Abstract

A review of the scientific technical literature in the field of modern research on silicone rubber compositions with high temperature resistance, including those with fire-resistant properties, is presented. The polymer bases and heat-stabilizing and flame-retardant additives used in the developments, as well as methods for preparing rubber mixes and rubbers are shown. Features of compounding materials with a combination of heat resistance and fire-resistance are noted. The relevance of research for the needs of aviation equipment is shown.

Keywords
rubber, silicone composition, rubber mix, vulcanization, heat resistance, flame retardancy.
Reference list
  1. Alifanov E.V., Chajkun A.M., Naumov I.S., Eliseev O.A. Elastomeric materials with high heat resistance (review). Trudy VIAM, 2017, no. 2 (50), paper no. 06. Available at: http://www.viam-works.ru (accessed: August 30, 2020). DOI: 10.18577/2307-6046-2017-0-2-6-6.
  2. Chaikun A.M., Venediktova M.A., Bryk Ya.A. Development of the compounding of rubber extremely high heat resistance with temperature range of exploitation from the -60 to +500°С. Trudy VIAM, 2019, no. 1 (73), paper no. 03. Available at: http://viam-works.ru (accessed: August 30, 2020). DOI: 10.18577/2307-6046-2019-0-1-21-30.
  3. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  4. Kablov E.N. Materials of a new generation – the basis of innovation, technological leadership and national security of Russia. Intellekt i technologii, 2016, no. 2 (14), pp. 16–21.
  5. Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  6. Kablov E.N. The role of chemistry in the creation of new generation materials for complex technical systems. Reports of XX Mendeleev Congress on General and Applied Chemistry. Ekaterinburg: UB of RAS, 2016, pp. 25–26.
  7. Laptev A.B., Barbotko S.L., Nikolaev E.V. The main research areas of the persistence properties of materials under the influence of climatic and operational factors. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 547–561. DOI: 10.18577/2071-9140-2017-0-S-547-561.
  8. Naumov I.S., Petrova A.P., Barbotko S.L., Vaniev M.A., Demidov D.V. Colored and black sealing rubbers of low combustibility based on siloxane rubbers. Vse materialy. Entsiklopedicheskiy spravochnik, 2017, no. 5, pp. 24–31.
  9. Reznichenko S.V., Morozov Yu.L. Great reference book of the rubber-maker. Moscow: Techinform, 2012., 744 p.
  10. High temperature mixing silicone rubber as well as preparation method and application thereof: pat. CN104761911B; filed 03.04.15; publ. 22.02.17.
  11. Heat-resistant composition based on siloxane block copolymer: pat. 2196154C2 Rus. Federation; filed 26.12.00; publ. 20.01.03.
  12. Todd H.E., Miazga J.F. Properties of Silicone Rubber for High-Temperature Static Seals. SAE Transactions, 1960, vol. 68, pp. 224–231.
  13. Heat resistant silicone rubber composition: pat. US9803062B2; filed 23.05.14; publ. 31.10.17.
  14. High-temperature resistant silicon rubber and preparation method thereof: pat. CN102061093A; filed 18.11.10; publ. 18.05.11.
  15. Mixed rubber for high-temperature-resistant silicon rubber die: pat. CN102796290A; filed 31.08.12; publ. 28.11.12.
  16. A kind of low cost high-temperature resisting methyl vinyl silicone rubber: pat. CN108102385A; filed 25.11.17; publ. 01.06.18.
  17. Su Z.-T., Wang J.-H. Properties of silicone rubber at high or low temperature. 2006. Available at: https://www.researchgate.net/publication/296737966_Properties_of_silicone_rubber_at_high_or_low_temperature (дата обращения: 30.08.2020).
  18. High-temperature-resistant silicon rubber additive and method: pat. CN102643550A; filed 28.04.12; publ. 22.08.12.
  19. High-temperature resisting methyl vinyl silicone rubber: pat. CN101735620B; filed 27.12.09; publ. 03.08.11.
  20. Heat-resistant silicone rubber composition and its molded product: pat. JP2001348481A; filed 09.06.00; publ. 18.12.01.
  21. Heat-resistant silicone rubber composition and molded article obtained by curing the composition: pat. JP2002220532A; filed 25.01.01; publ. 09.08.02.
  22. High-temperature-resisting silicon rubber and preparation method thereof: pat. CN104725862A; filed 17.12.14; publ. 24.06.15.
  23. Flame-retardant silicone rubber: pat. JP2006176778A; filed 21.12.05; publ. 06.07.06.
  24. Flame-retardant silicone rubber composition and flame-retardant silicone rubber molding using the same: pat. JPH09188815A; filed 05.01.96; publ. 03.02.04.
  25. Novel high-temperature-resistant silicon rubber and preparation method thereof: pat. CN111040454A; filed 30.12.19; publ. 21.04.20.
  26. Highly heat-resistant silicone rubber composition: pat. JP2006182902A; filed 27.12.04; publ. 13.07.06.