Tkachuk A.I., Afanaseva E.A. Reactive type flame retardants for epoxy resins. Part 2 // Proceedings of VIAM. 2020. No. 4-5 (88). Ст. 02. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-45-13-21.

Reactive type flame retardants for epoxy resins

Part 2
Tkachuk A.I., Afanaseva E.A.
Abstract

The second part paper considers such new and already used in industrial applications reactive type flame retardants for epoxy resins, which can reduce their combustibility without significantly reducing their heat resistance and mechanical properties, as different functionalized phosphazenes, organic compounds based on nitrogen or silicone atoms and rigid aromatic compounds with excellent thermal stability and high resistance to burning. The effects of these additives and their mechanism of action are shown.

Keywords
epoxy resins, modification, flame retardants, resistance to burning, functional groups.
Reference list
  1. Tkachuk A.I., Terekhov I.V., Afanasyeva E.A. Reactive type flame retardants for epoxy resins. Part 1. Trudy VIAM, 2020, no. 3 (87), paper no. 04. Available at: http://www.viam-works.ru (accessed: March 20, 2020). DOI: 10.18577/2307-6046-2020-0-3-41-48.
  2. Kablov E.N. Chemistry in Aviation Materials Science. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, no. 1, pp. 3–4.
  3. Podzhivotov N.Y., Kablov E.N., Antipov V.V., Erasov V.S., Serebrennikova N.Yu., Abdulin M.R., Limonin M.V. Laminated Metal-Polymeric Materials in Structural Elements of Aircraft. Inorganic Materials: Applied Research, 2017, vol. 8, pp. 211–221.
  4. Barbotko S.L. Development of the fire safety test methods for aviation materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 516–526. DOI: 10.18577/2071-9140-2017-0-S-516-526.
  5. Eliseev O.A., Naumov I.S., Smirnov D.N., Bryk Ya.A. Rubbers, sealants, fireproof and heat-shielding materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 437–451. DOI: 10.18577/2071-9140-2017-0-S-437-451.
  6. Merkulova Yu.I., Muhametov R.R. Development of a low-viscosity epoxy binder for processing by vacuum infusion. Aviacionnye materialy i tehnologii, 2014, no. 1, paper no. 39–41. DOI: 10.18577/2071-9140-2014-0-1-39-41.
  7. Barbotko S.L., Shurkova E.N., Volny O.S., Skrylyov N.S. Evolution of polymer composite fire-safety for the outer contour of aeronautical engineering. Aviacionnye materialy i tehnologii, 2013, no. 1, paper no. 56–59.
  8. Lu S.Y., Hamerton I. Recent developments in the chemistry of halogen-free flame retardant polymers. Progress in Polymer Science, 2002, no. 27, pp. 1661–1712.
  9. Neumeyer T., Bonotto G., Kraemer J. et al. Fire behaviour and mechanical properties of an epoxy hot-melt resin for aircraft interiors. Composite Interfaces, 2013, vol. 20, pp. 443–455.
  10. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  11. Terekhov I.V., Chistyakov E.M., Filatov S.N., Deev I.S., Kurshev E.V., Lonsky S.L. Factors affecting the fire resistance of epoxy compositions modified with epoxy-containing phosphazenes. Voprosy materialovedeniya, 2018, no. 1 (93), pp. 159–168.
  12. Liu R., Wang X. Synthesis, characterization, thermalproperties and flame retardancy of a novel nonflam-mable phosphazene-based epoxy resin. Polymer Degradation and Stability, 2009, vol. 94, pp. 617–624.
  13. Fantin G., Medici A., Fogagnolo M., Pedrini P. et. al. Functionalization of poly(organophosphazene). III. Synthesis of phosphazene materials containing carbon–carbon double bonds and epoxide groups. European Polymer Journal, 1993, vol. 29 (12), pp. 1571–1579.
  14. Allcock H.R. Recent advances in phosphazene (phosphonitrilic) chemistry. Chemical Reviews, 1972, vol. 72, pp. 315–356.
  15. Terekhov I.V., Yudaev P.A., Tupikov A.S. Domestic research in the field of phosphazenes and prospects for their use. Vse materialy. Entsiklopedicheskiy spravochnik, 2018, no. 9, pp. 34–42.
