Kirin B.S., Lonskii S.L., Petrova G.N., Sorokin A.E. Materials for the 3D-printing on the basis of polyetheretherketones // Proceedings of VIAM. 2019. No. 4 (76). Ст. 03. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2019-0-4-21-29.

Materials for the 3D-printing on the basis of polyetheretherketones

Kirin B.S., Lonskii S.L., Petrova G.N., Sorokin A.E.
Abstract

Development of foreign production polyetheretherketon materials for the 3D printing by the selection laser baking (SLS) and fiber fusing (FDM) methods of on the basis of polyetheretherketones of foreign production. 3D-technologies allow to make aviation details and designs of the composite geometry for a uniform production cycle with minimum labor costs and quantity of a wastage. Results of compositions properties research for processing by SLS- and FDM-methods on the basis of polyetheretherketon of Zypeek (China) brands 550PF and 330UPF and also production of the Victrex company (England) brands 90G, 150G and 380G has been shown in article. The main requirements to such compositions and the principles of their preparation for processing has been formulated.

Keywords
polyetheretherketone, additive technologies, selection laser sintering, 3D-printing, layer-by-layer fusing, rused deposition molding.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Tendentsii i oriyentiry innovatsionnogo razvitiya Rossii [Trends and benchmarks of innovative development of Russia] // Sb. nauch.-inform. materialov. 3-e izd. M.: VIAM. 2015. 720 s.
  3. Kablov E.N. Additivnyye tekhnologii – dominanta natsional'noy tekhnologicheskoy initsiativy [Additive technologies - the dominant of the national technology initiative] // Intellekt i tekhnologii. 2015. №2 (11). S. 52–55.
  4. Kablov E.N. Iz chego sdelat budushcheye? Materialy novogo pokoleniya, tekhnologii ikh sozdaniya i pererabotki – osnova innovatsiy [What to make the future from? Materials of the new generation, technologies of their creation and processing - the basis of innovation] // Krylya Rodiny. 2016. №5. S. 8–18.
  5. Bikas H., Stavropoulos P., Chryssolouris G. Additive manufacturing methods and modeling approaches: a critical review // International Journal of Advanced Manufacturing Technology. 2016. Vol. 83. P. 389–405. DOI: 10.1007/s00170-015-7576-2.
  6. Petrova G.N., Larionov S.A., Sorokin A.E., Sapego Yu.A. Sovremennyye sposoby pererabotki termoplastov [Modern ways of processing of thermoplastics] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №11 (59). St. 07. Available at: http://www.viam-works.ru (accessed: May 14, 2018). DOI: 10.18577/2307-6046-2017-0-11-7-7.
  7. Grashchenkov D.V. Strategiya razvitiya nemetallicheskih materialov, metallicheskih kompozicionnyh materialov i teplozashhity [Strategy of development of non-metallic materials, metal composite materials and heat-shielding] // Aviacionnye materialy i tehnologii. 2017. №S. S. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  8. Nikolayev A.F. Termostoykiye polimery [Heat-resistant polymers]. L.: LTI im. Lensoveta, 1988. S. 3–11.
  9. Mikhaylin Yu.A. Konstruktsionnyye polimernyye kompozitsionnyye materialy [Structural polymer composites]. SPb.: Nauchnyye osnovy i tekhnologii, 2008. 822 s.
  10. Golovkin G.S. Tekhnologicheskiye svoystva termoplastichnykh svyazuyushchikh dlya armirovannykh plastikov [Technological properties of thermoplastic binders for reinforced plastics] // Plasticheskiye massy. 2005. №1. S. 35–40.
  11. Petrova G.N., Beyder E.Ya., Starostina I.V. Lityevyye termoplasty dlya izdeliy aviatsionnoy tekhniki [Molding thermoplastics for aviation equipment products] // Vse materialy. Entsiklopedicheskiy spravochnik. 2016. №6. S. 10–15.
  12. Mikhaylin Yu.A. Termoustoychivyye polimery i polimernyye materialy na ikh osnove [Heat-resistant polymers and polymeric materials based on them]. SPb.: Professiya, 2006. S. 33–346.
  13. Sorokin A.E., Afonicheva O.V., Krasnov A.P. i dr. Vliyaniye molekulyarnoy massy i metodov pererabotki na svoystva poliarilata DV [Influence of molecular weight and processing methods on the properties of DV polyarylate] // Sb. tez. IX simpoziuma «Sovremennaya khimicheskaya fizika». Tuapse, 2011. S. 156–157.
  14. Petrova G.N., Starostina I.V., Rumyanceva T.V., Sapego Yu.A. Effektivnost povysheniya kachestva izdelij iz polikarbonata termoobrabotkoj [Efficiency of improvement of quality of products from polycarbonate heat treatment] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №9 (57). St. 06. Available at: http://www.viam-works.ru (accessed: March 28, 2018). DOI: 10.18577/2307-6046-2017-0-9-6-6.
  15. Trostyanskaya E.B., Stepanova M.I., Rassokhin G.I. Teplostoykiye lineynyye polimery [Heat resistant linear polymers]. RGASKHM: Rostov n/D, 2002. S. 3–22.
  16. Kirin B.S., Mishkin S.I., Tikhonov N.N., Osipchik V.S. Razrabotka materialov na osnove polimolochnoy kisloty s uluchshennymi tekhnologicheskimi svoystvami [Development of materials based on polylactic acid with improved technological properties] // Plasticheskiye massy. 2013. №9. S. 61–64.
  17. PEEK™ – polymer für hohe Beanspruchungen // Galvanotechnik. 2004. Vol. 95. No. 3. P. 779.
  18. Mazhirin P.Yu. Polifenilensulfid v aviastroyenii [Polyphenylene sulfide in aircraft industry] // Polimernyye materialy. 2003. №2. S. 22–24.
  19. Un polymère pour applications «haute température» // Matériaux et Techniques. 2003. Vol. 91. No. 3–4. P. 52–53.
  20. Kerber M.L., Vinogradov V.M., Golovkin G.S. i dr. Polimernyye kompozitsionnyye materialy: struktura, svoystva, tekhnologiya [Polymeric composite materials: structure, properties, technology]. SPb.: Professiya, 2008. 199 s.
  21. Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Russia needs new generation materials] // Redkiye zemli. 2014. №3. S. 8–13.
  22. Buznik V.M., Kablov E.N. Arctic materials science: current state and prospects [Arctic materials science: current state and prospects] // Herald of the Russian Academy of Sciences. 2017. T. 87. No. 5. P. 397–408.
  23. Lazareva T.K., Ermakin S.N., Kostyagina V.A. Problemy sozdaniya kompozitsionnykh materialov na osnove konstruktsionnykh termoplastov [Problems of creating composite materials based on structural thermoplastics] // Uspekhi v khimii khimicheskoy tekhnologii. 2010. T. 24. №4. S. 58–63.