Kan A.Ch., Zhelezina G.F., Solovjova N.A. Aramid organoplastics for increasing the bird resistance of elements of aircraft structures // Proceedings of VIAM. 2021. No. 1 (95). Ст. 08. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2021-0-1-77-84.

Aramid organoplastics for increasing the bird resistance of elements of aircraft structures

Kan A.Ch., Zhelezina G.F., Solovjova N.A.
Abstract

The possibility of using protective screens made of aramid organoplastics to ensure the bird resistance of carbon fiber wing flaps is investigated. Aramid organoplastics were selected for the production of a protective screen, taking into account the main requirements for the materials of external contour of the aircraft wing. The result of impact tests simulating the collision of a bird with carbon fiber flaps that are not protected and protected by organoplastics are presented. The optimal ratio of aramid organoplastics as part of the protective screen for carbon fiber wing flaps is presented.

Keywords
elements of aircraft structures, organoplastic, carbon plastic, protective screen, mechanical shock, bird resistance.
Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. New generation materials – the basis for innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  3. Fritsch O. Flight safety – task № 1. Kurer UNESCO, 1978, no. 4, pp. 20–22.
  4. Ongirsky G.G., Shupikov A.N., Ugrimov S.V. Influence of kinematic factors on the reaction of a deformable obstacle in a collision with a bird. Voprosy proektirovaniya i proizvodstva konstruktsij letatelnykh apparatov, 2008, no. 5, pp. 54–62.
  5. Ongirsky G.G., Shupikov A.N., Ugrimov S.V. Investigation of the reaction of a deformable obstacle to a blow by a bird and a simulator. Trudy TsAGI, 2009, is. 2683, pp. 89–95.
  6. Manual on the ICAO Bird Strike Information System (IBIS). Available at: http://aerohelp.ru/sysfiles/374_195.pdf (accessed: November 9, 2020).
  7. Kurteev V.A., Mozerov B.G., Sokolovsky M.I., Inozemtsev A.A. Assessment of the protective ability of the fan housing of a turbojet engine. Vestnik Permskogo Natsionalnogo Issledovatelskogo Universiteta. Aerodinamicheskaya tekhnika, 2015, no. 40, pp. 22–43.
  8. Kurteev V.A. Experimental modeling of the impact interaction of a detached blade with a fan housing of a turbojet engine. Vestnik Permskogo Natsionalnogo Issledovatelskogo Universiteta. Aerodinamicheskaya tekhnika, 2018, no. 52, pp. 97–116.
  9. Krundaeva A.N. Development of a lightweight design of the fan housing of an aircraft engine. Vestnik USATU, ser.: Aviatsionnaya i kosmicheskaya tekhnika, 2013, vol. 17, no. 1 (54), pp. 27–32.
  10. Inozemtsev A.A., Konyaev E.A., Medvedev V.V., Neradko A.V., Ryassov A.E. PS-90A aircraft engine: textbook. Moscow: Fizmatlit, 2007, 320 p.
  11. Kuzmin M.V., Kirsanov A.R. Estimation of the damageability of a gas turbine engine when birds hit the entrance. Nauchnyj vestnik MGTU GA, 2015, no. 212, pp. 127–132.
  12. Zhezina G.F., Voinov S.I., Karinbaev TD, Chernyshov A.A. Aramid Organoplastics for Aircraft Engine Fan Housings. Voprosy materialovedeniya, 2017, no. 32 (90), pp. 153-165.
  13. Shuldeshova P.M., Zhelezina G.F. The aramid layered and woven material for protection against impact and ballistic influences. Trudy VIAM, 2014, no. 9, paper no. 06. Available at: http://www.viam-works.ru (accessed: October 26, 2020). DOI: 10.18577/2307-6046-2014-0-9-6-6.
  14. Zhelezina G.F., Voinov S.I., Solovieva N.A., Kulagina G.S. Aramid organotexolites for shock-resistant aircraft structures. Zhurnal prikladnoy Khimii, 2019, vol. 92, is. 3, pp. 358–364. DOI: 10.1134/S0044461819030101.
  15. Zhelezina G.F., Gulyaev I.N., Soloveva N.A. Aramide organic plastics of new generation for aviation designs. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 368–378. DOI: 10.18577/2071-9140-2017-0-S-368-378.
  16. Dubinsky S.V., Feigenbaum Yu.M., Selikhov A.A., Gvozdev S.A., Ordyntsev V.M. Regularities of the implementation of random shock effects on the wing structure of a commercial aircraft. Izvestia Samarskogo nauchnogo tsentra Rossijskoj akademii nauk, 2016, vol. 18, no.4 (3), pp. 604–611.
  17. Kablov E.N., Startsev O.V. The basic and applied research in the field of corrosion and ageing of materials in natural environments (review). Aviacionnye materialy i tehnologii, 2015, no. 4 (37), pp. 38–52. DOI: 10.18577/2071-9140-2015-0-4-38-52.
  18. Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  19. Kablov E.N., Startsev V.O., Inozemtsev A.A. The moisture absorption of structurally similar samples from polymer composite materials in open climatic conditions with application of thermal spikes. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 56–68. DOI: 10.18577/2071-9140-2017-0-2-56-68.
  20. Zhelezina G.F., Bova V.G., Voinov S.I., Kan A.Ch. Prospects for the use of hybrid fabrics based on carbon and aramid fibers as a reinforcing filler of polymer composite materials. Voprosy materialovedeniya, 2019, no. 2 (98), pp. 86–95. DOI: 10.22349/1994-67-2019-98-2-86-95.