Batienkov R.V., Efimochkin I.Yu., Kolyshev S.G., Khudnev A.A. The effect of heat treatment on the structure and mechanical properties of an alloy of the Mo–Ti–Zr–C system obtained by electric pulse plasma sintering // Proceedings of VIAM. 2020. No. 4-5 (88). Ст. 01. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-45-3-12.

The effect of heat treatment on the structure and mechanical properties of an alloy of the Mo–Ti–Zr–C system obtained by electric pulse plasma sintering

Batienkov R.V., Efimochkin I.Yu., Kolyshev S.G., Khudnev A.A.
Abstract

The characteristics of structural changes during heat treatment of Mo–Ti–Zr–С powder alloy obtained by spark plasma sintering were studied. The sintering conditions to obtain nearly theoretical density were worked out. The mechanical and physical characteristics like density, bending strength and plasticity were defined. In order to improve mechanical properties of the material and to obtain dispersion-strengthened structure the heat treatment was carried out. After this the material’s structure was investigated using optical and scanning electron microscopy and mechanical tests were carried out.

Keywords
molybdenum, dispersion-reinforced composite, powder metallurgy, spark plasma sintering, heat treatment.
Reference list
  1. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  2. Kablov E.N. The key problem is materials. Tendentsii i oriyentiry innovatsionnogo razvitiya Rossii. Moscow: VIAM, 2015, pp. 458–464.
  3. Kablov E.N. Materials of a new generation – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  4. Ospennikova O.G., Podieiachev V.N., Stoliankov Yu.V. Refractory alloys for innovative equipment. Trudy VIAM, 2016, no. 10, paper no. 5. Available at: http://www.viam-works.ru (accessed: October 01, 20179). DOI: 10.18577/2307-6046-2016-0-10-5-5.
  5. Morgunova N.N., Klypin B.A., Boyarshinov V.A. et al. Molybdenum alloys. Moscow: Metallurgiya, 1975, 392 p.
  6. Grashchenkov D.V., Efimochkin I.Yu., Bolshakova A.N. High-temperature metal-matrix composite materials reinforced with particles and fibers of refractory compounds. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 318–328. DOI: 10.18577/2071-9140-2017-0-S-318-328.
  7. Majumdar S., Sharma I.G. Development of Mo base TZM (Mo–0.5Ti–0.1Zr–0.02C) alloy and its shapes. BARC Newsletter, 2010, vol. 312, pp. 21–27.
  8. Batiyenkov R.V., Bolshakova A.N., Efimochkin I.Yu. The problem of low-temperature plasticity of molybdenum and alloys based on it (review). Trudy VIAM, 2018, no. 3 (63), paper no. 02. Available at: http://www.viam-works.ru (accessed: April 11, 2019). DOI: 10.18577/2307-6046-2018-0-3-12-17.
  9. Majumdar S., Kapoor R., Raveendra S. et al. A study of hot deformation behavior and microstructural characterization of Mo–TZM alloy. Journal of Nuclear Materials, 2009, vol. 385 (3), pp. 545–551.
  10. Yavas B., Sahin F., Yucel O., Goller G. Preparation of Pre-Alloyed TZM Alloy with Addition of B4C by Using Spark Plasma Sintering. 6th International Conference on Materials Science and Technologies, 2016, pp. 75–76.
  11. Torresillas San Millan R., Pinargote Solis N.V., Okunkova A.A., Peretyagin P.Yu. Fundamentals of the process of spark plasma sintering of nanopowders. Moscow: Tekhnosfera, 2014. 96 p.
  12. ASTM B386-03. Standard Specification for Molybdenum and Molybdenum Alloy Plate, Sheet, Strip, and Foil. West Conshohocken: ASTM International, 2003, pp. 1–5.
  13. Batienkov R.V., Efimochkin I.Yu., Khudnev A.A. The research of a specific electrical conductivity of Mo–W powder alloys obtained by SPS. Trudy VIAM, 2019, no. 7 (79), paper no. 06. Available at: http://www.viam-works.ru (accessed: October 01, 2019). DOI: 10.18577 / 2307-6046-2019-0-7-50-58.
  14. Arzamasov B.N., Sidorin I.I., Kosolapov G.F. et al. Material science: textbook for technical colleges. 2nd ed., rev. and add. Moscow: Mashinostroyeniye, 1986, 384 p.
  15. Livshits B.G., Kraposhin V.S., Linetskiy Ya.L. Physical properties of metals and alloys. Moscow: Metallurgiya, 1980. 318 p.
  16. Danisman C.B., Yavas B., Yucel O. et al. Processing and characterization of spark plasma sintered TZM alloy. Journal of Alloys and Compounds, 2016, vol. 685, pp. 860–868.