Babashov V.G., Varrik N.M. Zirconia fibers as a component of high temperature thermal insulation (review) // Proceedings of VIAM. 2021. No. 10 (104). Ст. 08. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-10-79-86.

Zirconia fibers as a component of high temperature thermal insulation (review)

Babashov V.G., Varrik N.M.
Abstract

Based on the analysis of recent publications of scientific and technical literature, data on the production of zirconium oxide fibers used for the manufacture of high-temperature thermal insulation materials are presented. Information is provided on various methods of obtaining zirconium oxide fibers (methods of impregnation of the template and molding of the mixture, sol-gel method of spinning a fiber-forming precursor solution), as well as on the technique of fiber molding (manual pulling, dry and wet spinning, blowing and electrospinning). The use of such fibers for the production of thermal insulation materials (felts, cords and blocks) instead of currently existing materials made of aluminum oxide-based fibers can significantly increase the operating temperatures of the thermal protection systems.

Keywords
oxide fiber, zirconium oxide, high-temperature heat insulation, sol-gel method, electrospunning.
Reference list
  1. Kablov E.N. New generation materials – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  2. Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7-8, pp. 54–58.
  3. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  4. Babachov V.G., Stepanova E.V., Zimichev A.M., Basargin O.V. Oxide continuous fibers as a part of flexible high temperature insulation. Aviation materials and technology, 2021. no. 1 (62). paper no. 04. Available at: http://www.journal.viam.ru (accessed: July 8, 2021). DOI: 10.18577/2713-0193-2021-0-1-34-43.
  5. Babashov V.G., Maksimov V.G., Varrik N.M., Samorodova O.N. Studying of structure and pro-perties of samples of ceramic composite materials on the basis of mullite. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 54–63. DOI: 10.8577/2071-9140-2020-0-1-54-63.
  6. Saffil® Alumina Fibers. Available at: https://www.unifrax.com/product/saffil-fibers (accessed: July 1, 2021).
  7. Polycrystalline Alumina Fiber MAFTECTM. Available at: https://www.m-chemical.co.jp/en/products/departments/mcc/maf-metal/product/1201261_7532.html (accessed: July 2, 2021).
  8. Fibers. Available at: www.zircarceramics.com/product/category/fibers (accessed: July 2, 2021).
  9. Unifrax product catalog. Available at: www.unifrax.com/product-category/fibers/?productcategory=231 (accessed: July 4, 2021).
  10. Zircar Zirconia Inc. product catalog. Available at: www.zircarzirconia.com/products/ceramic-textiles#zirconia (accessed: July 4, 2021).
  11. STA Universe group Co. product catalog. Available at: http://stauniversegp.com/2200ZirconiaFiberBoard (accessed: August 4, 2021).
  12. Zhigachev A.O., Golovin Yu.I., Umrikhin A.V. et al. Ceramic materials based on zirconium dioxide. Ed. Yu.I. Golovin. Moscow: Tekhnosfera, 2018, 358 p.
  13. Bokiy G.B. Crystal chemistry. Moscow: Nauka, 1971, 00 p.
  14. Polezhaev Yu.M. Low-temperature cubic and tetragonal forms of zirconium dioxide. Zhurnal fizicheskoy khimii, 1967, vol. 41, no. 11, pp. 2958–2959.
  15. Voronkov A.A., Pyatenko Yu.A., Shumyatskaya N.G. Crystal chemistry of zirconium minerals and their artificial analogues. Moscow: Nauka, 1978, 184 p.
  16. Yashima M., Noma T., Ishizava N. Effects of Non-Compositional Inhomogeneity on t → m Phase Transformation during Grinding of Various Rare-Earth-Doped Zirconia. Journal of the American Ceramic Society, 2005, vol. 74, no. 12, pp. 3011–3016.
  17. Bechepeche A.P., Treu O., Longo E., Paiva-Santos C. Experimental and theoretical aspects of the stabilization of zirconia. Journal of Materials Science, 1999, vol. 34, no. 11, pp. 2751–2756.
  18. Stubican V.S. Phase Equilibria and Metastabilities in the Systems ZrO2–MgO, ZrO2–CaO, and ZrO2–Y2O3. Advances in Ceramics, 1988, vol. 24, pp. 71–82.
  19. Milovich F.O. Structure and mechanical properties of ZrO2 crystals partially stabilized by Y2O3: thesis, Cand. Sc. (Phys.&Math.). Moscow, 2013, 24 p.
