Guseva M.A., Aslanyan I.R., Ponomarenko S.A. Study of the rheology of model compositions depending on the nature and ratio of the main components // Proceedings of VIAM. 2020. No. 1 (85). Ст. 12. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2020-0-1-126-134.

Study of the rheology of model compositions depending on the nature and ratio of the main components

Guseva M.A., Aslanyan I.R., Ponomarenko S.A.
Abstract

In this work, the technological characteristics of model compositions for injection molding are evaluated by studying their rheological behavior when changing the content of the main components of the model composition. The influence of the ratios in «paraffin/petroleum resin» and «sevilen/polyethylene wax vapor», and also on the properties of polyvinyl alcohol used as solid filler on the rheology of model compositions of experimental compounds is considered. Based on the results, it was suggested that the ratio of petroleum resin and paraffin should be 2/1, the ratio of polyethylene wax and sevilen 1/1 respectively.

Keywords
rheological tests, model composition, filler, investment casting, viscosity.
Reference list
  1. Kablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7-8, pp. 54–58.
  2. Kablov E.N. Materials of a new generation – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), S. 16–21.
  3. Petrova A.P., Malysheva G.V. Glues, adhesive binders and adhesive prepregs.Scientific. Ed. E.N. Kablova. M.: VIAM, 2017. 472 p.
  4. Kablov E.N., Chursova L.V., Lukina N.F., Kutsevich K.E., Rubtsova E.V., Petrova A.P. The study of epoxy-polysulfone polymer systems as the basis of high-strength adhesives for aviation purposes. Klei. Germetiki. Tekhnologii, 2017, no. 3, pp. 7 – 12.
  5. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, No. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  6. Tkachuk A.I., Terekhov I.V., Gurevich Ya.M., Grigoreva K.N. Research of the influence of the modifying additives nature on the rheological and thermomechanical properties of a photopolymer composition based on epoxy vinyl ester resin. Aviacionnye materialy i tehnologii, 2019, No. 3 (56), pp. 31–40. DOI: 10.18577 / 2071-9140-2019-0-3-31-40.
  7. Guseva M.A. The use of the rheological tests in the development of polymeric materials for various purposes. Trudy VIAM, 2018, no. 11 (71), paper no. 05. Available at: http://www.viam-works.ru (accessed: November 20, 2019). DOI: 10.18577/2307-6046-2018-0-11-35-44.
  8. Antyufeeva N.V., Afanasyeva E.A., Guseva M.A., Haskov M.A. Investigation of the process of combining epoxy oligomers with polyarylate. Mekhanika kompozitsionnykh materialov i konstruktsiy, 2019, vol. 25, no. 1, pp. 19–28.
  9. Babin A.N., Guseva M.A., Haskov M.A., Tkachuk A.I. Study of the process of combining epoxy oligomers with thermoplastic modifiers. Mekhanika kompozitsionnykh materialov i konstruktsiy, 2016, vol. 22. no. 4, pp. 524–535.
  10. Guseva M.A., Aslanyan I.R. The effect of fillers on the rheology of model composition. Trudy VIAM, 2019. no. 5, paper no. 09. Available at: http://www.viam-works.ru (accessed: October 17, 2019). DOI: 10.18577/2307-6046-2019-0-5-94-102.
  11. Aslanyan I.R., Guseva M.A., Ospennikova O.G. A comparative study of the physicomechanical and rheological characteristics of model compositions. Vse materialy. Entsiklopedicheskiy spravochnik, 2019, no. 6, pp. 34–39.
  12. Loshchinin Yu.V., Shorstov S.Yu., Kuzmina I.G. Research of influence of technology factors on thermal conductivity of ceramic casting molds. Aviacionnye materialy i tehnologii, 2019, No. 2 (55), pp. 89–94. DOI: 10.18577/2071-9140-2019-0-2-89-94.
  13. Aslanyan I.R., Rassokhina L.I., Ospennikova O.G. Definition of quantitative factors, significantly influencing on technological characteristics of model compositions). Trudy VIAM, 2018, no. 12 (72), paper no. 01. Available at: http://www.viam-works.ru (accessed: November 10, 2019). DOI: 10.18577/2307-6046-2018-0-12-3-13.
  14. Ospennikova O.G. Influence research of fillers on properties and stability of modelling compositions, a choice of optimum structures. Aviacionnye materialy i tehnologii, 2014, no. 3, pp. 14–17. DOI: 10.18577/2071-9140-2014-0-3-14-17.
  15. Ospennikova O.G., Aslanyan I.R. Directions of development of manufacturing technology for model compositions for blades and other parts of gas turbine engines. Liteynoe proizvodstvo, 2018, no. 3, pp. 20–24.
  16. Vdovin R.A., Smelov V.G. The study of shrinkage of wax models obtained by rapid prototyping technology. Samara: Izd-vo Samarsk. Un-ta, 2017. 43 p.
  17. Rassokhina L.I., Parfenovich P.I., Narsky A.R. Problems of creating model compositions of a new generation on the basis of domestic materials for the manufacture of GTE blades. Novosti materialovedeniya. Nauka i tekhnika, 2015, no. 3 (15), paper no. 07. Available at: http: //www.materialsnews.ru (accessed: November 20, 2019).
  18. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.