the resulting semi-finished products and products, the relationship of alloying elements with the crystallographic lattice parameters, as well as the deformation mechanisms prevailing in various alloying systems.

Keywords
magnesium alloys, anisotropy of mechanical properties, twinning, slip system, pole density, texture.
Reference list
  1. Hirsch J., Al-Samman T. Superior light metals by texture engineering: Optimized aluminum and magnesium alloys for automotive applications. Acta Materialia, 2013, vol. 61, pp. 818–843.
  2. Betsofen S.Ya., Osintsev O.E., Grushin I.A., Petrov A.A., Speransky K.A. Influence of alloying elements on the deformation mechanism and texture of magnesium alloys. Deformatsiya i razrusheniye materialov, 2018, no. 8, pp. 2–17.
  3. Kelley E., Hosford W. The deformation characteristics of textured magnesium. Transactions of the Metallurgical Society of AIME, 1968, no. 242, pp. 654–660.
  4. Barnett M.R. Twinning and the ductility of magnesium alloys. Part II. "Contraction" twins. Materials Science and Engineering, 2007, no. A (464), pp. 8–16.
  5. Koike J., Fujiyama N., Ando D., Sutou Y. Roles of deformation twinning and dislocation slip in the fatigue failure mechanism of AZ31 Mg alloys. Original Research Article Scripta Materialia, 2010, no. 63, pp. 747–750.
  6. Ando D., Koike J., Sutou Y. Relationship between deformation twinning and surface step formation in AZ31 magnesium alloys. Acta Materialia, 2010, no. 58, pp. 4316–4324.
  7. Muránsky O., Carr D.G., Šittner P., Oliver E.C. In situ neutron diffraction investigation of deformation twinning and pseudoelastic-like behavior of extruded AZ31 magnesium alloy. Original Research Article International Journal of Plasticity, 2009, no. 25, pp. 1107–1127.
  8. Knezevic M., Levinson A., Harris R., Raja K. Mishra, Roger D. Doherty and Surya R. Kalidindi Deformation twinning in AZ31: Influence on strain hardening and texture evolution. Acta Materialia, 2010, no. 58, pp. 6230–6242.
  9. Martin E., Capolungo L., Jiang L., Jonas J. J. Variant selection during secondary twinning in Mg – 3% Al. Acta Materialia, 2010, no. 58, pp. 3970–3983.
  10. Barnett M.R., Keshavarz Z., Beer A.G., Ma X. Non-Schmidbehavior during secondary twinning in a polycrystalline magnesium alloy. Acta Materialia, 2008, no. 56, pp. 5–15.
  11. Bozhko S.A., Betsofen S.Ya., Kolobov Yu.R., Vershinina T.N. Formation of the Structure and Properties of an Mg – Al – Zn – Mn Alloy during Plastic Deformation by Rolling. Russian Metallurgy (Metally), 2015, no. 3, pp. 205–210.
  12. Ferro R., Saccone A., Delfino S. Magnesium alloys of the rare earth metals: systematics and properties. Metallurgical Science and Technology, 1998, no. 16, pp. 25–44.
  13. Betzofen S.Ya., Volkova E.F., Kolobov Yu.R. et al. Investigation of texture and anisotropy of mechanical properties of magnesium alloys with rare earth metals. Tekhnologiya legkikh splavov, 2012, no. 1, pp. 31–38.
  14. Liu X.B., Chen R.S., Han E.H. Effects of aging treatment on microstructures and properties of Mg – Gd – Y – Zr alloys with and without Zn additions. Journal of Alloys and Compounds, 2008, no. 465, pp. 232–238.
  15. Gao L., Chen R.S., Han E.H. Effects of rare-earth elements Gd and Y on the solid solution strengthening of Mg alloys. Journal of Alloys and Compounds, 2009, no. 481, pp. 379−384.
  16. Hang K., Li X., Li Y., Ma M. Effect of Gd content on microstructure and mechanical properties of Mg – Y – RE – Zr alloys. Transactions of Nonferrous Metals Society of China, 2008, no. 18, pp. 12–16.
  17. Ming S., Wu G., Wang W., Ding W. Effect of Zr on the microstructure, mechanical properties and corrosion resistance of Mg – 10Gd – 3Y magnesium alloy. Materials Science and Engineering A, 2009, no. 523, pp. 145–151.
  18. Peng Q., Wang L., Wu Y., Wang L. Structure stability and strengthening mechanism of die-cast Mg – Gd – Dy based alloy. Journal of Alloys and Compounds, 2009, no. 469, pp. 587–592.
  19. Rokhlin L.L., Dobatkina T.V., Nikitina N.I., Tarytina I.E., Lukyanova E.A. Behavior during annealing of high-strength magnesium alloy IMV7-1 of the Mg – Y – Gd – Zr system. Perspektivnye materialy, 2011, no. 6, pp. 53–58.
  20. Lukyanova E.A., Rokhlin L.L., Dobatkina T.V., Korolkova I.G. Investigation of the solubility of samarium in a solid solution based on magnesium containing yttrium and gadolinium. Metally, 2012, no. 4, pp. 85–89.
  21. Rokhlin L.L., Lukyanova E.A., Dobatkina T.V., Aladiev N.A., Korolkova I.G. Phase equilibria in alloys of the Mg – Y – Gd – Sm system. Metally, 2012, no. 5, pp. 71–77.
