Zhitnyuk S.V., Sorokin O.Ju., Juravleva P.L. Silicon carbide ceramics obtained by sintering granular powder // Proceedings of VIAM. 2020. No. 2 (86). Ст. 06. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-2-50-59.

Silicon carbide ceramics obtained by sintering granular powder

Zhitnyuk S.V., Sorokin O.Ju., Juravleva P.L.
Abstract

Silicon carbide-based ceramics with an addition of 1% wt. boron carbide were synthesized by spark plasma sintering at a firing temperature of 2000 °C. The resulting material had a three-point bending strength of 420±20 MPa, a relative density of 98,7% and an open porosity of 0,2%. The comparison of microstructure, phase composition, open porosity and relative density of ceramics obtained by pressureless sintering in the argon atmosphere and spark plasma sintering is carried out.

Keywords
silicon carbide, microstructure, mechanical properties, uniaxial pressing, pressureless sintering, spark plasma sintering.
Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Folomeikin Yu.I., Stolyarova V.L., Lopatin S.I. The processes of interaction of niobium-silicon melt with refractory ceramics. Zhurnal obshchey khimii, 2016, vol. 86, no. 9, pp. 1542-1546.
  3. Kablov E.N. The role of chemistry in creating new generation materials for complex technical systems. Tez. dokl. XX Mendeleyevskogo sezda po obshchey i prikladnoy khimii. UrO RAN, 2016, pp. 25–26.
  4. Kablov E.N., Zhestkov B.E., Grashchenkov D.V., Sorokin O.Yu., Lebedeva Yu.E., Vaganova M.L. Investigation of the oxidative stability of a high-temperature coating on a SiC material under the influence of a high enthalpy flow. Teplofizika vysokikh temperatur, 2017, vol. 55, no. 6, pp. 704–711.
  5. Berezovskij V.V., Shavnev A.A., Lomov S.B., Kurganova Yu.A. Receiving and the analysis of structure of the disperse strengthened composite materials of Al–SiC system with the different maintenance of the reinforcing phase. Aviacionnye materialy i tehnologii, 2014, no. S6, pp. 17–23. DOI: 10.185577/2071-9140-2014-0-S6-17-23.
  6. Sorokin O.Yu., Solntsev S.St., Evdokimov S.A., Osin I.V. Hybrid spark plasma sintering method: principle, possibilities, future prospects, Aviacionnye materialy i tehnologii, 2014, no. S6, pp. 11–16. DOI: 10.18577/2071-9140-2014-0-s6-11-16.
  7. Grishina O.I., Shavnev A.A., Serpova V.M. Features of influence of structural parameters on mechanical properties of metallic composite material based on particle-reinforced aluminum alloys by silicon carbide. Aviacionnye materialy i tehnologii, 2014, no. S6, pp. 24–27. DOI: 10.18577/2071-9140-2014-0-s6-24-27.
  8. Kurbatkina E.I., Kosolapov D.V., Hodykin L.G., Nigmetov M.S. Influence of the silicon addition on the phase composition of aluminum composite materials reinforced with silicone carbide particles. Aviacionnye materialy i tehnologii, 2014, no. S6, pp. 35–38. DOI: 10.18577/2071-9140-2014-0-s6-35-38.
  9. Zhitnyuk S.V. Ceramics based on silicon carbide, modified by additives of eutectic composition: thesis, Cand. Sc. (Tech.). Moscow: RCTU them. D.I. Mendeleev, 2014, 174 p.
  10. Balkevich V.L. Technical ceramics. Moscow: Stroyizdat, 1984, 256 p.
  11. Low I.M., Sakka Y., Hu C.F. MAX phases and ultra-high temperature ceramics for extreme environments. Engineering Science Reference, 2013, 649 p.
  12. Heimann R.B. Classic and Advanced Ceramics: From Fundamentals to Applications. Weinheim: WILEY-VCH Verlag GmbH & Co. KGaA, 2010, 553 p.
  13. Perevislov S.N. The role of structural modification of sintered and hot-pressed SiC materials. Ogneupory i tekhnicheskaya keramika, 2018, no. 10, pp. 18–24.
  14. Kuzmin R.I., Veselov S.V., Cherkasova N.Yu., Felofyanova A.V., Kvashnin V.I., Zykova E.D. The influence of preliminary free sintering of Al2O3–(3Y)ZrO2 ceramics on the structure and properties of preforms for subsequent HIP. Ogneupory i tekhnicheskaya keramika, 2018, no. 11-12, pp. 16-21.
  15. State Standard 2409–2014. Refractories. Method for determining apparent density, open and total porosity, water absorption. Moscow: Standartinform, 2014, 7 p.
  16. State Standard 24409–80. Ceramic electrotechnical materials. Test methods. Moscow: Standartinform, 2005,30 s.
  17. Cherkasova N.Yu., Veselov S.V., Felofyanova A.V., Kuzmin R.I., Maksimov R.A., Khabirov R.R. The effect of the molecular weight of the PEG processing aid on the structure and properties 3Y – TZP ceramics. Ogneupory i tekhnicheskaya keramika, 2018, no. 11-12, pp. 9–15.
  18. Fides M., Kovalcikova A., Hvizdos P. et al. Mechanical and tribological properties of electrically conductive SiC based cermets. International Journal of Refractory Metals and Hard Materials, 2017, no. 65, pp. 76–82.
  19. Shevchenko V.Ya. Introduction to technical ceramics. Moscow: Nauka, 1993, 112 p.
  20. Seo Y.-K., Kim Y.-W., Kim K.-J., Seo W.-S. Electrically conductive SiC–BN composites. Journal of the European Ceramic Society, 2016, vol. 16, no. 36, pp. 3879–3887.