Abstract

The review of polymeric benzoxazines – promising polymer resins is reported. Comparison of the main characteristics of benzoxazines with existing types of resins is given. The main advantages and disadvantages, as well as methods for the synthesis of benzoxazines are considered. The potential of synthetic methods of polymeric benzoxazines is described, comparison with low molecular weight benzoxazines is reported. The details of the prospects for the expansion of benzoxazines as resins for polymer composite materials are concluded.

Keywords
benzoxazines, polymeric benzoxazines, olygomer benzoxazines, thermosets, composite materials, polymer composite materials.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Materials of new generation are neces-sary to Russia] // Redkie zemli. 2014. №3. S. 8–13.
  3. Composite Materials Handbook (CMH-17) Volume 3, Polymer Matrix Composites: Materials Usage, Design, and Analysis. SAE International, 2002. Vol. 3. 694 p.
  4. Kondrashov S.V., Shashkeev K.A., Petrova G.N., Mekalina I.V. Polimernye kompozicionnye materialy konstrukcionnogo naznacheniya s funkcionalnymi svojstvami [Constructional polymer composites with functional properties] // Aviacionnye materialy i tehnologii. 2017. №S. S. 405–419. DOI: 10.18577/2071-9140-2017-0-S-405-419.
  5. Raskutin A.E. Strategiia razvitiia polimernykh kompozitsionnykh materialov [Development strategy of polymer composite materials] // Aviatsionnye materialy i tekhnologii. 2017. №S. S. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
  6. Kablov E.N., Chursova L.V., Babin A.N., Mukhametov R.R., Panina N.N. Razrabotki FGUP «VIAM» v oblasti rasplavnykh svyazuyushchikh dlya polimernykh kompozitsionnykh materialov [Development of VIAM Federal State Unitary Enterprise in the field of molten binding for polymeric composite materials] // Polimernye materialy i tekhnologii. 2016. T. 2. №2. S. 37–42.
  7. Ishida H., Froimowicz P. Advanced and Emerging Polybenzoxazine Science and Technology. Netherlands: Elsevier, 2017. 1126 p.
  8. Zheleznyak V.G., Muhametov R.R., Chursova L.V. Issledovanie vozmozhnosti sozdaniya termoreaktivnogo svyazujushhego na rabochuju temperaturu do 400°C [Study of possibility of thermoset binder creation for operating temperature up to 400°C] // Aviacionnye materialy i tehnologii. 2013. №S2. S. 58–61.
  9. Lin C.H., Chang S.L., Shen T.Y., Shih Y.S. Flexible polybenzoxazine thermosets with high glass transition temperatures and low surface free energies // Polymer Chemistry. 2012. Vol. 3. P. 935. DOI: 10.1039/C2PY00449F.
  10. Brunovska Z., Liu J.P., Ishida H. 1,3,5-Triphenylhexahydro-1,3,5-triazine – active intermediate and precursor in the novel synthesis of benzoxazine monomers and oligomers // Macromolecular Chemistry and Physics. 1999. Vol. 200. Р. 1745–1752. DOI: 10.1002/(SICI)1521-3935(19990701)200:71745::AID-MACP1745>3.0.CO;2-D.
  11. Lin C.H., Chang S.L., Hsieh C.W. Aromatic diamine-based benzoxazines and their high performance thermosets // Polymer. 2008. Vol. 49. P. 1220–1229. DOI: 10.1016/j.polymer.2007.12.042.
  12. Demir K.D., Kiskan B., Aydogan B., Yagci Y. Thermally curable main-chain benzoxazine prepolymers via polycondensation route // Reactive & Functional Polymers. 2013. Vol. 73. P. 346–359.
  13. Chao L., Shen D., Sebastián R.M., Marquet J. Mechanistic Studies on Ring-Opening Polymerization of Benzoxazines: A Mechanistically Based Catalyst Design // Macromolecules. 2011. Vol. 44. P. 4616–4622. DOI: 10.1021/ma2007893.
  14. Yelda E., Tamer U. Main-chain polybenzoxazine nanofibers via electrospinning // Polymer. 2014. Vol. 55. P. 556–564. DOI: 10.1016/j.polymer.2013.12.018.
  15. Rimdusit S., Hemvichian K., Kasemsiri P., Dueramae I. Shape memory polymers from benzoxazine-modified epoxy // Smart Materials Structures. 2013. Vol. 22. P. 12. DOI: 10.1088/0964-1726/22/7/075033.
  16. Ishida H., Agag T. Handbook of Benzoxazine Resins. Amsterdam: Elsevier, 2011. 688 p. DOI: doi.org/10.1016/B978-0-444-53790-4.00063-1.
  17. Aydogan B., Sureka D., Kiskan B., Yagci Y. Polysiloxane‐containing benzoxazine moieties in the main chain // Journal of Polymer Science. Part A: Polymer Chemistry. 2010. Vol. 48. P. 5156–5162.
  18. Demir K.D., Kiskan B., Yagci Y. Thermally Curable Acetylene-Containing Main-Chain Benzoxazine Polymers via Sonogashira Coupling Reaction // Macromolecules. 2011. Vol. 44. P. 1801–1807.