  20. Stabilized Tetragonal Zirconia Fibers and Textiles: pat. 3860529 USA, no. 249057; field 01.05.72; publ. 14.06.75.
  21. Process for Preparation of Zircon Coated Zirconia Fibers: pat. 3861947 USA, no. 29376872; field 02.10.72; publ. 25.01.75.
  22. Zirconium Oxide Fibers and Process for Their Preparation: pat. 4937212 USA, no. 286654; field 19.12.88; publ. 26.06.90.
  23. Fine coagulated particles of ultrafine monoclinic zirconia crystals oriented in a fiber bundle-like form and method of manufacturing them: pat. 4722833 USA, no. 93996186; field 10.12.86; publ. 02.02.88.
  24. Production of zirconia filament: pat. Н0491227 JP, no. 19900199017; field 30.07.90; publ. 24.03.92.
  25. Method for preparing fully-stabilized tetragonal-phase zirconia crystal fibers: pat. 102775143 CN, no. 20121299746; field 22.08.12; publ. 14.11.12.
  26. Method for preparing organic poly-zirconium precursor or silk-thrawn liquor thereof for zirconia fiber production by one-step solvent method: pat. 102766154 CN, no. 201210264131, field 28.07.12, publ. 07.11.12.
  27. Marshall D.B., Lange F.F., Morgan P.D. High-Strength Zirconia Fibers. Journal of the American Ceramic Society, 2005, vol. 70, no. 8, pp. 187–188.
  28. Kamiya K., Takahashi K., Maeda T. et al. Sol-gel Derived CaO and CeO2-stabilized ZrO2-fibers – Conversion Process of Gel to Oxide and Tensile Strength. Journal of 6the European Ceramic Society, 1991, vol. 7, pp. 295–305.
  29. Li J., Jiao X., Chen D. Preparation of Zirconia Fibers via a Simple Aqueous Sol-Gel Method. Journal of Dispersion Science and Technology, 2007, vol. 28, pp. 531–535.
  30. Zhao Y., Tang Y., Guo Y., Bao X. Studies of electrospinning process of zirconia nanofibers. Fibers and Polymers, 2010, vol. 11, no. 8, pp. 1119–1122.
  31. Bussarin K., Manop P. Fabrication of Ceramic Nanofibers Using Atrane Precurso. Nanofibers. Ed. by A. Kumar. INTECH, Croatia, 2010, pp. 367–382.
  32. Qin D., Gu A., Liang G., Yuan L. A facile method to prepare zirconia electrospun fibers with different morphologies and their novel composites based on cyanate ester resin. Royal Society of Chemistry Advances, 2012, no. 2, pp. 1364–1372.
  33. Sun G.X., Liu F.T., Bi J.Q., Wang C.A. Electrospun zirconia nanofibers and corresponding formation mechanism study. Journal of Alloys and Compounds, 2015, vol. 649, no. 15, pp. 788–792. DOI: 10.1016/J.JALLCOM.2015.03.068.
  34. Тyurin A.I., Rodaev V.V., Razlivalova S.S., Vasyukov V.M. Investigation of the influence of electrospinning parameters on the control of the morphology and diameter of nanofibers zirconium acetylacetonate/polyacrylonitrile. Mezhdunarodny nauchno-issledovatel'skiy zhurnal, 2019, no. 9 (87), pp. 67–70. DOI: 10.23670/IRJ.2019.87.9.011.
  35. Korenkov V.V., Rodaev V.V., Shuklinov A.V. et al. Synthesis and properties of multifunctional ceramic nanofibers obtained by electrospinning. Vestnik TGU, 2013, vol. 18, is. 6, pp. 3156–3159.
  36. Istomin A.V., Kolyshev S.G. Electrostatic method of forming ultrathin fibers of refractory oxides. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 40–46. DOI: 10.18577/2071-9140-2019-0-2-40-46.
  37. Abe Y., Kudo T., Tomioka H. et al. Preparation of continuous zirconia fibres from polyzirconoxane synthesized by the facile one-pot reaction. Journal of Materials Science, 1998, vol. 33, pp. 1863–1870.
  38. Pullar R.C., Taylor M.D., Bhattacharya A.K. The manufacture of partially-stabilised and fully-stabilised zirconia fibres blow spun from an alkoxide derived aqueous sol-gel precursor. Journal of the European Ceramic Society, 2001, vol. 21, pp. 19–27.
  39. Varrik N.M., Ivahnenko Ju.A. Features of producing zirconia fibers (review). Trudy VIAM, 2015, no. 10, paper no. 08. Available at: http://www.viam-works.ru (accessed: July 8, 2021). DOI: 10.18577/2307-6046-2015-0-10-8-8.
  40. Balinova Yu.A., Varrik N.M., Istomin A.V., Lyulyukina G.Yu. Obtaining zirconium oxide fibers by electrospinning. Steklo i keramika, 2020, no. 8, pp. 30–35.
  41. Lebedeva Yu.E., Shchegoleva N.E., Voronov V.A., Solntcev S.S. Al2O3 and ZrO2 ceramic materials obtained by sol-gel method. Trudy VIAM, 2021, no. 4 (98), paper no. 05. Available at: http://www.viam-works.ru (accessed: July 8, 2021). DOI: 10.18577/2307-6046-2021-0-4-61-73.