Kuznetsova V.A., Silaeva A.A., Shapovalov G.G., Marchenko S.A. Research of influence of mode of plastikation of carboxylated butadiene nitrile rubber and its contents in polymeric matrix on properties of fuel resistant coating // Proceedings of VIAM. 2019. No. 6 (78). Ст. 07. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2019-0-6-65-74.

Research of influence of mode of plastikation of carboxylated butadiene nitrile rubber and its contents in polymeric matrix on properties of fuel resistant coating

Kuznetsova V.A., Silaeva A.A., Shapovalov G.G., Marchenko S.A.
Abstract

In this work the analysis of researches of influence of the contents and time of plastikation of carboxylated butadiene nitrile rubber for properties of fuel resistant epoxy and rubber coatings is carried out. Researches of absorption process of free films and coatings on metal plates in water and in fuel were conducted, physicomechanical characteristics (tensile strength at break σр and relative lengthening εр) on the basis of what the optimum contents and time of plastikation of rubber for achievement of required properties was chosen. It is established that the content of rubber and way of its preparation influences the major indicators for fuel resistant coatings.

Keywords
fuel resistant coatings, rubber, epoxy, absorption curves, physicomechanical tests, free films.
Reference list
  1. Istoriya aviatsionnogo materialovedeniya. VIAM – 80 let: gody i lyudi / pod obshch. red. E.N. Kablova [History of Aeronautical Materials Science. VIAM – 80 years: years and people]. M.: VIAM, 2012. 520 s.
  2. Kablov E.N., Lukin V.I., Ospennikova O.G. Perspektivnyye alyuminiyevyye splavy i tekhnologii ikh soyedineniya dlya izdeliy aviakosmicheskoy tekhniki [Perspective aluminum alloys and technologies of their connection for aerospace products] // Tez. dokl. 2-oj Mezhdunar. konf. «Alyuminiy-21. Svarka i payka». Spb, 2012. St. 08.
  3. Kablov E.N. Na perekrestke nauki, obrazovaniya i promyshlennosti [At the crossroads of science, education and industry] // Ekspert. 2015. №15 (941). S. 49.
  4. Kablov E.N. Iz chego sdelat budushcheye? Materialy novogo pokoleniya, tekhnologii ikh sozdaniya i pererabotki – osnova innovatsiy [What to make the future from? Materials of the new generation, technologies of their creation and processing - the basis of innovation] // Krylya Rodiny. 2016. №5. S. 8–18.
  5. Shavnev A.A., Kurbatkina E.I., Kosolapov D.V. Metody soyedineniya alyuminiyevykh kompozitsionnykh materialov (obzor) [Methods for joining of aluminum composite materials (review)] // Aviacionnye materialy i tehnologii. 2017. №3 (48). S. 35–42. DOI: 10.18577/2071-9140-2017-0-3-35-42.
  6. Kondrashov E.K., Kuznetsova V.A., Semenova L.V., Lebedeva T.A. Osnovnyye napravleniya povysheniya ekspluatatsionnykh, tekhnologicheskikh i ekologicheskikh kharakteristik lakokrasochnykh pokrytiy dlya aviatsionnoy tekhniki [The main directions of improving the operational, technological and environmental performance of paint coatings for aircraft] // Rossiyskiy khimicheskiy zhurnal. 2010. T. LIV. №1. S. 96–102.
  7. Zhilikov V.P., Karimova S.A., Leshko S.S., Chesnokov D.V. Issledovanie dinamiki korrozii alyuminievyh splavov pri ispytanii v kamere solevogo tumana (KST) [Research of dynamics of corrosion of aluminum alloys when testing in the salt spray chamber (SSC)] // Aviacionnye materialy i tehnologii. 2012. №4. S. 18–22.
  8. Kablov E.N., Startsev O.V., Medvedev I.M. Obzor zarubezhnogo opyta issledovanij korrozii i sredstv zashhity ot korrozii [Review of international experience on corrosion and corrosion protection] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
  9. Chebotarevskiy V.V., Kondrashov E.K. Tekhnologiya lakokrasochnykh pokrytiy v mashinostroyenii [The technology of paint coatings in mechanical engineering]. M.: Mashinostroyeniye, 1978. S. 214–220.
  10. Vorobyev G.Ya. Khimicheskaya stoykost polimernykh materialov [Chemical resistance of polymeric materials]. M.: Khimiya, 1981. 296 s.
  11. Zuyev Yu.S. Razrusheniye polimera pod deystviyem agressivnykh sred. 2-ye izd. [The destruction of the polymer under the action of aggressive media. 2nd ed.]. M.: Khimiya, 1972. 232 s.
  12. Chertkov Ya.V., Spirkin V.G. Primeneniye reaktivnykh topliv v aviatsii [The use of jet fuels in aviation]. M.: Transport, 1974. 160 s.
