Kondrashov E.K., Naidenov N.D. Erosion-resistant paint and varnish coatings for aviation purposes. Part 2. Elastomeric erosion resistant radio-transparent coatings (review) // Proceedings of VIAM. 2020. No. 3 (87). Ст. 10. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-3-94-101.

Erosion-resistant paint and varnish coatings for aviation purposes

Part 2. Elastomeric erosion resistant radio-transparent coatings (review)
Kondrashov E.K., Naidenov N.D.
Abstract

This paper summarizes the results of research on the development of erosion-resistant coatings based on epoxy, polyurethane and polyimide film formers with heat resistance up to 350 °С. It is established that the erosion resistance of coatings depends not only on their strength and elongation, but also on their dynamic parameters and the properties of fillers. The second part of the article summarizes the results of research on the development of elastomeric erosion-resistant coatings based on chlorosulfated polyethylene and fluoro-rubber with heat resistance up to 250 °С, as well as coating systems with erosion-resistant enamels based on these elastomers designed to protect against erosion of radio-transparent antenna fairings made of fiberglass.

Keywords
erosion resistance, cycles, temperature resistance, chlorosulfonated polyethylene, fluorinated rubber.
Reference list
  1. Kondrashov E.K., Naidenov N.D. Erosion resistant paint coverings of aviation purpose. Part 1. Erosion resistant paint coatings based on epoxy and polyurethane films forming (review). Trudy VIAM, 2020, no. 2 (86), paper no. 09. Available at: http://www.viam-works.ru (accessed: February 20, 2020). DOI: 10.18577/2307-6046-2020-0-2-81-90.
  2. Chebotarevskiy V.V., Kondrashov E.K. Technology of coatings in mechanical engineering. Moscow: Mashinostroyeniye, 1978, 296 p.
  3. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  4. Buznik V.M., Kablov E.N., Koshurina A.A. Materials for complex technical devices of the Arctic application. Nauchno-tekhnicheskiye problemy osvoyeniya Arktiki. Moscow: Nauka, 2015, pp. 275–285.
  5. Kablov E.N. Quality control of materials – a guarantee of the safety of operation of aircraft. Aviacionnye materialy i tehnologii, 2001, no. 1, pp. 3–8.
  6. Erosion. Ed. Yu.V. Polezhaev. Moscow: Mir, 1982, 2644 p.
  7. Kashcheev V.N. Abrasive destruction of solids. Moscow: Nauka, 1970, 248 p.
  8. Kleis I.R. Theory of friction, wear and standardization problems. Bryansk, 1978, 387 p.
  9. Ratner A.V., Zelinsky V.G. Erosion of materials of heat power equipment. Moscow; Leningrad: Energiya, 1966, 271 p.
  10. Urvantsev L.A. Erosion and metal protection. Moscow: Mashinostroyeniye, 1966, 235 p.
  11. Gorlin S.M. Experimental aeromechanics. Moscow: Vysshaya shkola, 1970, 424 p.
  12. Kozyrev S.P. Hydroabrasive wear of metals during cavitation. Moscow: Mashinostroyeniye, 1964, 139 p.
  13. Perelman R.G. Erosive strength of engine parts and aircraft power plants. Moscow: Mashinostroyeniye, 1980. 246 p.
  14. Kondrashov E.K. Heat-resistant putties on base silicone resins. Trudy VIAM, 2017, no. 10 (58), paper no. 07. Available at: http://www.viam-works.ru (accessed: January 12, 2020). DOI: 10.18577/2307-6046-2017-0-10-7-7.
  15. Kondrashov E.K. Erosion-resistant radiolucent enamel VE-14. Aviatsionnaya promyshlennost, 1976, no. 1, pp. 67–68.
  16. Goldberg M.M. Materials for coatings. Moscow: Khimiya, 1972 344 p.
  17. ЛPaintwork materials: reference book. Ed. I.N. Sapgira. Moscow: Izd-vo khim. lit., 1961. 506 p.
  18. Paintwork materials. Technical requirements and quality control. Мoscow: Khimiya, 1977, vol. 2. 286 p.
  19. Semenova L.V., Novikova T.A., Nefedov N.I. Study of removing ability of removers for paint systems removal. Aviacionnye materialy i tehnologii, 2017, no. 1 (46), pp. 32–37. DOI: 10.18577 / 2071-9140-2017-0-1-32-37.
  20. Elastomer coated layer for erosion and/or fire protection: pat. US5908528; field 16.04.98; publ. 06.01.99.
  21. Elastomer coated layer for erosion and/or fire protection: pat. US5912195; field 16.04.98; publ. 15.06.99.
  22. Kuznetsova V.A., Shapovalov G.G. Tendencies of development of the erosion-resistant coatings (review. Trudy VIAM, 2018, no. 11 (71), paper no. 09. Available at: http://www.viam-works.ru (accessed: January 12, 2020). DOI: 10.18577/2307-6046-2018-0-11-74-85.
  23. Zhelezina G.F., Solovyeva N.A., Makrushin K.V., Rysin L.S. Polymer composite materials for manufacturing engine air particle separation of advanced helicopter engine. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 58–63. DOI: 10.18577/2071-9140-2018-0-1-58-63.
  24. Pavlyuk B.Ph. The main directions in the field of development of polymeric functional materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 388–392. DOI: 10.18577/2071-9140-2017-0-S-388-392.
  25. Grashchenkov D.V. Strategy of development of non-metallic materials, metal composite materials and heat-shielding. Aviacionnye materialy i tehnologii, 2017, No. S, pp. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.