Kasharina L.A., Makhsidov V.V. Identification of defects in polymeric composite materials by fiber bragg grating response (review). Part II // Proceedings of VIAM. 2019. No. 6 (78). Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2019-0-6-43-50.

Identification of defects in polymeric composite materials by fiber bragg grating response (review)

Part II
Kasharina L.A., Makhsidov V.V.
Abstract

The paper discusses the methods of detection, differentiation of the type of defects and their localization in polymer composite materials using embedded fiber-optic sensors using direct fiber-optic interrogation with an increased sampling rate of sensors. The types and stages of occurrence of defects are considered and the stages of their growth are described. The specific features of the response form from fiber-optic sensors are presented, which allow the analysis of formation mechanisms and the identification of defects types that occur in polymer composites under impact effects of different nature.

Keywords
defect identification, structure monitoring, polymer composite materials, fiber optic Bragg grating, deformation, impact damage.
Reference list
  1. Kablov У.N. Marketing materialovedeniya, aviastroyeniya i promyshlennosti: nastoyashcheye i budushcheye [Marketing materials, aviation and industry: present and future] // Direktor po marketingu i sbytu. 2017. №5–6. S. 40–44.
  2. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Kablov E.N. Stanovleniye otechestvennogo kosmicheskogo materialovedeniya [Formation of domestic space materials science] // Vestnik RFFI. 2017. №3. S. 97–105.
  4. Kablov E.N., Startsev O.V., Medvedev I.M., Shelemba I.S. Volokonno-opticheskiye datchiki dlya monitoringa korrozionnykh protsessov v uzlakh aviatsionnoy tekhniki (obzor) [Fiber optic sensors for monitoring corrosion processes in units of aviation engineering (review)] // Aviacionnye materialy i tehnologii. 2017. №3 (48). S. 26–34. DOI: 10.18577/2071-9140-2017-0-3-26-34.
  5. Sorokin K.V., Murashov V.V. Mirovye tendencii razvitiya raspredelennyh volokonno-opticheskih sensornyh sistem (obzor) [Global trends in development of distributed fiber-optic sensor systems (review)] //Aviacionnye materialy i tehnologii. 2015. №3 (36). S. 90–94. DOI: 10.18577/2071-9140-2015-0-3-90-94.
  6. Kablov E.N., Sivakov D.V., Gulyayev I.N. i dr. Primeneniye opticheskogo volokna v kachestve datchikov defopmatsii v polimepnykh kompozitsionnykh matepialakh [The use of optical fibers as sensors of deformation in polymeric composite materials] // Vse materialy. Entsiklopedicheskiy spravochnik. 2010. №3. S. 10–15.
  7. Kablov E.N., Startsev V.O. Sistemnyj analiz vliyaniya klimata na mekhanicheskie svojstva polimernykh kompozitsionnykh materialov po dannym otechestvennykh i zarubezhnykh istochnikov (obzor) [Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review)] // Aviacionnye materialy i tehnologii. 2018. №2 (51). S. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58..
  8. Beklemisheva K.A., Petrov I.B. Modelirovaniye razrusheniya gibridnykh kompozitov pod deystviyem nizkoskorostnogo udara [Simulation of the destruction of hybrid composites under the action of low-speed impact] // Matematicheskoye modelirovaniye. 2018. T. 3. №11. S. 27–43.
  9. Kudrin A.M., Karayeva O.A., Gabriyels K.S., Solopchenko A.V. Opredeleniye predela prochnosti polimernogo kompozitsionnogo materiala na szhatiye posle udara v sootvetstvii so standartom ASTM D 7137 [Determination of the tensile strength of a polymer composite material in compression after impact in accordance with ASTM D 7137] // Vestnik Voronezhskogo gos. tekhn. un-ta, 2018. T. 14. №2. S. 164–169.
