Sarychev I.A. S, Serkova E.A., Khmelnitskiy V.V., Zastrogina O.B. Thermosetting binders for aircraft floor panel materials (review) // Proceedings of VIAM. 2019. No. 7 (79). Ст. 03. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2019-0-7-26-33.

Thermosetting binders for aircraft floor panel materials (review)

Sarychev I.A. S, Serkova E.A., Khmelnitskiy V.V., Zastrogina O.B.
Abstract

A review of thermosetting binders used for the production of three-layer honeycomb floor panels in domestic and foreign practice has been carried out; the main types have been identified. Mechanical properties and fire resistance of floor panels on phenol-formaldehyde and epoxy binders are given. Describes some of the binder compositions and the ways of their physical and chemical modification necessary to meet the requirements for strength and fire safety. Designated features of the production of honeycomb panels, depending on the type of binder. The conclusion was made about the direction of research in the development of new binders for aircraft floor panels.

Keywords
thermosetting binders, composite materials, three-layer honeycomb panel, phenol-formaldehyde resins, epoxy resins, fire retardant, combustibility, fire safety.
Reference list
  1. Kablov E.N. Iz chego sdelat budushcheye? Materialy novogo pokoleniya, tekhnologii ikh sozdaniya i pererabotki – osnova innovatsiy [What to make the future from? Materials of the new generation, technologies of their creation and processing - the basis of innovation] // Krylya Rodiny. 2016. №5. S. 8–18.
  2. Raskutin A.E. Rossiiskie polimernye kompozitsionnye materialy novogo pokoleniia, ikh osvoenie i vnedrenie v perspektivnykh razrabatyvaemykh konstruktsiiakh [Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions] // Aviacionnye materialy i tehnologii. 2017. №S. S. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
  3. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  4. Kablov E.N., Startsev V.O. Sistemnyj analiz vliyaniya klimata na mekhanicheskie svojstva polimernykh kompozitsionnykh materialov po dannym otechestvennykh i zarubezhnykh istochnikov (obzor) [Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review)] // Aviacionnye materialy i tehnologii. 2018. №2 (51). S. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  5. Lukina N.F., Petrova A.P., Muhametov R.R., Kogtjonkov A.S. Novye razrabotki v oblasti kleyashhih materialov aviacionnogo naznacheniya [New developments in the field of adhesive aviation materials] // Aviacionnye materialy i tehnologii. 2017. №S. S. 452–459. DOI: 10.18577/2071-9140-2017-0-S-452-459.
  6. Malysheva G.V., Grashchenkov D.V., Guzeva T.A. Otsenka tekhnologichnosti ispolzovaniya kleyev i kleyevykh prepregov pri izgotovlenii trekhsloynykh paneley [Evaluation of technological use efficiency of adhesives and glue prepregs in the manufacture of three-layer panels] // Aviacionnye materialy i tehnologii. 2018. №4 (53). S. 26–30. DOI: 10.18577/2071-9140-2018-0-4-26-30.
  7. Barbotko S.L. Razvitie metodov ocenki pozharobezopasnosti materialov aviacionnogo naznacheniya [Development of the fire safety test methods for aviation materials] // Aviacionnye materialy i tehnologii. 2017. №S. S. 516–526. DOI: 10.18577/2071-9140-2017-0-S-516-526.
  8. Veshkin E.A., Postnov V.I., Zastrogina O.B., Satdinov R.A. Tekhnologiya uskorennogo formovaniya trekhsloynykh sotovykh paneley interera samoleta [Accelerated molding technology of three-layer honeycomb interior panels of an aircraft] // Izvestiya Samarskogo nauchnogo tsentra Rossiyskoy akademii nauk. 2013. T. 15. №4. S. 799–805.
  9. Kondrashov E.K., Postnov V.I., Petukhov V.I., Kavun N.S., Abramov P.A., Yudin A.A., Barbotko S.L. Issledovaniye svoystv trekhsloynykh paneley na modifitsirovannom svyazuyushchem FPR-520G [Research of properties technological panels on the modified binding FPR-520G] // Aviatsionnye materialy i tehnologii. 2009. №3. S. 19–23.
  10. Zastrogina O.B., Shvets N.I., Serkova E.A., Veshkin E.A. Pozharobezopasnyye materialy na osnove fenolformaldegidnykh svyazuyushchikh [Fireproof materials based on phenol-formaldehyde binders] // Klei. Germetiki. Tekhnologii. 2017. №7. S. 22–27.
