Sorokin O.Ju., Kuznetsov B.Yu., Lunegova Yu.V., Erasov V.S. High-temperature composites with a multi-layered structure (review) // Proceedings of VIAM. 2020. No. 4-5 (88). Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-45-42-53.
High-temperature composites with a multi-layered structure (review)
Abstract
Properties, processing techniques and possible applications in «hot sections» of gas turbine engine of different structural high-temperature materials with an operating temperature higher than 1200 °С are highlighted. Composites with a multi-layered structure based on «ceramic/carbon», «ceramic/ceramic», «ceramic/metal» systems have demonstrated to be promising materials. Layer widths with low/high Young modules, their ratio and arrangement have a significant impact on the strength parameters. High-temperature composites with a multi-layered structure can have a «graceful failure» mode and higher toughness as compared to particle reinforced ceramic composites.
Keywords
ceramic, composite materials, multi-layered structure, toughness, graceful fracture mode, strength, oxidation.
Reference list
- Kablov E.N., Ospennikova O.G., Svetlov I.L. Highly efficient cooling of GTE hot section blades. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 3–14. DOI: 10.18577/2071-9140-2017-0-2-3-14.
- Kablov E.N., Petrushin N.V., Parfenovich P.I. Design of castable refractory nickel alloys with polycrystalline structure. Metal Science and Heat Treatment, 2018, vol. 60, no. 1–2, pp. 106–114.
- Kablov E.N., Ospennikova O.G., Petrushin N.V., Visik E.M. Single-crystal nickel-based superalloy of a new generation with low-density. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 14–25. DOI: 10.18577/2071-9140-2015-0-2-14-25.
- Zhao J.-C., Westbrook J.H. Ultrahigh-temperature materials for jet engines. MRS Bulletin, 2003, no. 9, pp. 622–627.
- Harada H. High Temperature Materials for gas turbines: the present and future. Proceedings of the International Gas Turbine Congress, Tokyo, 2003, pp. 1–9.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Mileiko S.T. High temperature molybdenum matrix composites. Ceramics International, 2018, vol. 45, is. 7, pp. 9439–9443.
- Kablov E.N., Zhestkov B.E., Grashchenkov D.V., Sorokin O.Yu. et al. Investigation of the oxidative resistance of high-temperature coating on a SiC material under exposure to high-enthalpy flow. High Temperature, 2017, vol. 55, no. 6, pp. 873–879. DOI: 10.7868/S0040364417060059.
- Kablov E.N., Ospennikova O.G., Vershkov A.V. Rare metals and rare earth elements – materials of modern and future high technologies. Trudy VIAM, 2013, no. 2, paper no. 01. Available at: http://www.viam-works.ru (accessed: December 04, 2019).
- Bewlay B.P., Jackson M.R., Zhao J.-C., Subramanian P.R. A review of very-high-temperature Nb silicide-based composites. Metallurgical and Materials Transactions A, 2003, vol. 34A, no. 10, pp. 2043–2052.
- Iždinsky K., Senčekova L., Simančik F. et al. Mo/Mo silicide composites prepared by pressure-assisted reactive infiltration. Kovove Materialy, 2015, no. 53, pp. 391–397.
- Seeműller H.Ch.M. Evaluation of Powder Metallurgical Processing Routes for Multi-Component Niobium Silicide-Based High-Temperature Alloys: thesis, PhD. Karlsruher Institut für Technologie, 2016, 177 p.
- Drawin S., Justin J.F. Advanced Lightweight Silicide and Nitride Based Materials for Turbo-Engine Applications. Aerospacelab, 2011, is. 3, pp. 1–12.
- Murasheva V.V., Shchetanov B.V., Sevostyanov N.V., Efimochkin I.Yu. High-temperature Mo – Si composite materials (review). Konstruktsii iz kompozitsionnykh materialov, 2014, no. 2 (134), pp. 24–35.
- Trofimenko N.N., Efimochkin I.Yu., Bolshakova A.N. Problems of creation and prospects for the use of heat-resistant high-entropy alloys. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 3–8. DOI: 10.18577/2071-9140-2018-0-2-3-8.
