Stepanova E.V., Zimichev A.M. Thermal insulation material for cords made of refractory oxide fibers // Proceedings of VIAM. 2020. No. 2 (86). Ст. 08. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-2-72-80.

Thermal insulation material for cords made of refractory oxide fibers

Stepanova E.V., Zimichev A.M.
Abstract

The work is devoted to production of heat-insulating materials from refractory fibers of aluminium oxide and silicon. Refractory fibres are prepared by sol-gel technology from highly viscous solutions based on precursors of water-soluble aluminium salts with addition of fibre-forming component to the solution. Methods of scanning differential calorimetry and gravimetric studies during heating have studied the processes of changing the composition and structure of oxide fibers. Mechanical properties of sealing cords with refractory fiber core were tested.

Keywords
fibers, heat-resistant oxides, heat insulation, linear density, examination structura, cord, temperature.
Reference list
  1. Ivakhnenko Yu.A., Baruzdin B.V., Varrik N.M., Maksimov V.G. High-temperature fibrous sealing materials. Aviacionnye materialy i tehnologii, 2017, No. S, pp. 272–289. DOI: 10.18577/2071-9140-2017-0-S-272-289.
  2. Kablov E.N. Russia needs new generation materials. Redkiye zemli, 2014, no. 3, pp. 8–13.
  3. Kablov E.N. Materials of a new generation - the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  4. Kablov E.N. Formation of domestic space materials science. Vestnik RFFI, 2017, no. 3, pp. 97–105.
  5. Kablov E.N. At the crossroads of science, education and industry. Ekspert, 2015, no. 15 (941), pp. 49–53.
  6. Babashov V.G., Varrik N.M. Thermal insulation materials for modern aircraft. Novosti materialovedeniya. Nauka i tekhnika, 2016, no. 3 (21), paper no. 01. Available at: http://www.materialsnews.ru (accessed: October 28, 2019).
  7. High temperature rope seal type joint packing: pat. US5301595; filed 25.06.92; publ. 12.04.94.
  8. Balinova Yu.A. Continuous polycrystalline alumina fibers for composite materials: thesis, Cand. Sc. (Tech.). Moscow: VIAM, 2012, 19 p.
  9. Control surface seal development for future re-entry vehicles: technical report / NASA. Available at: http: //www.ntrs.nasa.gov.search.jsp (accessed: October 29, 2019).
  10. High temperature resistant rope system and methods: pat. US7437437869; filed 30.01.07; publ. 21.10.08.
  11. Istomin A.V., Kolyshev S.G. Electrostatic method of forming ultrathin fibers of refractory oxides. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 40–46. DOI: 10.18577/2071-9140-2019-0-2-40-46.
  12. A method of obtaining a combined yarn based on short fibers and a device for its implementation: pat. 2419692 Rus. Federation; filed 29.04.10; publ. 27.05.11.
  13. Balinova Yu.A., Kiriyenko T.A. Continuous high-temperature oxide fibers for heat-shielding, heat-insulating and composite materials. Vse materialy. Entsiklopedicheskiy spravochnik, 2012, no. 4, pp. 24–29.
  14. Zimichev A.M., Varrik N.M., Sumin A.V. On the issue of ceramic yarns based on refractory oxides. Novosti materialovedeniya. Nauka i tekhnika, 2016, no. 3 (21), paper no. 09. Available at: http://www.materialsnews.ru (accessed: November 05, 2019).
  15. Zimichev A.M., Varrik N.M. Thermogravimetric researches of alumina-based filaments. Trudy VIAM, 2014, no. 6, paper no. 6. Available at: http://www.viam-works.ru (accessed: November 05, 2019). DOI: 10.18577/2307-6046-2014-0-6-6-6.
  16. Butakov V.V., Basargin O.V., Babashov V.G., Ivakhnenko Yu.A. A behavioral model of the fibrous material during bending tests. Trudy VIAM, 2014, no. 12, paper no. 6. Available at: http://www.viam-works.ru (accessed: October 30, 2019). DOI: 10.18577/2307-6046-2014-0-12-6-6.