  16. Terekhov I.V., Yudaev P.A., Tupikov A.S. Domestic research in the field of phosphazenes and prospects for their use. Vse materialy. Entsiklopedicheskiy spravochnik, 2018, no. 10, pp. 32–38.
  17. Terekhov I.V., Filatov S.N., Chistyakov E.M. et al. Synthesis of oligomeric epoxycyclotriphosphazenes and their properties as reactive flame-retardants for epoxy resins. Phosphorus, Sulfur and Silicon and the Related Elements, 2017, vol. 192 (5), pp. 544–554.
  18. Terekhov I.V., Filatov S.N., Chistyakov E.M. et al. Halogenated hydroxy-aryloxy phosphazenes and epoxy oligomers based on them. Russian Journal of Applied Chemistry, 2013, vol. 86, no. 10, pp. 1600–1604.
  19. Liu J., Tang J., Wang X., Wu D. Synthesis, characterization and curing properties of a novel cyclolinear phosphazene-based epoxy resin for halogen-free flame retardancy and high performance. RSC Advances, 2012, vol. 2, no. 13, pp. 5789–5799.
  20. Terekhov I.V., Chistyakov E.M., Filatov S.N. et al. Hexa-para-aminophenoxycyclo-triphosphazene as a curing agent/modifier for epoxy resins. International Polymer Science and Technology, 2015, vol. 42, pp. T31-T34.
  21. Levchik S.V., Camino G., Luda M.P. et al. Thermal decomposition of cyclotriphosphazenes. 1. Alkyl–aminoaryl ethers. Journal of Applied Polymer Science, 1998, vol. 67, no. 3, pp. 461–472.
  22. Buckingham M.R., Lindsay A.J., Stevenson D.E. et al. Synthesis and formulation of novel phosphorylated flame retardant curatives for thermoset resins. Polymer Degradation and Stability, 1996, vol. 54, no. 2–3, pp. 311–315.
  23. Kumar D., Fohlen G.M., Parker J.A. The curing of epoxy resins with aminophenoxycyclotriphosphazenes. Journal of Polymer Science, Part A: Polymer Chemistry, 1986, vol. 24, no. 10, pp. 2415–2424.
  24. Terekhov I.V., Chistyakov E.M., Filatov S.N., Kireev V.V., Borisov R.S. Synthesis of hexakis(hydroxyaryloxy)cyclotriphosphazene based on bisphenol A. Mendeleev Communications, 2014, vol. 24, no. 3, pp. 154–155.
  25. Medici A., Fantin G., Pedrini P., Gleria M., Minto F. Functionalisation of phosphazenes. 1. Synthesis of phosphazene materials containing hydroxyl groups. Macromolecules, 1992, vol. 25, no. 10, pp. 2569–2574.
  26. Chistyakov E.M., Terekhov I.V., Shapagin A.V., Filatov S.N., Chuev V.P. Curing of epoxy resin DER-331 by hexakis(4-acetamidophenoxy)cyclotriphosphazene and properties of the prepared composition. Polymers, 2019, vol. 11, no. 7, pp. 1191.
  27. You G., Cai Z., Peng H., Tan X., He H. A Well-Defined Cyclotriphosphazene-Based Epoxy Monomer and Its Application as A Novel Epoxy Resin: Synthesis, Curing Behaviors, and Flame Retardancy. Phosphorus, Sulfur, and Silicon and the Related Elements, 2014, vol. 189, no. 4, pp. 541–550.
  28. Duan H., Chen Y., Ji S. et al. A novel phosphorus/nitrogen-containing polycarboxylic acid endowing epoxy resin with excellent flame retardance and mechanical properties. Chemical Engineering Journal, 2019. Available at: http://www.sciencedirect.com (accessed: April 20, 2020). DOI: 10.1016/j.cej.2019.121916.
  29. Huo S., Wang J., Yang S. et al. Synthesis of a DOPO-containing imidazole curing agent and its application in reactive flame retarded epoxy resin. Polymer Degradation and Stability, 2019, vol. 159, pp. 79–89.
  30. Zhang Q., Yang S., Wang J. et al. A DOPO based reactive flame retardant constructed by multiple heteroaromatic groups and its application on epoxy resin: curing behavior, thermal degradation and flame retardancy. Polymer Degradation and Stability, 2019, vol. 167, pp. 10–20.