  22. Rokhlin L.L. Magnesium Alloys Containing rare Earth Metals. Taylor and Francis. 2003, no. 1, p. 245.
  23. Drits M.E., Dobatkina T.V., Muratova E.V. Investigation of magnesium alloys containing lanthanum and zirconium. Metallurgy and processing of non-ferrous alloys. On the occasion of the 90th anniversary of the birth of Academician A.A. Bochvara: collection scientific articles. Moscow: Nauka, 1992, pp. 32–37.
  24. Drits M.E., Rokhlin L.L., Nikitina N.I. Research of magnesium – scandium alloys. Tekhnologiya legkikh splavov, 1976, no. 1, pp. 22–26.
  25. Rokhlin L.L. Structure and properties of alloys of the Mg – REM system. Materials Science and Heat Treatment of Metals, 2006, no. 11, pp. 18–22.
  26. Rokhlin L.L., Lukyanova E.A., Dobatkina T.V., Korolkova I.T., Tarytina I.E., Ovchinnikova O.A. Features of the structure of state diagrams of alloys magnesium with two rare-earth metals of different groups and predicting fragments of the investigated phase diagrams of this type on their basis. Tekhnologiya legkikh splavov, 2016, no. 4, pp. 41–49.
  27. Dobatkin S.V., Rokhlin L.L., Dobatkina T.V., Nikitina N.I., Tarytina I.E. Investigation of magnesium alloys of the Mg – Sm – Y system subjected to severe plastic deformation and subsequent heat treatment. Metally, 2011, no. 4, pp. 32–37.
  28. Rokhlin L.L., Dobatkin S.V., Dobatkina T.V. et al. Investigation of aging Mg – Sm alloys subjected to severe plastic deformation. Metally, 2006, no. 1, pp. 89–95.
  29. Volkova E.F., Duyunova V.A. About modern tendencies of development of magnesium alloys. Tekhnologiya legkikh splavov, 2016, no. 3, pp. 94–105.
  30. Bozhko S.A. Regularities of the formation of the structure and properties of magnesium alloys under the influence of plastic deformation: thesis, Cand. Sc. (Tech.). Belgorod, 2016, 113 p.
  31. Betzofen S.Ya., Osintsev O.E., Grushin I.A., Petrov A.A., Speransky K.A. Regularities of the formation of texture and anisotropy of mechanical properties of magnesium alloys. Deformatsiya i razrusheniye materialov, 2018, no. 9, pp. 2–15.
  32. Shaforostov A.A. Study of the influence of alloying elements on the formation of texture and anisotropy of the properties of magnesium alloys: thesis, Cand. Sc. (Tech.). Moscow, 2011, 136 p.
  33. Betsofen S.Ya., Ilyin A.A., Ashmarin A.A., Shaforostov A.A. Influence of the deformation mechanism on the anisotropy of mechanical properties and manufacturability of magnesium alloys. Metally, 2008, no. 3. S. 83–90.
  34. Betzofen S.Ya., Volkova E.F., Shaforostov A.A. Influence of alloying elements on the formation of rolling texture of Mg – Nd – Zr and Mg – Li alloys. Metally, 2011, no. 1, pp. 78–84.
  35. Haferkamp H., Boehem R., Holzkamp U., Jachik C., Kaese V., Niemeyer M. Alloy development, processing and applications in magnesium lithium alloys. Materials Transactions, 2001, no. 7, pp. 1160-1166.
  36. Volkova E.F. The analysis and results of the International conference «Magnesium–21. Broad horizons» (review). Aviacionnye materialy i tehnologii, 2016, no. 1 (40), pp. 86–94. DOI: 10.18577/2071-9140-2016-0-1-86-94.
  37. Kozlov I.A., Vinogradov S.S., Tarasova K.G., Kulyushina N.V., Manchenko V.A. Plasma electrolytic oxidation of magnesium alloys (review). Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 23–36. DOI: 10.18577/2071-9140-2019-0-1-23-36.
  38. Kablov E.N., Akinina M.V., Volkova E.F., Mostyaev I.V., Leonov A.A. The research of aspects of phase composition and fine structure of magnesium alloy ML9 in the as-cast and heat-treated conditions. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 17–24. DOI: 10.18577/2071-9140-2020-0-2-17-24.
  39. Vetrova E.Yu., Shchekin V.K., Kurs M.G. Comparative evaluation of methods for the determination of corrosion aggressivity of the atmosphere. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 74–81. DOI: 10.18577/2071-9140-2019-0-1-74-81.
  40. Kablov E.N., Startsev V.O. Measurement and forecasting of materials samples’ temperature during weathering in different climatic zones. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 47–58. DOI: 10.18577 / 2071-9140-2020-0-4-47-58.
  41. Kablov E.N. Structural and functional materials – the basis of economic, scientific and technical development of Russia. Voprosy materialovedeniya, 2006, no. 1 (61). S. 64–67.
  42. Zhu T., Cui C., Zhang T. et al. Influence of the combined addition of Y and Nd on the microstructure and mechanical properties of Mg – Li alloy. Materials and Design, 2014, no. 57, pp. 245–249.
  43. Cui C., Zhu T., Zhang T. et al. Microstructure and texture evolution of Mg – Li alloy during rolling. International Journal of Materials Research, 2014, no. 105, pp. 1111–1117.