Doriomedov M.S., Sevastyanov D.V., Shein E.A. Technological, institutional and economic trends in the industry of rare and rare-earth metals (review) // Proceedings of VIAM. 2019. No. 7 (79). Ст. 01. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2019-0-7-3-11.

Technological, institutional and economic trends in the industry of rare and rare-earth metals (review)

Doriomedov M.S., Sevastyanov D.V., Shein E.A.
Abstract

Technological, institutional and economic trends in the field of rare and rare-earth metals are presented. It was stated that the development of the above-mentioned trends was governed by China’s global leadership in rare-earth industry and general global trends concerning steady supply of rare and rare-earth metals as well as rational utilization of mineral raw materials. Elucidation of trends is of profound importance for development and intensification of domestic industry of rare and rare-earth metals.

Keywords
rare metals, rare-earth metals, technological trends, institutional trends, economic trends, development.
Reference list
  1. Sevastyanov D.V., Doriomedov M.S., Sutubalov I.V., Kulagina G.S. Napravleniya razvitiya proizvodstvennykh tekhnologij v oblasti redkozemelnykh metallov [Directions for the development of manufacturing technolo-gies in the field of rare earth metals] // Trudy VIАM: ehlektron. nauch.-tekhnich. zhurn. 2018. №1. St. 4. Available at: http://www.viam-works.ru (accessed: April 16, 2019). DOI: 10.18577/2307-6046-2018-0-1-4-4.
  2. Litiy: sverkhvozmozhnosti supermetalla [Lithium: supermechanical superopportunities] // Redkiye Zemli. Available at: http://rareearth.ru/ru/pub/20161026/02870.html (accessed: January 16, 2019).
  3. New partnership announced for large-scale lithium-geothermal project in California. Available at: http://www.thinkgeoenergy.com/new-partnership-announced-for-large-scale-lithium-geothermal-project-in-california/ (accessed: April 15, 2019).
  4. Minpromtorg provel soveshchaniye po razvitiyu litiyevoy otrasli v Rossii // Redkiye Zemli. Available at: http://rareearth.ru/ru/pub/20180914/04086.html (accessed: December 18, 2018).
  5. Minprirody Rossii razrabotalo mekhanizmy po sovershenstvovaniyu dobychi poputnykh poleznykh iskopayemykh i poputnykh komponentov. Available at: http://www.mnr.gov.ru/press/news/ minprirody_rossii_razrabotalo_mekhanizmy_po_sovershenstvovaniyu_dobychi_poputnykh_
  6. poleznykh_iskopaem/ (accessed: April 15, 2019).
  7. Mudring A. Ionic liquids open door to better rare-earth materials processing. Available at: https://www.ameslab.gov/news/news-releases/ionic-liquids-open-door-better-rare-earth-materials-processing (accessed: March 04, 2019).
  8. Dupont D., Binnemans K. Rare-earth recycling using a functionalized ionic liquid for the selective dissolution and revalorization of Y2O3: Eu3+ from lamp phosphor waste // Green Chemistry. 2015. Vol. 17. No. 2. P. 856–868.
  9. Method for direct separation of rare earth metals in uranium dioxide or spent fuel: pat. CN108538417A; appl. 03.04.18; publ. 14.09.18.
  10. Bagri P., Luo H., Dehaudt J. et al. Electrodeposition of neodymium using room temperature ionic liquids // 256th ACS National Meeting & Exposition (Boston, August 19–23, 2018). 2018. INOR-98.
  11. Matsumiya M. Purification of Rare Earth Amide Salts by Hydrometallurgy and Electrodeposition of Rare Earth Metals Using Ionic Liquids // Progress and Developments in Ionic Liquids. DOI: 10.5772/66300. Available at: https://www.intechopen.com/books/progress-and-developments-in-ionic-liquids/purification-of-rare-earth-amide-salts-by-hydrometallurgy-and-electrodeposition-of-rare-earth-metals (accessed: March 04, 2019).
  12. Chen L., Chen J., Li H. et al. Applying basic research on a dialkylphosphoric acid based task-specific ionic liquid for the solvent extraction and membrane separation of yttrium // Separation and Purification Technology. 2018. Vol. 207. P. 179–186.
  13. Separation of rate earth metals: International application WO2018109483A1; publ. 21.06.18.
  14. «VNIIKhT» razrabotal tekhnologiyu izvlecheniya redkozemelnykh metallov s pomoshchyu mikrovolnovogo izlucheniya [VNIIHT has developed a technology for extracting rare earth metals using microwave radiation] // Redkiye Zemli. Available at: http://rareearth.ru/ru/news/20180601/03957.html (accessed: March 04, 2019).
  15. «Dalur» vypustit pervuyu promyshlennuyu partiyu oksida skandiya v iyune 2017 goda [«Dalur» will release the first industrial batch of scandium oxide in June 2017] // Redkiye Zemli. Available at: http://rareearth.ru/ru/news/20170425/03131.html (accessed: February 15, 2019).
