Duyunova V.A., Kozlov I.A., Oglodkov M.S., Kozlova A.A. Modern trends in the anodic oxidation of aluminum-lithium and aluminum alloys (review) // Proceedings of VIAM. 2019. No. 8 (80). Ст. 09. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2019-0-8-79-89.

Modern trends in the anodic oxidation of aluminum-lithium and aluminum alloys (review)

Duyunova V.A., Kozlov I.A., Oglodkov M.S., Kozlova A.A.
Abstract

The work is devoted to the analysis of modern scientific works in the field of application of non-metallic inorganic coatings by anodic oxidation on aluminum and aluminum-lithium alloys. The modern trends of anodic oxidation technology are considered, and the results of scientific research are compared with traditional technologies. The main attention in the analysis of scientific research is focused on the mechanism of influence of alloying elements of aluminum alloys coming to the surface, technological solutions to eliminate the use of toxic compounds in anodic oxidation and subsequent filling.

Keywords
aluminum, aluminum-lithium alloys, anodic oxidation, protective coatings, corrosion.
Reference list
  1. Kablov E.N., Antipov V.V., Klochkova Yu.Yu. Alyuminiy-litiyevyye splavy novogo pokoleniya i sloistyye alyumostekloplastiki na ikh osnove [New-generation aluminum-lithium alloys and layered aluminum-glass-reinforced plastics based on them] // Tsvetnye metally. 2016. №8. S. 86–91.
  2. Kablov E.N., Lukina E.A., Sbitneva S.V., Khokhlatova L.B., Zaytsev D.V. Formirovaniye metastabilnykh faz pri raspade tverdogo rastvora v protsesse iskusstvennogo stareniya Al-splavov [The formation of metastable phases during the decomposition of a solid solution in the process of artificial aging of Al-alloys] // Tekhnologiya legkikh splavov. 2016. №3. S. 7–17.
  3. Fridlyander I.N., Drits A.M., Vovnyanko A.G. Novyye alyuminiyevyye splavy dlya otvetstvennykh silovykh konstruktsiy samoletov [New aluminum alloys for critical power structures of aircraft] // Aviatsionnaya promyshlennost. 1985. №6. S. 56–58.
  4. Shalin R.E., Fridlyander I.N., Leshchiner L.N., Butusova I.V., Kuznetsova N.B. Alyuminiyevyye splavy dlya passazhirskikh samoletov [Aluminum alloys for passenger aircraft] // Aviatsionnaya promyshlennost. 1988. №6. S. 88–89.
  5. Fridlyander I.N., Leshchiner L.N., Sandler V.S., Latushkina L.V., Vorobev O.I., Nikolskaya T.I. Struktura i svoystva splavov sistemy Al–Cu–Mg–Li [Structure and properties of alloys of the Al–Cu–Mg–Li system] // Aviatsionnaya promyshlennost. 1986. №8. S. 59–61.
  6. Fridlyander I.N., Grushko O.Ye., Antipov V.V., Kolobnev N.I., Khokhlatova L.B. Alyuminiylitiyevye splavy [Aluminum-lithium alloys] // Vse materialy. Entsiklopedicheskiy spravochnik. 2008. №8. S. 22–27.
  7. Antipov V.V., Serebrennikova N.Yu., Nefedova Yu.N., Kozlova O.Yu., Panteleev M.D., Osipov N.N., Klychеv A.V. Tekhnologicheskie osobennosti Izgotovleniya detalej iz alyuminiy-litievogo splava 1441 [Manufacturing capability of Al–Li 1441 alloy details] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2018. №10 (70). St. 03 Available at: http://www.viam-works.ru (accessed: June 17, 2019). DOI: 10.18577/2307-6046-2018-0-10-17-26.
  8. Antipov V.V. Perspektivy razvitiya alyuminievyh, magnievyh i titanovyh splavov dlya izdelij aviacionno-kosmicheskoj tehniki [Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering] // Aviacionnye materialy i tehnologii. 2017. №S. S. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
  9. Antipov V.V., Klochkova Yu.Yu., Romanenko V.A. Sovremennye alyuminievye i alyuminij-litievye splavy [Modern aluminum and aluminum-lithium alloys] // Aviacionnye materialy i tehnologii. 2017. №S. S. 195–211.
