Shpagin A.S., Kucheryaev V.V., Bubnov M.V. Computer simulation of thermomechanical processing of heat-resistant nickel alloys VZh175 and EP742 // Proceedings of VIAM. 2019. No. 8 (80). Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2019-0-8-27-35.

Computer simulation of thermomechanical processing of heat-resistant nickel alloys VZh175 and EP742

Shpagin A.S., Kucheryaev V.V., Bubnov M.V.
Abstract

This article represents the results of the database development of the rheological properties related to the heat-resistant Nickel alloys VZh175 and EP742. It also shows the sequence of actions for creating of rheological model of material and checking its operability. The using of the mentioned database in the program QForm will provide the possibility of computer simulation of various processes of pressure treatment of alloys VZh175 and EP742 for the development of new technologies for obtaining deformed semi-finished products from these alloys.

Keywords
heat-resistant nickel alloys, computer simulation, metal forming, database, rheological properties, flow stress, stamping, deformation.
Reference list
  1. Kablov E.N. Na perekrestke nauki, obrazovaniya i promyshlennosti [At the crossroads of science, education and industry] // Ekspert. 2015. №15 (941). S. 49–53.
  2. Kablov E.N. Klyuchevaya problema – materialy [The key problem is materials] // Tendentsii i oriyentiry innovatsionnogo razvitiya Rossii. M.: VIAM, 2015. S. 458–464.
  3. Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Russia needs new generation materials] // Redkiye zemli. 2014. №3. S. 8–13.
  4. Ospennikova O.G., Bubnov M.V., Kapitanenko D.V. Kompyuternoe modelirovanie processov obrabotki metallov davleniem [Computer modeling of metal working processes by pressure] // Aviacionnye materialy i tehnologii. 2012. №S. S. 141–147.
  5. Razuvaev E.I., Moiseev N.V., Kapitanenko D.V., Bubnov M.V. Sovremennye tehnologii obrabotki metallov davleniem [Modern technologies of plastic working of metals] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №2. St. 03. Available at: http://www.viam-works.ru (accessed: June 26, 2019). DOI: 10.18577/2307-6046-2015-0-2-3-3.
  6. Gun G.Ya. Teoreticheskiye osnovy obrabotki metallov davleniyem [Theoretical foundations of metal forming]. M.: Metallurgiya, 1980. 456 s.
  7. Biba N.V., Lishniy A.I., Stebunov S.A. Effektivnost primeneniya modelirovaniya dlya razrabotki tekhnologii shtampovki [The effectiveness of modeling for the development of stamping technology] // Kuznechno-shtampovochnoye proizvodstvo. 2001. №5. S. 39–44.
  8. Bakradze M.M., Skugorev A.V., Kucheryayev V.V., Bubnov M.V. Kompyuternoye modelirovaniye tekhnologicheskikh protsessov obrabotki metallov davleniyem kak instrument razrabotki novykh tekhnologiy [Computer modeling of technological metal forming processes as effective instrument for development of new technologies] // Aviacionnye materialy i tehnologii. 2017. №S. S. 175–185. DOI: 10.18577/2071-9140-2017-0-S-175-185.
  9. Stebunov S.A., Biba N.V. QForm – programma, sozdannaya dlya tekhnologov [QForm – a program created for technologists] // Kuznechno-shtampovochnoye proizvodstvo. 2004. №9. S. 38–43.
  10. Polukhin P.I., Gun G.Ya., Galkin A.M. Soprotivleniye plasticheskoy deformatsii metallov i splavov [Resistance to plastic deformation of metals and alloys]. M.: Metallurgiya, 1983. 488 s.
  11. Gladkov Yu.A., Mordvintsev P.S. Modelirovaniye tekhnologicheskikh protsessov shtampovki pri reshenii zadach avia- i dvigatelestroyeniya [Certification of aviation forgings based on process modeling in the QForm program] // Kuznechno-shtampovochnoye proizvodstvo. Obrabotka materialov davleniyem. 2012. №5. S. 38–47.
  12. Stebunov S.A., Bocharov Yu.A. Sertifikatsiya aviatsionnykh pokovok na osnove modelirovaniya protsessov v programme QForm [Certification of aviation forgings based on process modeling in the QForm program] // Kuznechno-shtampovochnoye proizvodstvo. Obrabotka materialov davleniyem. 2011. №6. S. 33–35.
  13. Lomberg B.S., Ovsepjan S.V., Bakradze M.M., Letnikov M.N., Mazalov I.S. Primenenie novyh deformiruemyh nikelevyh splavov dlja perspektivnyh gazoturbinnyh dvigatelej [The application of new wrought nickel alloys for advanced gas turbine engines] // Aviacionnye materialy i tehnologii. 2017. №S. S. 116–129. DOI: 10.18577/2071-9140-2017-0-S-116-129.
  14. Volkov A.M., Vostrikov A.V., Bakradze M.M. Printsipy sozdaniya i osobennosti legirovaniya granuliruyemykh zharoprochnykh nikelevykh splavov dlya diskov GTD [Development principles and alloying features of p/m NI base superalloys for jet-engine disks application] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №8 (44). St. 02. Available at: http://www.viam-works.ru (accessed: June 24, 2019). DOI: 10.18577/2307-6046-2016-0-8-2-2.
  15. Khenzel A., Shpittel T. Raschet energosilovykh parametrov v protsessakh obrabotki metallov davleniyem: sprav. izd. Per. s nem. [Calculation of power parameters in metal forming processes: reference edition. Line from Germ.]. M.: Metallurgiya, 1982. 360 s.
  16. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  17. Ponomarenko D.A., Moiseev N.V., Skugorev A.V. Shtampovka diskov GTD iz zharoprochnykh splavov na izotermicheskikh pressakh [Punching of disks GTE from hot strength alloys on isothermal presses] // Aviacionnye materialy i tekhnologii. 2013. №1. S. 13–16.
  18. Ponomarenko D.A., Moiseyev N.V., Skugorev A.V. Effektivnaya tekhnologiya izgotovleniya diskov GTD iz zharoprochnykh nikelevykh splavov [An effective technology for the manufacture of gas-turbine engine disks from heat-resistant nickel alloys] // Kuznechno-shtampovochnoye proizvodstvo. Obrabotka materialov davleniyem. 2013. №10. S. 13–17.