Serpova V.M., Sidorov D.V., Kurbatkina E.I., Shavnev A.A. The destruction of the fibrous metal matrix composites system Ti–SiC under cyclic loads (review) // Proceedings of VIAM. 2020. No. 4-5 (88). Ст. 12. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-45-108-118.

The destruction of the fibrous metal matrix composites system Ti–SiC under cyclic loads (review)

Serpova V.M., Sidorov D.V., Kurbatkina E.I., Shavnev A.A.
Abstract

The paper presents the features of the destruction of fibrous metal matrix composites (ММСs) system Ti–SiC under cyclic loads under the review of foreign scientific and technical literature. The main factors affecting the nature of fracture and the fatigue life of fibrous MCMs system Ti–SiC under cyclic loads with different asymmetry coefficients are considered. The stages of destruction of fibrous MCMs system Ti–SiC under the action of mechanical and thermomechanical fatigue are presented. In conclusion of the review, conclusions are drawn and it is shown that in order to achieve high performance characteristics of parts made of MCMs system Ti–SiC, it is necessary to take into account the structural features of the material.

Keywords
metal matrix composite, aluminum matrix composites, silicon carbide, fiber, titanium matrix composites, fatigue.
Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. What to make the future of? Materials of a new generation, technologies for their creation and processing – the basis of innovation. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  3. Kablov E.N., Valueva M.I., I.V. Zelenina, Khmelnitskiy V.V., Aleksashin V.M. Carbon plastics based on benzoxazine oligomers – perspective materials. Trudy VIAM, 2020, no. 1, paper no. 07. Available at: http://www.viam-works.ru (accessed: February 19, 2020). DOI: 10.18577/2307-6046-2020-0-1-68-77.
  4. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, No. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  5. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  6. Volkov A.M., Vostrikov A.V. Low-cycle fatigue resistance of PM Ni-base superalloys (review). Aviacionnye materialy i tehnologii, 2016, no. S1, pp. 74–79. DOI: 10.18577/2071-9140-2016-0-S1-74-79.
  7. Chawla N., Chawla K.K. Metal Matrix Composites. N.Y.: Springer Sience+Business Media, 2006, pp. 351–379.
  8. Doorbar P.J., Kyle-Henney S. Development of Continuously-Reinforced Metal Matrix Composites for Aerospace Applications. Comprehensive Composite Materials II, 2018, vol. 4, pp. 439–463.
  9. Gorbovets M.A., Kochetkov D.A., Khodinev I.A. The analysis and comparison of the RF and foreign standards for method of thermomechanical fatigue tests. Trudy VIAM, 2017, no. 4, paper no. 11. Available at: http://www.viam-works.ru (accessed: February 04, 2020). DOI: 10.18577/2307-6046-2017-0-4-11-11.
  10. Hayat M.D., Singh H., Zhen H., Peng C. Titatium metal matrix composites: An overiew. Composites Part A: Applied Science and Manufacturing, 2019, vol. 121, pp. 418–438. DOI: 10.1016/j.compositesa.2019.04.005.
  11. Smith P.R., Graves J.A., Rhodes C. Comparison of orthorhombic and alpha-two titanium aluminides as matrices for continuous SiC-reinforced composites. Metallurgical Materials Transaction A, 1994, vol. 25A, pp. 1267–1283. DOI: 10.1007/BF02652301.
  12. Guanghai F., Yanqing Y., Jian L. et al. Fatigue behavior and damage evolution of SiC Fiber reinforced Ti–6Al–4V alloy matrix composites. Rare Metal Materials and Engineering, 2014, vol. 43, is. 9, p. 2049–2054. DOI: 10.1016/S1875-5372(14)60146-6.
  13. Neu R.W. A mechanistic-based thermomechanical fatigue life prediction model for metal matrix composites. Fatigue & Fracture of Engineering Materials and Structures, 1993, vol. 16, is. 8, p. 811–828. DOI: 10.1111/j.1460-2695.1993.tb00121.x.
  14. Leyens C., Kocian F., Hausmann J., Kaysser W.A. Materials and design concepts for high performance compressor components. Aerospace Science Technology, 2003, vol. 7, is. 3, P. 201–210. DOI: 10.1016/S1270-9638(02)00013-5.
  15. Durodola J.F., Derby B., Ruiz C. Fatigue characterization of Ti–6Al–4V/SiC metal-matrix composites. International Journal of Fatigue, 1994, vol. 16, is. 7, pp. 461–467. DOI: 10.1016/0142-1123(94)90196-1.
  16. Covey S.J., Lerch B.A., Jayaraman N. Fiber volume fraction effects on fatigue crack growth in SiC/Ti-15-3 composite. Materials Science and Engineering: A, 1995, vol. 200, is. 1–2, pp. 68–77. DOI: 10.1016/0921-5093(95)07007-9.
  17. González C., Llorca J. Micromechanical modelling of deformation and failure in Ti–6Al–4V/SiC composites. Acta Materialia, 2001, vol. 49, is. 17, pp. 3505–3519. DOI: 10.1016/s1359-6454(01)00246-4.
  18. Gundel D.B., Wawner F.E. Experimental and theoretical assessment of the longitudinal tensile strength of unidirectional SiC-fiber/titanium-matrix composites. Composites Science and Technology, 1997, vol. 57, is. 4, pp. 471–481. DOI: 10.1016/s0266-3538(96)00163-7.
  19. Boyum E.A., Mall S. Fatigue behavior of a cross-ply titanium matrix composite under tension-tension and tension-compression cycling. Materials Science and Engineering: A, 1995, vol. 200, pp. 1–11. DOI: 10.1016/0921-5093(95)07006-0.
  20. Gabb T.P., Gayda J., Mackay R. A. Isothermal and Nonisothermal Fatigue Behavior of a Metal Matrix Composite. Journal of Composite Materials, 1990, vol. 24, pp. 667–686. DOI: 10.1177/002199839002400605.
  21. Mall S., Portner B. Characterization of Fatigue Behavior in Cross-Ply Laminate of SCS-6/Ti-15-3 Metal Matrix Composite at Elevated Temperature. Journal of Engineering Materials and Technology, 1992, vol. 114, pp. 409–415. DOI:10.1115/1.2904193.
  22. Mall S., Schubbe J. Thermo-mechanical fatigue behavior of a cross-ply SCS-6/Ti-15-3 metal-matrix composite. Composites Science and Technology, 1994, vol. 50, pp. 49–57. DOI: 10.1016/0266-3538(94)90125-2.
  23. Mall S., Ermer P.G. Thermal Fatigue Behavior of a Unidirectional SCS6/Ti-15-3 Metal Matrix Composite. Journal of Composite Materials, 1991, vol. 25, pp. 1668–1686. DOI: 10.1177/002199839102501207.