  10. Kablov E.N., Antipov V.V., Senatorova O.G. Sloistyye alyumostekloplastiki SIAL-1441 i sotrudnichestvo s Airbus i TU Delft [SIAL-1441 laminated aluminoglassplactics and cooperation with Airbus and TU Delft] // Tsvetnyye metally. 2013. №9. S. 50–53.
  11. Kutyrev A.E., Chesnokov D.V., Antipov V.V., Vdovin A.I. Razrabotka rastvora dlya naneseniya korrozionnykh porazheniy na alyuminiyevykh splavakh v galvanostaticheskom rezhime [The development of a solution for promotion of corrosion attack on aluminium alloys in a galvanostatic mode] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2018. №9 (69). St. 11. Available at: http://www.viam-works.ru (accessed: June 17, 2019). DOI: 10.18577/2307-6046-2018-0-9-105-118.
  12. Kozlov I.A., Vinogradov S.S., Tarasova K.G., Kulyushina N.V., Manchenko V.A. Plazmennoye elektroliticheskoye oksidirovaniye magniyevykh splavov (obzor) [Plasma electrolytic oxidation of magnesium alloys (review)] // Aviatsionnyye materialy i tekhnologii. 2019. №1 (54). S. 23–36. DOI: 10.18577/2071-9140-2019-0-1-23-36.
  13. Pavlovskaya T.G., Volkov I.A., Kozlov I.A., Naprienko S.A. Ekologicheski uluchshennaya tehnologiya obrabotki poverhnosti alyuminievyh splavov [Ecologically improved technology of aluminum alloys surface treatment] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №7. St. 02 (accessed: June 17, 2019). DOI: 10.18577/2307-6046-2016-0-7-2-2.
  14. Antipov V.V., Petrova A.P., Kozlov I.A., Fomina M.A., Volkov I.A. Vliyaniye tekhnologicheskikh nagrevov i sposobov podgotovki poverkhnosti pod skleivaniye na mekhanicheskiye svoystva alyuminiyevoy folgi iz splava AMg2N [Influence of technological heatings and ways of surface preparation under pasting on mechanical properties of aluminum foil from alloy AMg2N] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2018. №7 (67). St. 02. Available at: http://www.viam-works.ru (accessed: June 17.06.2019). DOI: 10.18577/2307-6046-2018-0-7-10-24.
  15. Sposob polucheniya pokrytiya na alyuminiyevykh splavakh: pat. 2547983 Ros. Federatsiya [A method of obtaining a coating on aluminum alloys: pat. 2547983 Rus. Federation]; zayavl. 14.04.14; opubl. 10.04.15.
  16. Antipov V.V., Chesnokov D.V., Kozlov I.A., Volkov I.A., Petrova A.P. Podgotovka poverkhnosti alyuminiyevogo splava V1469 pered primeneniyem v sostave sloistogo gibridnogo materiala [Surface preparation aluminum alloy V-1469 before use in the composition of layered hybrid material] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2018. №4 (64). St. 07. Available at: http://www.viam-works.ru (accessed: Juny 16, 2019). DOI: 10.18577/2307-6046-2018-0-4-59-65.
  17. Rastvor dlya uplotneniya anodno-okisnogo pokrytiya alyuminiyevykh splavov: pat. 2447201 Ros. Federatsiya [The solution for sealing the anodic oxide coating of aluminum alloys: pat. 2447201 Rus. Federation]; zayavl. 05.04.11; opubl. 10.04.12.
  18. Harscoet E., Froelich D. Use of LCA to evaluate the environmental benefits of substituting chromic acid anodizing (CAA) // Journal of Cleaner Production. 2007. No. 16. P. 1294–1305.
  19. Kozlov I.A., Pavlovskaya T.G., Zakharov K.E., Volkov I.A. Ekologicheski uluchshennyye tekhnologii podgotovki poverkhnosti alyuminiyevykh splavov [ Ecologically improved technologies for preparing the surface of aluminum alloys ] // Adgezionnyye materialy: sb. dokl. nauch.-tekhnich. konf. M.: VIAM, 2016. S. 13.