  16. Rosatom dobyl pervuyu partiyu skandiya [Rosatom extracted the first batch of scandium] // Redkiye Zemli. Available at: http://rareearth.ru/ru/news/ 20170713/03295.html (accessed: December 18, 2019).
  17. Mine of the Future // RioTinto. Available at: http://www.riotinto.com/ australia/pilbara/mine-of-the-future-9603.aspx (accessed: December 15, 2019).
  18. Raynesh E. Robot za rulem. «Intellektualnye karery», «umnyye mashiny» i bezopasnoe budushchee [Robot behind the wheel. «Intellectual careers», «smart machines» and a safe future] // Ugol Kuzbassa. 2017. №3. Available at: http://www.uk42.ru /index.php?id=5292 (accessed: March 15, 2019).
  19. Klebanov D.A., Makeyev M.A. Robotizirovannyye tekhnologii dobychi poleznykh iskopayemykh rozhdayutsya v nedrakh innovatsionnogo tsentra Skolkovo [Robotic technologies of mining are born in the depths of the innovation center Skolkovo] // Gornaya promyshlennost. 2012. №4. S. 132. Available at: https://mining-media.ru/ru/article/anonsy/2826-robotizirovannye-tekhnologii-dobychi-poleznykh-iskopaemykh-rozhdayutsya-v-nedrakh-innovatsionnogo-tsenta-skolkovo (accessed: November 15, 2018).
  20. Intellektualnyy karer – eto proyekt polnost'yu robotizirovannogo, bezlyudnogo gornogo predpriyatiya [Intellectual quarry is a project of a fully robotized, uninhabited mining enterprise] // Vist Grupp. Available at: http://vistgroup.ru/media/news/nid/intellectual-careers-project/ (accessed: November 15, 2018).
  21. Kabirov V.R., Reyshakhrit E.I. Effektivnost kompleksnogo podkhoda k razrabotke mestorozhdeniy metallicheskikh rud v gruppakh [The effectiveness of an integrated approach to the development of metal ore deposits in groups] // Zapiski Gornogo instituta. 2014. T. 208. S. 23–26.
  22. A Federal Strategy To Ensure Secure and Reliable Supplies of Critical Minerals / Executive Office of the President. Executive order 13817 of December 26, 2017.
  23. Kofner Yu.K. Konsolidatsiya redkozemelnoy industrii v Evropeyskom soyuze: rekomendatsii dlya Evraziyskogo ekonomicheskogo soyuza [Consolidation of the rare-earth industry in the European Union: recommendations for the Eurasian Economic Union] // Mezhdunar. konf. «Redkozemelnye metally 2019» (Moskva, 28 marta 2019 g.). Available at: http://eurasian-studies.org/archives/11704 (accessed: April 17, 2019).
  24. Doriomedov M.S., Sevastyanov D.V., Skripachev S.Yu., Daskovskiy M.I. Normativnaya dokumentatsiya v oblasti redkozemelnykh metallov [Reference documentation in the field of rare earth elements] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2018. №5 (65). St. 03. Available at: http://www.viam-works.ru (accessed: April 01, 2019). DOI: 10.18577/2307-6046-2018-0-5-18-23.
  25. The rise of electric cars could leave us with a big battery waste problem. Available at: https://www.theguardian.com/sustainable-business/2017/aug/10/electric-cars-big-battery-waste-problem-lithium-recycling (accessed: November 15, 2018).
  26. Analitiki predpolagayut izbytok predlozheniya litiya na rynke k 2022 godu [Analysts suggest an excess supply of lithium on the market by 2022] // Redkiye Zemli. Available at: http://rareearth.ru/ru/news/20170428 /03143.html (accessed: September 25, 2018).
  27. Shein E.A., Doriomedov M.S., Daskovskiy M.I. Sovremennyye materialy dlya raboty v usloviyakh arkticheskogo klimata [Advanced materials for arctic application] // Novosti materialovedeniya. Nauka i tekhnika: elektron. nauch.-tekhnich. zhurn. 2016. №1 (19). St. 07. Available at: http://materialsnews.ru/ru/articles (accessed: April 01, 2019).
  28. Buznik V.M., Kablov E.N. Sostoyaniye i perspektivy arkticheskogo materialovedeniya [State and prospects of the Arctic material science] // Vestnik Rossiyskoy akademii nauk. 2017. T. 87. №9. S. 827–839.
  29. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  30. Gasanov A.A., Naumov A.V., Yurasova O.V. i dr. Nekotoryye tendentsii mirovogo rynka RZM i perspektivy Rossii [Some trends in the world market of rare-earth metals and the prospects for Russia] // Izvestiya vuzov. Tsvetnaya metallurgiya. 2018. №4. S. 31–44. DOI: 10.17073/0021-3438-2018-4-31-44.
  31. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements – materials of modern and future high technologies] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №2. St. 01. Available at: http://www.viam-works.ru (accessed: May 20, 2015).