- Perepezko J.H., Sossaman T. A., Taylor M. Environmentally Resistant Mo–Si–B-Based Coatings. Journal of Thermal Spray Technology, 2017, vol. 26, pp. 929–940.
- Roode M.V. Ceramic gas turbine development: need for a 10 year plan. Journal of Engineering for gas Turbine and Power, 2010, vol. 132, no. 1, pp. 1–7.
- Nozhnitsky Y.A., Fedina Y.A., Rekin A.D. et al. Development and investigation of ceramic parts for gas-turbine engines. International Gas Turbine and Aeroengine Congress and Exhibition, Orlando, Florida, 1997, pp. 1–8.
- Nozhnitskiy Y.A., Fishgoyt A.V., Fedina Y.A. et al. Development of methods and experimental investigation of ceramic, carbon-carbon and other composite materials structural Strength at Ultra-High Temperature, 1998. Available at: https://archive.org/details/DTIC_ADA349444/mode/1up (accessed: January 03, 2020).
- Bewlay B.P., Jackson M.R., Gigliotti M.F.X. Niobium Silicide High Temperature In Situ Composites. Intermetallic Compounds – Principles and Practice, 2002, vol. 3: Progress, pp. 541–560.
- Hebsur M.G. MoSi2-base composites. Handbook of Ceramic Composites, Boston, MA: Springer, 2005, pp. 173–196.
- Petrovic J.J. High-temperature structural silicides. Proceedings of 21st Annual conference on composites, advanced ceramics, materials and structures, USA, 1997, pp. 3–17.
- Corman S.G., Luthra K.L. Development history of GE’s prepreg melt infiltrated ceramic matrix composite material and application. Comprehensive Composite Materials II, 2018, vol. 5, p. 325–328.
- Klemm H., Kunz W., Wamser T. et al. Hot gas stability of various ceramic matrix composites. Advances in High Temperature Ceramic Matrix Composites and Materials for Sustainable Development, 2017, vol. 263, pp. 253–260.
- Bansal N.P., Lamon J. Ceramic matrix composites: materials, modeling and technology. Wiley, 2015, 715 p.
- Behrendt T., Hackemann S., Mechnich P. et al. Development and test of oxide/oxide ceramic matrix composites combustor liner demonstrators for Aero-engines. Journal of Engineering for Gas Turbines and Power, 2016, vol. 139, no. 3, pp. 1–12.
- Holmquist M., Lundberg R., Sudre O. et al. Alumina/alumina composite with a porous zirconia interphase – processing, properties and component testing. Journal of the European Ceramic Society, 2000, vol. 20, pp. 599–606.
- Roode M.V., Bhattacharya A.K. Durability of Oxide/Oxide Ceramic Matrix Composites in Gas Turbine Combustors. Journal of Engineering for Gas Turbines and Power, 2013, vol. 5, pp. 1–9.
- Schawaller D., Clauß B., Buchmeiser M.R. Ceramic Filament Fibers – A Review. Macromolecular Materials and Engineering, 2012, no. 297, pp. 502–522.
- Porter M.M., Mckittrick J. It's tough to be strong: Advances in bioinspired structural ceramic based materials. American Ceramic Society Bulletin, 2014, vol. 93, no. 5, pp. 18–24.
- Clegg W.J., Kendall K., Alford N.M.N. et al. A simple way to make tough ceramics. Nature, 1990, vol. 347, no. 10, pp. 455–457.
- Clegg W.J. The fabrication and failure of laminar ceramic composites. Acta Metallurgica et Materialia, 1992, vol. 40, no. 11, pp. 3085–3093.
- Clegg W.J., Andrees G., Carlstrom E. et al. The properties of ceramic laminates. Ceramic Engineering & Science Proceedings, 1999, vol. 20, no. 4, pp. 421–426.
- Xiang L., Cheng L., Shi L. et al. Laminated HfC–SiC ceramics produced by aqueous tape casting and hot pressing. Ceramics International, 2015, vol. 41, is. 10, part B, pp. 14406–14411.
- Wei Ch., Yin K., Ji W. et al. Ablation behavior of laminated Graphite/ZrB2-SiC ceramics in two different directions. Ceramics International, 2018, vol. 44, is. 13, pp. 15674–15680.