  20. Chakravarthy V., Canulescu S., Shabadi R. et al. Structure of anodized Al–Zr sputter deposited coatings and effect on optical appearance // Applied Surface Science. 2014. No. 317. P. 1113–1124.
  21. Zahavi J., Zangvil A., Metzger M. Structure and stability of anodic films formed on aluminum containing dispersed Al3Fe phase // Journal of The Electrochemical Society. 1978. No. 125. P. 438–444.
  22. Mukhopadhyay A.K., Sharma A.K. Influence of Fe-bearing particles and nature of electrolyte on the hard anodizing behaviour of AA7075 extrusion products // Surface and Coatings Technology. 1997. No. 92 (3). P. 212–220.
  23. Mukhopadhyay A.K. On the nature of the Fe-bearing particles influencing hard anodizing behavior of AA7075 extrusion products // Metallurgical and Materials Transactions. 1998. No. 29 (3). P. 979–987.
  24. Fratila-Apachitei L.E., Terryn H., Skeldon P. et al. Influence of substrate microstructure on the growth of anodic oxide layers // Electrochimica Acta. 2004. No. 49 (7). P. 1127–1140.
  25. Iglesias-Rubianes L., Garcia-Vergara S.J., Skeldon P. et al. Cyclic oxidation processes during anodizing of Al–Cu alloys // Electrochimica Acta. 2007. No. 52 (24). P. 7148–7157.
  26. Kikuchia T., Kunimotoa K., Ikedaa H. Fabrication of anodic porous alumina via galvanostatic anodizing in alkaline sodium tetraborate solution and their morphology // Journal of Electroanalytical Chemistry. 2019. Vol. 846. P. 113–152.
  27. Wu H., Ma Y., Huang W. et al. Effect of Iron-Containing Intermetallic Particles on Film Structure and Corrosion Resistance of Anodized AA2099 Alloy // Journal of the Electrochemical Society. 2018. Vol. 165 (9). Р. 573–581.
  28. Liu J., Rong G., Cen S. et al. Dissolution Behavior of Intermetallic Particles in AA2297-T87 during Anodizing in Adipic-Sulfuric Acid // Journal of the Electrochemical Society. 2018. No. 165 (16). P. C980–C990.
  29. Ma Y., Zhou X., Thompson G.E. et al. Anodic film growth on Al–Li–Cu alloy AA2099-T8 // Electrochimica Acta. 2012. No. 80. Р. 148–159.
  30. Skeldon P., Thompson G.E., Wood G.C. et al. Effects of alloying elements in anodizing of aluminium // Philosophical Magazine. 1997. No. 76. Р. 729–738.
  31. Bailey P., Skeldon P., Noakes T.C.Q. et al. Composition and structure of enriched alloy layers in filmed Al alloys studied by medium-energy ion scattering // Surface and Interface Analysis. 2001. No. 31. Р. 480–488.
  32. Shimizu K., Brown G.M., Kobayashi K. et al. Anodising as pre-treatment before organic coating of extruded and cast aluminium alloys // Corrosion Science. 1998. No. 40 (7). Р. 1049–1055.
  33. Ma Y., Zhou X., Thompson G.E. et al. Discontinuities in the porous anodic film formed on AA2099-T8 aluminium alloy // Corrosion Science. 2011. No. 53. Р. 4141–4151.
  34. Ma Y., Zhou X., Thompson G.E. et al. Microstructural Modification Arising from Alkaline Etching and Its Effect on Anodizing Behavior of Al–Li–Cu Alloy // Journal of the Electrochemical Society. 2013. No. 160. P. 111–118.
  35. Gharbia O., Birbilisb N., Oglea K. Li reactivity during the surface pretreatment of Al–Li alloy AA2050-T3 // Electrochimica Acta. 2017. No. 243. P. 207–219.