  13. Narisava I. Prochnost polimernykh materialov. Per. s yap. [Strength of polymeric materials. Trans. from Jap.] M.: Khimiya, 1987. 364 s.
  14. Chalykh A.E. Diffuziya v polimernykh sistemakh [Diffusion in polymer systems]. M.: Khimiya, 1987. 312 s.
  15. Eskov A.A., Lebedeva T.A., Belova M.V. Lakokrasochnye materialy s ponizhennym soderzhaniem letuchih veshhestv (obzor) [Paint-and-lacquer materials with lowered content of volatile organic compounds (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №6. St. 08. Available at: http://www.viam-works.ru (accessed: February 01, 2019). DOI: 10.18577/2307-6046-2015-0-6-8-8.
  16. Kuznetsova V.A., Kuznetsov G.V., Shapovalov G.G. Issledovanie vliyaniya molekulyarnoj massy epoksidnoj smoly na adgezionnye, fiziko-mehanicheskie svojstva i erozionnuyu stojkost pokrytij [Investigation of epoxy resin molecular mass influence by physiomechanical property and erosive resistant of coatings] // Trudy VIAM: elektron. nauchn.-tehnich. zhurn. 2014. №8. St. 08. Available at: http://www.viam-works.ru (accessed: Novenber 19, 2018). DOI: 10.18577/2307-6046-2014-0-8-8-8.
  17. Pavlyuk B.Ph. Osnovnye napravleniya v oblasti razrabotki polimernyh funktsionalnyh materialov [The main directions in the field of development of polymeric functional materials] // Aviacionnye materialy i tekhnologii. 2017. №S. S. 388–392. DOI: 10.18577/2071-9140-2017-0-S-388-392.
  18. Sosnina S.A., Kuleshova I.D. Regulirovaniye vzaimodeystviya komponentov v napolnennykh lakokrasochnykh kompozitsiyakh [Regulation of the interaction of components in the filled paint and varnish compositions] // Lakokrasochnyye materialy i ikh primeneniye. 2011. №1. S. 60–62.
  19. Kuznecova V.A., Kuznecov G.V. Tendencii razvitiya v oblasti toplivostojkih lakokrasochnyh pokrytij dlya zashhity toplivnyh kesson-bakov letatelnyh apparatov (obzor) [Development trends in the field of fuel resistant paintwork coatings for protection of integral fuel tanks of aircrafts (review)] // Trudy VIAM: elektron. nauchn.-tehn. zhurn. 2014. №11. St. 08. Available at: http://www.viam works.ru (accessed: December 07, 2018). DOI: 10.18577/2307-6046-2014-0-11-8-8.
  20. Kochnova Z.A., Zhavoronok E.S., Kotova A.V. Osobennosti polucheniya epoksidno-kauchukovykh kompozitsiy na osnove zhidkikh butadiyen-nitrilnykh kauchukov i epoksidnykh oligomerov [Features of obtaining epoxy-rubber compositions based on liquid nitrile-butadiene rubbers and epoxy oligomers] // Lakokrasochnyye materialy i ikh primeneniye. 1998. №11. S. 27–28.
  21. Sostav dlya pokrytiya po metallu: pat. 2260610S1 Ros. Federatsiya [Composition for coating on metal: pat. 2260610С1 Rus. Federation]; zayavl. 13.05.04; opubl. 20.09.05.
  22. Sorokin M.F., Kochnova Z.A., Zakharova A.A., Golova N.A. Otverzhdeniye epoksidnykh oligomerov aminoalkoksisilanami [Curing of epoxy oligomers with aminoalkoxysilanes] // Lakokrasochnyye materialy i ikh primeneniye. 1986. №5. S. 24–28.
  23. Berlin A.A., Basin V.E. Osnovy adgezii polimerov [Basics of adhesion of polymers]. M.: Khimiya, 1969. 319 s.
  24. Kuznetsova V.A., Deyev I.S., Kondrashov E.K., Kuznetsov G.V. Vliyaniye otverditeley na mikrostrukturu i svoystva modifitsirovannogo epoksidnogo svyazuyushchego dlya toplivostoykogo pokrytiya [The effect of hardeners on the microstructure and properties of the modified epoxy binder for fuel resistant coating] // Vse materialy. Entsiklopedicheskiy spravochnik. 2012. №11. S. 38–41.
  25. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  26. Lutsenko A.N., Slavin A.V., Erasov V.S., Khvackij K.K. Prochnostnye ispytaniya i issledovaniya aviacionnyh materialov [Strength tests and researches of aviation materials] // Aviacionnye materialy i tehnologii. 2017. №S. S. 527–546. DOI: 10.18577/2071-9140-2017-0-S-527-546.
  27. Kochnova Z.A. Modifitsirovannyye epoksidnyye lakokrasochnyye materialy dlya antikorrozionnoy zashchity: dis. … d-ra khim. nauk [Modified epoxy paints for anticorrosion protection: thesis, Dr. Sc. (Tech.)]. M.: MKhTI, 1990. 464 s.
  28. Sorokin M.F., Kochnova Z.A., Zakharova A.A., Golova N.A. Otverzhdeniye epoksidnykh oligomerov aminoalkoksisilanami [Curing of epoxy oligomers with aminoalkoxysilanes] // Lakokrasochnyye materialy i ikh primeneniye. 1986. №5. S. 24–27.