Postnov V.I., Postnova M.V., Bogatov V.A., Strelnikov S.V. Influence laser are sharp on properties plexiglasses // Proceedings of VIAM. 2020. No. 4-5 (88). Ст. 11. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-45-100-107.

Influence laser are sharp on properties plexiglasses

Postnov V.I., Postnova M.V., Bogatov V.A., Strelnikov S.V.
Abstract

Growth of volumes of output of products from nonmetallic materials demands introduction in manufacture of products from them modern highly productive technologies. In this connection in the given work possibility of use of laser radiation for cutting details from organic glasses is considered, are spent comparative strength tests of samples received by means of laser and mechanical cutting. As results of researches on influence of thermal radiation laser beam cutting on residual pressure in plexiglass and in particular on it «silverfirmness» are resulted.

Keywords
plexiglass, the laser, residual pressure, durability, zone of thermal effect.
Reference list
  1. 1. Kablov E.N. Materials of a new generation - the basis of innovation, technological leadership and national security of Russia. Intellekt & Tekhnologii, 2016, no. 2, pp. 41–46.
  2. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Podzhivotov N.Yu., Kablov E.N., Antipov V.V., Erasov V.S., Serebrennikova N.Yu., Abdulin M.R., Limonin M.V. Layered metal-polymer materials in aircraft structural elements. Perspektivnyye materialy, 2016, no. 10, pp. 5–19.
  4. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, No. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  5. Sentyurin E.G., Mekalina I.V., Ajzatulina M.K., Isaenkova Yu.A. The history of aircraft materials of glass and polymer materials with special properties (To the 75th anniversary Laboratory of polymer materials with special properties). Aviacionnye materialy i tehnologii, 2017, No. 3 (48), pp. 81–86. DOI: 10.18577/2071-9140-2017-0-3-81-86.
  6. Grigoryants A.G. Fundamentals of laser processing of materials. Moscow: Mashinostroyenie, 1989, 304 p.
  7. Postnov V.I., Postnova M.V. The mechanics of processes for cutting polymer materials with a laser. Mekhanika i protsessy upravleniya: sb. nauch. tr. Ulyanovsk: Ulyanovskiy gos. tekhn. un-t, 2000, pp. 64–70.
  8. Vinogradov B.A., Gavrilenko V.N., Lee Benson M.N. The theoretical basis of the effects of laser radiation on materials. Blagoveshchensk: BPI, 1993, 344 pp.
  9. Golubenko Yu.V., Bondarev A.V., Ponomarenko K.V. Laser cutting of polymers and non-metallic composite materials. Tekhnologiya mashinostroyeniya, 2005, no. 10, pp. 57–59.
  10. Postnov V.I., Postnov M.V., Postnov A.V. Study of the parameters of laser cutting of prepregs from organotissue. Sbornik materialov III Vseros. nauch.-prakt. konf. «Sovremennyye tekhnologii v mashinostroyenii». Penza: Privolzhskiy dom znaniy, 2000, pp. 35–38.
  11. Kharitonov G.M., Yakovlev N.O., Mekalina I.V. Influence of physicomechanical characteristics of organic glasses on tension in aircraft glazing at aerodynamic heating. Aviacionnye materialy i tehnologii, 2015, no. S1, pp. 56–60. DOI: 10.18577/2071-9140-2015-0-S1-56-60.
  12. Methods of testing, control and research of engineering materials: a reference manual: in 3 vol. / Ed. A.T. Tumanov. Moscow: Mashinostroyenie, 1973, vol. 3: Metody issledovaniya nemetallicheskikh materialov, 146 p.
  13. Akseeva R.M., Zaikova G.E. Combustion of polymer materials. Moscow: Nauka, 1981, 280 pp.
  14. Khalturinsky N.A., Berlin A.A. Regularities of the macrokinetics of the pyrolysis of polymers. Uspekhi khimii, 1983, vol. 52, no. 12, pp. 2819–2838.
  15. Aseeva R.M., Smutkina Z.S., Berlin A.A., Kasatokin V.I. On the thermal transformations of carbo- and hetero-chain polymers. Strukturnaya khimiya ugleroda i ugley. Moscow: Nauka, 1969, pp. 161–200.