  36. Gharbi O., Birbilis N., Ogle K. In-Situ Monitoring of Alloy Dissolution and Residual Film Formation during the Pretreatment of Al-Alloy AA2024-T3 // Journal of The Electrochemical Society. 2016. No. 163 (5). P. 240–251.
  37. Nelson K.J.H., Hughes A.E., Taylor R.J. et al. Characterisation of aluminium alloys after HNO3/HF–NaOH–HNO3/HF pretreatment // Materials Science and Technology. 2001. No. 17 (10). P. 1211–1221.
  38. Hughes A.E., Theodossiou G., Elliott S. et al. Study of deoxidation of 2024-T3 with various acids // Materials Science and Technology. 2001. No. 17 (12). P. 1642–1652.
  39. García-Rubio M., Ocón P., Climent-Font A. Influence of molybdate species on the tartaric acid/sulphuric acid anodic films grown on AA2024-T3 aerospace alloy // Corrosion Science. 2009. No. 51. P. 2034–2042.
  40. Marzocchi V., Iglesias-Rubianes L., Thompson G.E., Bellucci F. The influence of tartaric acid additions on the anodizing behaviour of AA2024-T3 alloy in sulphuric acid // Corrosion Science. 2009. No. 25. P. 461–473.
  41. Curioni M., Skeldon P., Koroleva E. et al. Role of tartaric acid on the anodizing and corrosion behavior of a 2024-T3 aluminum alloy // Journal of the Electrochemical. 2009. No. 156. P. 147–153.
  42. Arenas M.A., Conde A., de Damborenea J.J. Effect of acid traces on hydrothermal sealing of anodising layers on 2024 aluminium alloy // Electrochimica Acta. 2010. No. 55. P. 8704–8708.
  43. Bononi M., Conte M., Giovanardi R., Bozza A. Hard anodizing of AA2099-T8 aluminum lithium copper alloy: Influence of electric cycle, electrolytic bath composition and temperature // Surface & Coatings Technology. 2017. Vol. 325. Р. 627–635.
  44. Sposito G. The Environmental Chemistry of Aluminum/ CRC Press, 1995. 480 р.
  45. Bozza A., Giovanardi R., Manfredini T., Mattioli P. Pulsed current effect on hard anodizing process of 7075-T6 aluminium alloy // Surface and Coatings Technology. 2015. No. 270. P. 139–144.
  46. Ma Y., Zhou X., Liao Y. et al. Effect of anodizing parameters on film morphology and corrosion resistance of AA2099 // Journal of the Electrochemical Society. 2016. No. 163 (7). P. 369–376.
  47. Pearlstein F., Agarwala V.S. Trivalent Chromium Solutions for Applying Chemical Conversion Coatings to Aluminum Alloys or for Sealing Anodized Aluminum // Surface and Coatings Technology. 1994. No. 81 (7). P. 50–55.
  48. Gordovskaya I.V., Hashimoto T., Walton J. Development of Cerium-Rich Layers on Anodic Films Formed on Pure Aluminium and AA7075-T6 Alloy // Journal of The Electrochemical Society. 2014. No. 161 (14). P. 601–606.
  49. Kuznetsov B., Serdechnova M., Tedim J. Sealing of tartaric sulfuric (TSA) anodized AA2024 with nanostructured LDH layers // RSC Advanced. 2016. No. 6. P. 13942–13952.
  50. Capelossi V.R., Poelman M., Recloux I. et al. Corrosion protection of clad 2024 aluminum alloy anodized in tartaric-sulfuric acid bath and protected with hybrid sol–gel coating // Electrochimica Acta. 2014. No. 124. P. 69–79.
  51. Balaraju J.N., Srinivasan A., Yoganandan G. Effect of Mn/Mo incorporated oxide layer on the corrosion behavior of AA2024 alloy // Corrosion Science. 2011. No. 53. P. 4084–4092.
  52. Yoganandan G., Balaraju J.N., Christopher H.C. et al. Electrochemical and long term corrosion behavior of Mn and Mo oxyanions sealed anodic oxide surface developed on aerospace aluminum alloy (AA2024) // Surface & Coatings Technology. 2016. No. 288. P. 115–125.