Guseva M.A., Aslanyan I.R. The effect of fillers on the rheology of model composition // Proceedings of VIAM. 2019. No. 5 (77). Ст. 11. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2019-0-5-94-102.

The effect of fillers on the rheology of model composition

Guseva M.A., Aslanyan I.R.
Abstract

This paper presents the possibilities of assessing the technological properties of model compositions using the rheological method at the stage of developing of prayer compositions for investment casting. The analysis of the results of studies of the rheological behavior of the composition with the introduction of solid fillers – terephthalic acid, polyvinyl alcohol and rosin is carried out. It is shown that the rheological model of these compositions, regardless of the nature of the filler, is described by a model for a viscoplastic body. The influence of the filler concentration on the melting temperature range of model composition was established.

Keywords
rheological tests, rheological model, viscosity, model compositions, filler, investment casting.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Ospennikova O.G., Svetlov I.L. Vysokoeffektivnoe ohlazhdenie lopatok goryachego trakta GTD [Highly efficient cooling of GTE hot section blades] // Aviacionnye materialy i tehnologii. 2017. №2 (47). S. 3–14. DOI: 10.18577/2071-9140-2017-0-2-3-14.
  3. Kablov E.N., Ospennikova O.G., Lomberg B.S. Strategicheskiye napravleniya razvitiya konstruktsionnykh materialov i tekhnologiy ikh pererabotki dlya aviatsionnykh dvigateley nastoyashchego i budushchego [Strategic directions of development of structural materials and technologies for their processing for aviation engines of the present and the future] // Avtomaticheskaya svarka. 2013. №10. S. 23–32.
  4. Ospennikova O.G. Issledovanie i razrabotka parametrov tehnologicheskogo processa izgotovleniya modelej iz modelnyh kompozicij na osnove sinteticheskih voskov [Research and working out of parametres of technological process of manufacturing of models from modelling compositions on the basis of synthetic waxes] // Aviacionnye materialy i tehnologii. 2014. №3. S. 18–21. DOI: 10.18577/2071-9140-2014-0-3-18-21.
  5. Postizhenko V.K., Beregovaya O.S. Optimizatsiya tekhnologicheskikh parametrov modelnykh sostavov s pomoshch'yu matematicheskogo modelirovaniya [Strategic directions of development of structural materials and technologies for their processing for aviation engines of the present and the future] // Protsessy litya. 2009. №3. S. 43–47.
  6. Kablov E.N. Materialy i tekhnologii VIAM dlya «Aviadvigatelya» [Materials and technologies of VIAM for Aviadvigatel] // Permskiye aviatsionnyye dvigateli. 2014. №31. S. 43–47.
  7. Aslanyan I.R., Rassokhina L.I., Ospennikova O.G. Opredeleniye kolichestvennykh faktorov, sushchestvenno vliyayushchikh na tekhnologicheskiye kharakteristiki modelnykh kompozitsiy [Definition of quantitative factors, significantly influencing on technological characteristics of model compositions] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2018. №12 (72). St. 01. Available at: http://www.viam-works.ru (accessed: March 21, 2019). DOI: 10.18577/2307-6046-2018-0-12-3-13.
  8. Repyakh S.I. Klassifikatsiya vyplavlyayemykh modelnykh sostavov dlya tochnogo lit'ya // Informatsionnyy resurs po liteynomu proizvodstvu. Available at: http://www.lityo.com.ua (accessed: March 18, 2019).
  9. Aslanyan I.R., Guseva M.A., Ospennikova O.G. Sravnitel'noye issledovaniye fiziko-mekhanicheskikh i reologicheskikh kharakteristik modelnykh kompozitsiy [Determination of quantitative factors that significantly affect the technological characteristics of model compositions] // Vse materialy. Entsiklopedicheskiy spravochnik. 2019. №6. S. 34–39.
  10. Rassokhina L.I., Parfenovich P.I., Narskiy A.R. Problemy sozdaniya modelnykh kompozitsiy novogo pokoleniya na baze otechestvennykh materialov dlya izgotovleniya lopatok GTD [The issues of developing model compositions of new generation on the basis of domestic materials for the manufacture of gas turbine engine blades] // Novosti materialovedeniya. Nauka i tekhnika: elektron. nauch.-tekhnich. zhurn. 2015. №3 (15). St. 07. Available at: http://www.materialsnews.ru (accessed: March 20, 2019).
  11. Modelnaya kompozitsiya dlya vyplavlyayemykh modeley: pat. 2088370 Ros. Federatsiya [Model composition for smelted models: pat. 2088370 Rus. Federation]; zayavl. 07.04.95, opubl. 27.08.97.
  12. Prokopchuk N.R., Klyuyev A.Yu., Kozlov N.G. i dr. Issledovaniye vozmozhnosti ispolzovaniya modifitsirovannoy kanifoli v modelnykh sostavakh dlya tochnogo litya [Investigation of the possibility of using modified rosin in model compositions for precision casting] // Trudy BGTU. 2012. №4. S. 106–118.
  13. Modelnyy sostav: certificate of authorship 329949 SSSR. No. 1424395/22-2 [Model composition: a. with. 329949 USSR №1424395/22-2]; zayavl. 09.04.70; opubl. 24.11.72.
  14. Babin A.N., Guseva M.A. Reologicheskiy metod issledovaniya rastvorimosti komponentov v polimernykh kompozitsiyakh [Rheological method for studying the solubility of components in polymer compositions] // Vse materialy. Kommentarii k standartam, TU, sertifikatam. 2016. №4. S. 17–20.
  15. Ospennikova O.G. Issledovanie vliyaniya napolnitelej na svojstva i stabilnost modelnyh kompozicij, vybor optimalnyh sostavov [Influence research of fillers on properties and stability of modelling compositions, a choice of optimum structures] // Aviacionnye materialy i tehnologii. 2014. №3. S. 14–17. DOI: 10.18577/2071-9140-2014-0-3-14-17.
  16. Guseva M.A. Ispolzovaniye reologicheskogo metoda ispytaniy pri razrabotke polimernykh materialov razlichnogo naznacheniya [The use of the rheological tests in the development of polymeric materials for various purposes] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2018. №11 (71). St. 05. Available at: http://www.viam-works.ru (accessed: March 26, 2019). DOI: 10.18577/2307-6046-2018-0-11-35-44.