- Zhang T., Jin H., Wang Y., Jin Zh. The Mechanical Properties of AlN/BN Laminated Ceramic Composites. Materials Science Forum, 2008, vol. 569, pp. 97–100.
- Li C., Huang Y., Wang C. et al. Mechanical properties and microstructure of laminated Si3N4+SiCw/BN+Al2O3 ceramics densified by spark plasma sintering. Materials Letters, 2002, vol. 57, pp. 336–342.
- Shavnev A.A., Vaganova M.L., Sorokin O.Yu., Evdokimov S.A., Zhitnyuk S.V., Kuznetsov B.Yu. The effect of a multilayer structure on the physicomechanical properties of a ceramic composite material based on the Si – B – Mo – C system. Fizicheskaya mezomekhanika, 2019, no. 1, pp. 1–8.
- Patterson M.C.L., Fulcher M., Halloran J., Singh R. Application of Sinboron fibrous monoliths for air breathing engine applications. Proceedings of 41st Joint Propulsion Conference & Exhibition, Tucson, Arizona, 2005, pp. 1–7.
- Koh Y.-H., Kim H.-W., Kim H.-E., Halloran J.W. Thermal shock resistance of fibrous monolithic Si3N4/BN ceramics. Journal of the European Ceramic Society, 2004, vol. 24, pp. 2339–2347.
- Trice R.W., Halloran J.W. Elevated-temperature mechanical properties of silicon nitride/ boron nitride fibrous monolithic ceramics. Journal of American Ceramic Society, 2000, vol. 83, no. 2, pp. 311–316.
- Koh Y.-H. Fibrous monolithic ceramics. Ceramic-Matrix Composites: Microstructure, Properties and Applications. Woodhead Publishing Limited, 2006, pp. 9–32.
- Guo H., Yoon D.-H., Shin D.-W. Prediction of Fracture Toughness in Fibrous Si3N4 Monolithic Ceramics. Key Engineering Materials, 2006, vol. 317–318, pp. 301–304.
- Ivanov D.A., Sitnikov A.I., Shlyapin S.D. Dispersion-strengthened fibrous and layered inorganic composite materials: textbook. Moscow: MGIU, 2010. 228 p.
- Krstic Z., Krstic V. D. Fracture toughness of concentric Si3N4-based laminated structures. Journal of American Ceramic Society, 2009, vol. 29, pp. 1825–1829.
- Show L., Abbaschian R. Toughening MoSi2 with niobium metal-effects of morphology of ductile reinforcements. Journal of Materials Science, 1995, vol. 30, pp. 849–854.
- Mainzer B., Lin C., Frieβ M. et al. Novel ceramic matrix composites with tungsten and molybdenum fiber reinforcement. Journal of the European Ceramic Society, 2020, vol. 31, pp. 254–268. DOI: 10.1016/j.jeurceramsoc.2019.10.049.
- Vaganova M.L., Erasov V.S., Sorokin O.Yu., Efimochkin I.Yu., Kuznetsov B.Yu. Investigation of the structure and properties of a multilayer composite material based on the system «high-temperature ceramic – refractory metal». Perspektivnye materialy, 2019, no. 9, pp. 15–23.
- Lee S.P., Lee J.K., Son I.S., Bae D.S. Fabrication of Nb/MoSi2 laminate composites and their thermal shock properties. Journal of Ceramic Processing Research, 2013, vol. 14, no. 2. P. 206–209.
- Bai Y., Ma Y., Sun M. et al. Strong and tough ZrB2 materials using a heterogeneous ceramic–metal layered architecture. Journal of American Ceramic Society, 2019, vol. 102, no. 9, pp. 5013–5019.
- Wang H., Wang C. Preparation and mechanical properties of laminated zirconium diboride/molybdenum composites sintered by spark plasma sintering. Frontiers of Materials Science China, 2009, vol. 3, no. 3, pp. 273–280. DOI: 10.1007/s11706-009-0050-z.
- Bai Y., Sun M., Cheng L., Fan S. Developing high toughness laminated HfB2-SiC ceramics with ductile Nb interlayer. Ceramics International, 2019, vol. 45, pp. 20977–20982.