Krylov S.А., Makarov А.А., Druzhnov M.A. Study of high-strength low-alloy steel with super-equilibrium nitrogen content // Proceedings of VIAM. 2020. No. 12 (94). Ст. 01. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-12-3-13.

Study of high-strength low-alloy steel with super-equilibrium nitrogen content

Krylov S.А., Makarov А.А., Druzhnov M.A.
Abstract

In continuation of joint work of FSUE «VIAM» and IMET RAN named after Baikov, in the field of obtaining low-alloy steels with increased mechanical properties with a super-equilibrium nitrogen content, the mechanical properties, structure, and chemical composition of the obtained steel were studied. It is shown that steel 10KH3A with a super-equilibrium nitrogen content (up to 0,2) electroslag remelting under pressure DESHP-0,1 (FSUE «VIAM») provides a high level of properties (ultimate strength 1670 MPa) while maintaining high mechanical characteristics (elongation 10%, constriction 50%).

Keywords
high-strength steel, low-alloy steel, nitrogen-containing steel, nitrogen, super-equilibrium nitrogen content, electroslag remelting under pressure, structure, mechanical properties.
Reference list
  1. Kablov E.N. Innovative development is the most important priority of the state. Metally Evrazii, 2010, no. 2, pp. 6–11.
  2. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Kablov E.N., Lomberg B.S., Ospennikova O.G. Creation of modern heat-resistant materials and technologies for their production for aircraft engine building. Krylya Rodiny, 2012, no. 3–4, pp. 34–38.
  4. Kablov E.N., Ospennikova O.G., Lomberg B.S., Sidorov V.V. Priority directions of development of technologies for the production of heat-resistant materials for aircraft engine building. Problemy chernoy metallurgii i materialovedeniya, 2013, no. 3, pp. 47–54.
  5. Rashev Ts.V., Eliseev A.V., Zhekova L.Ts., Bogev P.V. High-nitrogen steels. Izvestiya vysshikh uchebnykh zavedeniy. Chernaya metallurgiya, 2019, vol. 62, no. 7, pp. 503–510. DOI: 10.17073/0368-0797-2019-7-503-510.
  6. Gavriljuk V.G., Berns H. High Nitrogen Steels: Structure, Properties, Manufacture, Applications. Berlin: Heidelberg; New York: Springer-Verlag, 1999, 379 p.
  7. Stein G., Hucklenbroich I. Manufacturing and Applications of High Nitrogen Steels. Journal Materials and Manufacturing Processes, 2004, vol. 19, is. 1, p. 7–17.
  8. High Nitrogen Steels and Stainless Steels. Manufacturing, Properties and Applications. Ed. B. Raj. Woodhead Publishing, 2004. 224 p.
  9. Speidel M.O. Nitrogen Containing Austenitic Stainless Steels. Mathematischnaturwissenschaftlichen und Werkstofftechnik, 2006, vol. 37, no. 10, pp. 876–880.
  10. Rashev Ts.V., Zhekova L.Ts., Bogev P.V. On the development of metallurgy under pressure. News of higher educational institutions. Ferrous metallurgy, 2017, vol. 60, no. 1, pp. 60–66. DOI: 10.17073/0368-0797-2017-1-60-66.
  11. High-strength low-alloy nitrogen-containing martensitic steel: pat. 2638873 Rus. Federation; filed 26.12.16; publ. 18.12.17.
  12. Bannykh O.A., Blinov V.M., Kostina M.V. Structure and properties of low-alloyed high-nitrogen martensitic steels. Metallovedeniye i termicheskaya obrabotka metallov, 2003, no. 2, pp. 3–7.
  13. Blinov V.M., Kostina M.V., Lukin E.I., Blinov E.V., Rigina L.G., Muradyan S.O. Influence of heat treatment on the structure and mechanical properties of low-alloy steel 10Kh3A with a super-equilibrium nitrogen content. Deformatsiya i razrusheniye materialov, 2019, no. 7, pp. 38–41.
  14. Rigina L.G. Research and development of ESR and ESRD technology for chrome-manganese steels alloyed with nitrogen: thesis, Cand. Sc. (Tech.). Moscow: TsNIITMASh, 2005, 146 p.
  15. Krylov S.A., Evgenov A.G., Shherbakov A.I., Makarov A.A. New pressure electroslag remelting furnace PESR-0,1: development and prospects for improvement. Trudy VIAM, 2016, no. 5, paper no. 04. Available at: http://www.viam-works.ru (accessed: August 6, 2020). DOI: 10.18577/2307-6046-2016-0-5-4-4.
  16. Krylov S.A., Evgenov A.G., Makarov A.A., Tonysheva O.A. The ingot PESR. Trudy VIAM, 2017, no. 3, paper no. 03. Available at: http://www.viam-works.ru (accessed: July 21, 2020). DOI: 10.18577/2307-6046-2017-0-3-3-3.
  17. Kostina M.V., Rigina L.G., Blinov V.M., Muradyan S.O., Krylov S.A. Technology of obtaining low-alloy martensitic steel 10Kh3A with super-equilibrium nitrogen content. Elektrometallurgiya, 2019, no. 2, pp. 18–26. DOI: 10.31044/1684-5781-2019-0-2-18-26.
  18. Rigina L.G., Vasiliev Ya.M., Dub V.S. et al. Alloying steels with nitrogen. Elektrometallurgiya, 2005, no. 2, pp. 14–19.
  19. Krylov S.A., Shcherbakov A.I., Makarov A.A., Tonysheva O.A. Reduction of non-metallic inclusions in the nitrogen-containing corrosion-resistant steels. Trudy VIAM, 2017, no. 5 (53), paper no. 01. Available at: http://www.viam-works.ru (accessed: June 08, 2020). DOI: 10.18577/2307-6046-2017-0-5-1-1.
  20. Shestakov I.I., Voznesenskaya N.M., Tonysheva O.A. Influence of high-temperature thermomechanical treatment on the structure and properties of high-strength corrosion-resistant steel of grade 17H13N4К6SАМ3ch. Trudy VIAM, 2016, no. 6 (42), paper no. 02. Available at: http://viam-works.ru (access: July 13, 2020). DOI: 10.18577/2307-6046-2016-0-6-2-2.
  21. Bernstein M.L., Zaimovsky V.A. Structure and mechanical properties of metals. Moscow: Metallurgiya, 1969, 472 p.
  22. Bernstein M.L. The structure of deformed metals. Moscow: Metallurgiya, 1977, 431 p.
  23. Metals and alloys: reference book. Ed. Yu.P. Solntsev. Saint Petersburg: Professional; Peace and Family, 2003, 1066 p.
  24. Barannikova S.A., Zuev L.B. The effect of Interstitial Impurity Content in Austenitic Steel Monocrystals. High Nitrogen Steels, 2009 (MISIS, Moscow, 2009), 189 p.