Kuzmina N.A., Petrushin N.V., Visik E.M., Eremin N.N., Naprienko S.A. Application of the Laue method to study the structure of a nickel heat-resistant alloy sample destroyed during mechanical processing // Proceedings of VIAM. 2020. No. 10 (92). Ст. 01. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-10-3-12.

Application of the Laue method to study the structure of a nickel heat-resistant alloy sample destroyed during mechanical processing

Kuzmina N.A., Petrushin N.V., Visik E.M., Eremin N.N., Naprienko S.A.
Abstract

A study of the structure of a single-crystal sample of a nickel heat-resistant alloy, brittle destroyed by mechanical cutting. The study was carried out using x-ray diffractometry – «swing» and the Laue method. The possibilities of the Laue method for studying local defects of various origin are shown. Based on the obtained data, an assumption is made about the recrystallization nature of structural defects in a single crystal of a nickel heat-resistant alloy; the elastic properties of the single crystal are estimated.

Keywords
Laue method, single crystal, crystallographic orientation, subgrain misorientation, x-ray diffraction, structure defects, single crystals of nickel heat-resistant alloys, recrystallization.
Reference list
  1. Cast blades of gas turbine engines: alloys, technologies, coatings / ed. E.N. Kablov. 2nd ed. Moscow: Nauka, 2006. 632 p.
  2. Petrushin N.V., Ospennikova O.G., Svetlov I.L. Single-crystal Ni-based superalloys for turbine blades of advanced gas turbine engines. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 72−103. DOI: 10.18577/2071-9140-2017-0-S-72-103.
  3. Petrushin N.V., Elyutin E.S., Korolev A.V. Monocrystalline heat-resistant alloys: composition, technologies, structure and properties. Materials of Vseros. scientific and technical conf. «Fundamental and applied research in the field of creation of cast heat-resistant nickel and intermetallic alloys and high-performance technologies for the manufacture of GTE parts». Moscow: VIAM, 2017, pp. 271–303.
  4. Toloraya V.N., Kablov E.N., Demonis I.M. Technology of obtaining monocrystalline castings of turbine blades of gas turbine engine of a given crystallographic orientation from rhenium-containing heat-resistant alloys. Liteinye heat-resistant alloys. The effect of S.T. Kishkina / ed. E.N. Kablov. Moscow: Nauka, 2006, pp. 206–218.
  5. Petrushin N.V., Elyutin E.S., Visik E.M., Golynets S.A. Development of a single-crystal high-temperature nickel alloy of the V generation. Metally, 2017, no. 6, pp. 38–51.
  6. Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7-8, pp. 54–58.
  7. Reed R.C. The Superalloys: Fundamentals and Applications. Cambridge University Press, 2006. 372 pp.
  8. Shalin R.E., Svetlov I.L., Kachanov E.B., Toloraya V.N., Gavrilin O.S. Monocrystals of heat-resistant nickel alloys. Moscow: Mashinostroenie, 1997. 336 p.
  9. Toloraya V.N., Kablov E.N., Svetlov I.L., Orekhov N.G., Golubovsky E.R. Anisotropy of strength characteristics of single crystals of heat-resistant nickel alloys. Gorny information-analytical bulletin. 2005. Special issue, pp. 225-236.
  10. Toloraya V.N., Kablov E.N., Orekhov N.G., Ostroukhova G.A. The structure and growth defects of single crystals of heat-resistant nickel alloys. Gornyy informatsionno-analiticheskiy byulleten, 2005. Special issue, pp. 190–202.
  11. Nazarkin R.M., Kolodochkina V.G., Ospennikova O.G., Orlov. M.R. The microstructure modifications of single crystals of Ni-based superalloys in time-tested turbine blades. Aviacionnye materialy i tehnologii, 2016, no. 4 (45), pp. 9–17. DOI: 10.18577/2071-9140-2016-0-4-9-17.
  12. Nazarkin R.M. X-ray diffraction techniques for precise determination of lattice constants in Ni-based superalloys: a brief review. Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 41–48. DOI: 10.18577/2071-9140-2015-0-1-41-48.
  13. Kuzmina N.A., Pyankova L.A. Control of crystallographic orientation of monocrystalline nickel castings heat-resistant alloys by х-ray diffractometry. Trudy VIAM, 2019, no. 12 (84), paper no. 02. Available at: http://www.viam-works.ru (accessed: August 12, 2020). DOI: 10.18577/2307-6046-2019-0-12-11-19.
  14. Khayutin S.G. About misorientation of grains during directional crystallization. Metallovedeniye i termicheskaya obrabotka metallov, 2007, no. 6, pp. 42–43.
  15. Sidokhin E.F., Sidokhin F.A., Khayutin S.G. On the substructure of monocrystalline GTE blades. Aviatsionnaya promyshlennost, 2009, no. 1, pp. 34–36.
  16. Sidokhin F.A., Sidokhin A.F., Sidokhin E.F. On the determination of the crystallographic orientation of single crystals by the Laue method. Zavodskaya laboratoriya. Diagnostika materialov, 2009, vol. 75, no. 1, pp. 35–37.
  17. Potrakhov N.N., Khayutin S.G., Lifshits V.A., Oses R. Installation PRDU-KROS for express determination of crystallographic orientation of cubic single crystals by inverse Laue patterns. Zavodskaya laboratoriya. Diagnostika materialov, 2015, vol. 81, no. 8, pp. 27–30.
  18. Oses R., Lifshits V.A., Potrakhov E.N., Potrakhov N.N. Program for decoding inverse laue patterns of fcc single crystals to determine the crystallographic orientation of samples (CGO analysis): certificate. about the state. reg. Computer programs, no. 201164448. 2011.
  19. Kuzmina N.A., Lifshits V.A., Potrakhov E.N., Potrakhov N.N. Comparative structure control of single-crystal castings of nickel superalloys x-ray diffraction methods of oscillation and Laue. Trudy VIAM, 2019, no. 9 (81), paper no. 02. Available at: http://www.viam-works.ru (accessed: August 12, 2020). DOI: 10.18577/2307-6046-2019-0-9-15-25.
  20. Krivko A.I., Epishin A.I., Svetlov I.L. et al. Elastic properties of single crystals of nickel alloys. Problemy prochnosti, 1988, no. 2, pp. 68–75.
  21. Svetlov I.L., Sukhanov N.N., Samoilov A.I. et al. Temperature-orientation dependences of the characteristics of short-term strength, Young's modulus and the coefficient of linear expansion of single crystals of the ZhC6F alloy. Problemy prochnosti, 1987, no. 1, pp. 51–56.
  22. Cast heat-resistant alloys. The effect of S.T. Kishkina / ed. E.N. Kablov. Moscow: Nauka, 2006. 272 p.
  23. Neiman A.V., Filonova E.V., Iskhodzhanova I.V. On local recrystallization in single crystals of high-temperature nickel alloys. Metallurgiya i mashinostroyeniye, 2013, no. 1, pp. 19–22.