  31. Xu M.J., Xu G.R., Leng Y., Li B. Synthesis of a novel flame retardant based on cyclotriphosphazene and DOPO groups and its application in epoxy resins. Polymer Degradation and Stability, 2016, vol. 123, pp. 105–114.
  32. Qian L., Ye L., Qiu Y., Qu S. Thermal degradation behavior of the compound containing phosphaphenanthrene and phosphazene groups and its flame retardant mechanism on epoxy resin. Polymer, 2011, vol. 52, pp. 5486–5493.
  33. Jian R.K., Wang P., Xia L., Zheng X. Effect of a novel P/N/S-containing reactive flame retardant on curing behavior, thermal and flame-retardant properties of epoxy resin. Journal of Analytical and Applied Pyrolysis. 2017, vol. 127, pp. 360–368.
  34. Zhang W.C., Li X.M., Yang R.J. Novel flame retardancy effects of DOPO-POSS on epoxy resins. Polymer Degradation and Stability, 2011, vol. 96, pp. 2167–2173.
  35. Qiu Y., Qian L., Feng H.S. et al. Toughening effect and flame-retardant behaviors of phosphaphenanthrene/phenylsiloxane bigroup macromolecules in epoxy thermoset. Macromolecules, 2018, vol. 51, pp. 9992–10002.
  36. Alagar M., Velen T.V.T., Kumar A.A., Mohan V. Synthesis and characterization of high performance polymeric siliconized epoxy composites for aerospace applications. Materials and Manufacturing Processes, 1999, vol. 14, no. 1, pp. 67–83.
  37. Hsiue G.H., Liu Y.L., Tsiao J. Phosphorus-containing epoxy resin for flame retardancy. V: Synergistic effect of phosphorus-silicon on flame retardancy. Journal of Applied Polymer Science, 2000, vol. 78, no. 1, pp. 1–7.
  38. Wang W.J., Perng L.H., Hsiue G.H., Chang F.C. Characterisation and properties of new silicone-containing epoxy resin. Polymer, 2000, vol. 41, no. 16, pp. 6113–6122.
  39. Hsiue G.H., Wang W.J., Chang F.C. Synthesis, characterization, thermal and flame-retardant properties of silicon-based epoxy resins. Journal of Applied Polymer Science, 1999, vol. 73, no. 7, pp. 1231–1238.
  40. Meenakshi K.S., Sudhan E.P.J., Kumar S.A., Umapathy M.J. Development and characterization of novel DOPO based phosphorus tetraglycidyl epoxy nanocomposites for aerospace applications. Progress in Organic Coatings, 2011, vol. 72, no. 3, pp. 402–409.
  41. Weil E., McSwigan B. Melamine phosphates and pyrophosphates in flame-retardant coatings: old products with new potential. Journal of Coatings Technology, 1994, vol. 66, no. 839, pp. 75–82.
  42. Thermosetting resin composition, prepreg and laminated plate: pat. JP2015166431; filed 04.03.14; publ. 24.09.15.
  43. Thermosetting resin composition, and prepreg, laminated board for wiring board and printed wiring board using the same: pat. JP2012188669; filed 07.05.12; publ. 04.10.12.
  44. Song T., Li Z., Liu J., Yang S. Synthesis, characterization and properties of novel crystalline epoxy resin with good melt flowability and flame retardancy based on an asymmetrical biphenyl unit. Polymer Science Series B, 2013, vol. 55, no. 3–4, pp. 147–157.
  45. Iji M., Kiuchi Y. Flame‐retardant epoxy resin compounds containing novolac derivatives with aromatic compounds. Polymers for Advanced Technologies, 2001, vol. 12, pp. 393–406.
  46. Iji M., Kiuchi Y. Flame resistant glass-epoxy printed wiring boards with no halogen or phosphorus compounds. Journal of Materials Science: Materials in Electronics, 2004, vol. 15, pp. 175–182.
  47. Epoxy resin composition containing reactive flame retardant phosphonate oligomer and filler: pat. EP1570000; filed 07.11.03; publ. 20.09.06.
  48. Dai J., Peng Y., Teng N. et al. High-performing and fire-resistant biobased epoxy resin from renewable sources. ACS Sustainable Chemistry and Engineering, 2018, vol. 6, pp. 7589–7599.