Anisotropy of low cycle fatigue characteristics of single-crystal heat-resistant nickel alloys
Abstract
The low cycle fatigue of heat-resistant nickel alloys with a single crystal structure VZHM7 and VIN3 was studied. The tests were carried out under conditions of monitoring the complete deformation in the cycle, loading of the type «tension-compression» occurred according to a sinusoidal law with a frequency of 0,5 Hz. For both alloys, tests were carried out for three crystallographic orientations ([001], [011], [111]) at two temperatures: 500 and 850 °C. Regression lines were constructed, the limits of limited endurance were found on the basis of 104 cycles. The influence of test temperature and crystallographic orientation on the endurance limit of alloys and RMS is analyzed.
Keywords
low cycle fatigue (LCF), directional crystallization, crystallographic orientation (CGO), high-temperature nickel alloy, mechanical characteristics, alloys VZhM7 and VIN3, intermetallic alloy, single-crystal alloy.
Reference list
- Ospennikova O.G. Tendencies of development of heat-resistant nickel alloys of low density with polycrystalline and single-crystal structures (review). Aviacionnye materialy i tehnologii, 2016, no. 1 (40), pp. 3–19. DOI: 10.18577/2071-9140-2016-0-1-3-19.
- Inozemtsev A.A., Ratchiev A.M., Nikhamkin M.Sh. et al. Low-cycle fatigue and cyclic crack resistance of a nickel alloy under loading typical for turbine disks. Tyazheloe mashinostroyeniye, 2011, no. 4, pp. 30–33.
- Gorbovets M.A., Bazyleva O.A., Belyaev M.S., Khodinev I.A. Low-cycle fatigue of a single-crystal intermetallic alloy of the VKNA type under conditions of «hard» loading. Metallurg, 2014, no. 8, pp. 111–114.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Reed R.C. The superalloys: Fundamentals and applications. Cambridge University Press, 2006. 372 p.
- Belyaev M.S., Gorbovets M.A., Shvedov V.A. Influence of test conditions on low-cycle fatigue and parameters of cyclic deformation of high-temperature alloy VZh175. Novosti materialovedeniya. Nauka i tekhnika, 2017, no. 5-6 (28). S. 74–82. Available at: http://www.materialsnews.ru ( accessed: July 01, 2020).
- Belyaev M.S., Terentyev V.F., Gorbovets M.A., Bakradze M.M., Antonova O.S. Low-cycle fatigue of heat-resistant nickel alloy VZh175 under conditions of hard loading. Deformatsiya i razrusheniye materialov, 2015, no. 9, pp. 17–24.
- Golubovsky E.R., Svetlov I.L., Petrushin N.V., Cherkasova S.A., Volkov M.E. Low-cycle fatigue of single crystals of heat-resistant nickel alloys at elevated temperatures. Deformatsiya i razrusheniye materialov, 2009, no. 8, pp. 41–48.
- Wright J.K., Carroll L.J., Simpson J.A. et al. Low cycle fatigue of alloy 617 at 850 ° C and 950 ° C. Journal of Engineering Materials and Technology, 2013, vol. 135, no. 7, pp. 031005 (1–8).
- Zhong Z., Gu Y., Yuan Y. et al. On the low cycle fatigue behavior of a Ni-based superalloy containing high Co and Ti contents. Materials Science and Engineering, 2012, vol. A552, pp. 434–443.
- Gao G., Duan S., Zhang W. A study of high temperature low cycle fatigue life prediction for two superalloys. Journal of Engineering Research, 2015, vol. 3, no. 1. P. 114–126.
- Kablov E.N., Ospennikova O.G., Lomberg B.S., Sidorov V.V. Priority directions of development of technologies for the production of heat-resistant materials for aircraft engine building. Problems of ferrous metallurgy and material science, 2013, no. 3, pp. 47–54.
- Dimitrienko Yu.I., Lucenko A.N., Gubareva E.A., Oreshko E.I., Sborshhikov S.V., Bazyleva O.A., Turenko E.Yu. The data storage integrated information system on properties of heat resistant nickel alloys and calculation of their mechanical characteristics. Aviacionnye materialy i tehnologii, 2017, no. 1 (46), pp. 86–94. DOI: 10.18577/2071-9140-2017-0-1-86-94.
- Petrushin N.V., Ospennikova O.G., Svetlov I.L. Single-crystal Ni-based superalloys for turbine blades of advanced gas turbine engines. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 72−103. DOI: 10.18577/2071-9140-2017-0-S-72-103.
- Kablov E.N., Ospennikova O.G., Petrushin N.V. New single crystal heat-resistant intermetallic γʹ-based alloy for GTE blades. Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 34–40. DOI: 10.18577/2071-9140-2015-0-1-34-40.
- Bazyleva O.A., Ospennikova O.G., Arginbaeva E.G., Letnikova E.Yu., Shestakov A.V. Development trends of nickel-based intermetallic alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 104–115. DOI: 10.18577/2071-9140-2017-0-S-104-115.
- Kablov E.N., Ospennikova O.G., Petrushin N.V., Visik E.M. Single-crystal nickel-based superalloy of a new generation with low-density. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 14–25. DOI: 10.18577/2071-9140-2015-0-2-14-25.
- Gorbovets M.A., Khodinev I.A., Ryzhkov P.V. Equipment for testing carrying out the strain-controlled low-cycle fatigue. Trudy VIAM, 2018, no. 9 (69), paper no. 06. Available at: http://www.viam-works.ru (accessed: July 01, 2020). DOI: 10.18577/2307-6046-2018-0-9-51-60.
- Vildeman V.E., Babushkin A.V., Tretyakov M.P. et al Mechanics of materials. Methods and tools for experimental research. Moscow: Publ. house of the Perm National Research Polytechnic University, 2011. 164 p.
- Stepnov M.N. Statistical methods for processing the results of mechanical tests: a reference book. Moscow: Mashinostroenie, 1985. 232 p.