  10. Zhao G., Li S., Hu H. et al. Impact localization on composite laminates using fiber Bragg grating sensors and a novel technique based on strain amplitude // Optical Fiber Technology. 2018. Vol. 40. P. 172–179. DOI: 10.1016/j.yofte.2017.12.001.
  11. Rezayat A., De Pauw B., Lamberti A. et al. Reconstruction of impacts on a composite plate using fiber Bragg gratings (FBG) and inverse methods // Composite Structures. 2016. Vol. 149. P. 1–10. DOI: 10.1016/j.compstruct.2016.03.065.
  12. Kim H., Shin H., Lee M., Kwac L. Impact Properties of Laminating Type in EVA and CFRP // Indian Journal of Science and Technology. 2015. Vol. 8 (26). P. 1–7. DOI: 10.17485/ijst/2015/v8i326/80679.
  13. Ostré B., Bouvet C., Minot C., Aboissière J. Experimental analysis of CFRP laminates subjected to compression after edge impact // Composite Structures. 2016. Vol. 152. P. 767–778. DOI: 10.1016/j.compstruct.2016.05.068.
  14. García-Moreno I., Caminero M.Á., Rodríguez G.P., López-Cela J.J. Effect of Thermal Ageing on the Impact Damage Resistance and Tolerance of Carbon-Fibre-Reinforced Epoxy Laminates // Polymers. 2019. Vol. 11. No. 160. DOI: 10.3390/polym11010160.
  15. Li H., Wang Z., Forrest J., Jiang W. Low-Velocity Impact Localization on Composites Under Sensor Damage by Interpolation Reference Database and Fuzzy Evidence Theory // Access IEEE. 2018. Vol. 6. P. 31157–31168. DOI: 10.1109/ACCESS.2018.2844802.
  16. Jiang M., Sai Y., Geng X., Sui Q. Development of an FBG Sensor Array for Multi-Impact Source Localization on CFRP Structures // Sensors. 2016. Vol. 16. No. 1770. P. 1–12. DOI: 10.3390/s16101770.
  17. Sai Y., Zhao X., Wang L., Hou D. Impact Localization of CFRP Structure Based on FBG Sensor Network // Photonic Sensors. 2019. DOI: 10.1007/s13320-019-0546-9.
  18. Kasharina L.A., Mahsidov V.V., Smirnv O.I., Ruzakov I.A. Differintsirovanie defektov v PKM po otkliku volokonno-opticheskih sensorov (obzor). Chast I [Identification of defects in polymeric composite materials by fiber Bragg grating response (review). Part I] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2019. №2 (74). St. 10. Available at: http://www.viam-works.ru (accessed: March 21, 2019) DOI: 10.18577/2307-6046-2019-0-2-97-104.
  19. Takeda N., Minakuchi S. Recent development of structural health monitoring technologies for aircraft composite structures in japan // Smart materials structure. 2003. No. 6. P. 456–467.
  20. Stukhlyak P.D., Buketov A.V., Panin S.V. i dr. Strukturnyye urovni razrusheniya epoksidnykh kompozitnykh materialov pri udarnom nagruzhenii [Structural destruction levels of epoxy composite materials under shock loading] // Fizicheskaya mezomekhanika. 2014. T. 17. №2. C. 65–83.
  21. Han G., Guan Z., Li X., Du S. Failure analysis of carbon fiber reinforced composite subjected to low velocity impact and compression after impact // Journal of Reinforced Plastics and Composites. 2016. DOI: 10.1177/0731684415627381.
  22. Ganesh Babu M., Velmurugan R., Gupta N.K. Heavy mass projectile impact on thin and moderately thick unidirectional fiber/epoxy laminates // Latin American Journal of Solids and Structures. 2007. No. 4. P. 247–265.
  23. Dellicolli A. Development of self-diagnostic composite structures using embedded fiber-bragg graying sensors: master of science dissertation. Michigan State University, 2012. URL: https://d.lib.msu.edu/etd/434 (дата обращения: 11.04.2019). DOI: 10.25335/M5VB6J.
  24. Brian Jenkins R., Joyce P., Mechtel D. Localized Temperature Variations in Laser-Irradiated Composites with Embedded Fiber Bragg Grating Sensors // Sensors. 2017. Vol. 17. No. 251. P. 2–18. DOI: 10.3390/s17020251.