  11. Serkova E.A., Shvets N.I., Zastrogina O.B., Postnov V.I., Barbotko S.L., Veshkin E.A. Bystrootverzhdayemoye fenolformaldegidnoye svyazuyushcheye, pererabatyvayemoye po «crush core» tekhnologii, dlya pozharobezopasnykh materialov interera [Fast-curing phenol-formaldehyde binder, processed by «crush core» technology, for fireproof interior materials] // Tezisy dokladov XIX konferentsii «Konstruktsii i tekhnologii polucheniya izdeliy iz nemetallicheskikh materialov». Obninsk. 2010. S. 70–71.
  12. Barannikov A.A., Veshkin E.A., Postnov V.I., Strelnikov S.V. K voprosu proizvodstva paneley pola iz PKM dlya letatelnykh apparatov (obzornaya statya) [On the production of floor panels from PCM for aircraft (review article)] // Izvestiya Samarskogo nauchnogo tsentra Rossiyskoy akademii nauk. 2017. T. 19. №4 (2). S. 198–212.
  13. Dushin M.I., Ermolayev A.M., Katyrev I.YA., Neydonov P.N. Ugleplastiki v panelyakh pola trekhsloynoy konstruktsii [Carbon plastics in floor panels of a three-layer construction] // Aviatsionnaya promyshlennost. 1978. №6. S. 8–12.
  14. Dveyrin A.Z., Mayorova E.V. Analiz effektivnosti vnedreniya integralnykh konstruktsiy s trubchatymi elementami iz polimernykh kompozitsionnykh materialov [Analysis of the effectiveness of the introduction of integrated structures with tubular elements made of polymer composite materials] // Voprosy proyektirovaniya i proizvodstva konstruktsiy letatelnykh apparatov. 2011. №4. S. 65–77.
  15. Dementyeva L.A., Tyumeneva T.Yu., Sharova I.A. Klei s ponizhennoy goryuchestyu dlya aviatsionnoy tekhniki [Adhesives with low flammability for aviation technology] // Nauchnyye publikatsii sotrudnikov VIAM. Available at: https://viam.ru/public/files/2011/2011-205777.pdf (accessed: April 29, 2019).
  16. Sostav i sposob izgotovleniya svyazuyushchego, preprega i sotovoy paneli: pat. 2460745. Ros. Federatsiya [The composition and method of manufacturing a binder, prepreg and honeycomb: pat. 2460745. Rus. Federation]; zayavl. 29.12.10; opubl. 10.09.12.
  17. Termoplavkoye svyazuyushcheye, sposob polucheniya yego, prepreg i sotovaya panel, vypolnennyye na yego osnove: pat. 2486217. Ros. Federatsiya [A hot-melt binder, a method for its preparation, a prepreg and a honeycomb panel based on it: pat. 2486217. Rus. Federation]; zayavl. 21.12.11; opubl. 27.06.13.
  18. Shokin G.I., Shershak P.V., Andryunina M.A. Opyt razrabotki i osvoyeniya proizvodstva sotovykh paneley pola iz otechestvennykh materialov [Experience in the development and development of the production of honeycomb floor panels from domestic materials] // Aviatsionnaya promyshlennost. 2017. №1. S. 32–40.
  19. Prepreg na osnove kleyevogo svyazuyushchego ponizhennoy goryuchesti i stekloplastik, ugleplastik na yego osnove: pat. 2676634. Ros. Federatsiya [The prepreg based on adhesive bonding low flammability and fiberglass, carbon fiber based on it: pat. 2676634. Rus. Federation]; zayavl. 19.04.18; opubl. 09.01.19.
  20. Resins curable into fire-retardant and heat-resistant plastic materials, and method for their preparation: pat. EP 0356379A1; publ. 28.02.90.
  21. Aerospace Qualified Prepreg Materials // Gurit. Available at: https://www.gurit.com/Our-Business/Composite-Materials/Prepregs/Aerospace (accessed: April 29, 2019).
  22. Advanced materials for aircraft interiors // Compositesworld. Available at: https://www.compositesworld.com/articles/advanced-materials-for-aircraft-interiors (accessed: April: 26, 2019).
  23. Rimdusit S., Jubsilp C., Tiptipakorn S. Alloys and Composites of Polybenzoxazines: Properties and Applications. Springer Science & Business Media, 2013. 164 p.
  24. Aircraft floor and interior panels using edge coated honeycomb: pat. US 7988809B2; publ. 02.08.11.
  25. CYCOM 6826 | Cytec, CYCOM 6826, Phenolic Resin | Aircraft products | Cytec | 48862 JACO Aerospace Products. Available at: https://www.e-aircraftsupply.com/products/ Cytec/48862/CYCOM-6826 (accessed: April 26, 2019).
  26. Epoxy foil resins // 5M S.R.O. Company. Available at: https://www.5m.cz/en/products/epoxidove-pryskyrice/epoxy-foil-resins (accessed: May 05, 2019).
  27. Krípal L. Mechanical testing of composite specimens made by RFI technology // Aviation. 2007. Vol. 11. P. 6–14.
  28. Floor panels // The Gill Corporation. Available at: https://www.thegillcorp.com/home.php?cPath=38_23 (accessed: May 05, 2019).