  19. Ghosh N., Kiskan B., Yagci Y. Polybenzoxazines – new high performance thermosetting resins: synthesis and properties // Progress in Polymer Science. 2007. Vol. 32. P. 1344–1391.
  20. Lin C.H., Chang S.L., Shen T.Y. et al. Flexible polybenzoxazine thermosets with high glass transition temperatures and low surface free energies // Polymer Chemistry. 2012. Vol. 3. P. 935–945.
  21. Wang M., Jeng R., Lin C. The robustness of a thermoset of a main-chain type polybenzoxazine precursor prepared through a strategy of A–A and B–B polycondensation // RSC Advances. 2016. Vol. 6. P. 18678–18684. DOI: 10.1039/C5RA25619D.
  22. Allen D.J., Ishida H. Effect of phenol substitution on the network structure and properties of linear aliphatic diamine based benzoxazines // Polymer. 2009. Vol. 50. P. 613–626.
  23. Sawaryn C., Landfester K., Taden A. Benzoxazine miniemulsions stabilized with multifunctional main-chain benzoxazine protective colloids // Macromolecules. 2011. Vol. 44. P. 5650–5658. DOI: /doi/10.1021/ma200973g.
  24. Velez-Herrera P., Doyama K., Abe H., Ishida H. Synthesis and characterization of highly fluorinated polymer with the benzoxazine moiety in the main chain // Macromolecules. 2008. Vol. 41. P. 9704–9714.
  25. Deliballi Z., Kiskan B., Yagci Y. Main-chain benzoxazine precursor block copolymers // Polymer Chemistry. 2018. Vol. 9. P. 178–183.
  26. Ishida H., Lee Y. Infrared and thermal analyses of polybenzoxazine and polycarbonate blends // Application Polymer Science. 2001. Vol. 81. P. 1021–1034. DOI: 10.1002/app.1524.
  27. Chernykh A., Agag T., Ishida H. Synthesis of linear polymers containing benzoxazine moieties in the main chain with high molecular design versatility via click reaction // Polymer. 2009. Vol. 50. P. 382–390. DOI: 10.1016/j.polymer.2008.11.017.
  28. Chen N.H., Li H.Y., Lai J.-Y., Liu Y.-L. Synthesis and characterization of benzoxazine-containing, crosslinkable, and sulfonated polymer through Diels–Alder reaction for direct methanol fuel cells // Polymer. 2013. Vol. 54. P. 2096–2104.
  29. Gacal B., Akat H., Balta D.K. et al. Synthesis and Characterization of Polymeric Thioxanthone Photoinitatiors via Double Click Reactions // Macromolecules. 2008. Vol. 41. P. 2401–2405.
  30. Baqar M., Agag T., Ishida H. Poly(benzoxazine-co-urethane)s: A new concept for phenolic/urethane copolymers via one-pot method // Polymer. 2011. Vol. 52. P. 307–317. DOI: 10.1016/j.polymer.2010.11.052.
  31. Aydogan B., Sureka D., Kiskan B., Yagci Y. Polysiloxane‐containing benzoxazine moieties in the main chain // Polymer Science Part A: Polymer Chemistry. 2010. Vol. 48. P. 5156–5162. DOI: 10.1002/pola.24313.
  32. Kiskan B., Aydogan B., Yagci Y. Recent advancement on polybenzoxazine – A newly developed high performance thermoset // Polymer Science. Part A: Polymer Chemistry. 2010. Vol. 47. P. 804–811. DOI: 10.1002/pola.23597.
  33. Takeichi T., Kano T., Agag T. Synthesis and thermal cure of high molecular weight polybenzoxazine precursors and the properties of the thermosets // Polymer. 2005. Vol. 46. P. 12172–12180. DOI: /10.1016/j.polymer.2005.10.088.
  34. Barrett D.G., Yousaf M.N. Biocompatible multiblock aliphatic polyesters containing ether-linkages: influence of molecular architecture on solidstate properties and hydrolysis rate // Soft Matterials. 2010. Vol. 6. P. 5026–5036. DOI: 10.1039/C4RA04248D.
  35. Chernykh A., Liu J.P., Ishida H. Synthesis and properties of a new cross linkable polymer containing benzoxazine moiety in the main chain // Polymer. 2006. Vol. 47. P. 7664–7669. DOI: /10.1016/j.polymer.2006.08.041.
  36. Kiskan B., Yagci Y., Ishida H. Synthesis, characterization and properties of new thermally curable polyetheresters containing benzoxazine moieties in the main chain // Journal Polymer Science. Part A: Polymer Chemistry. 2008. Vol. 46. P. 414–420.
  37. Binder W.H., Zirbs R. Encyclopedia of Polymer Science and Technology: «Click» Chemistry in Macromolecular Synthesis. New York: John Wiley&Sons, 2002. p. 45.
  38. Zhang M., Feng C., Lin K., Lunn D. Modular Synthesis of Polyferrocenylsilane Block Copolymers by Cu-Catalyzed Alkyne/Azide «Click» Reactions // Macromolecules. 2013. Vol. 46. P. 1296–1304. DOI: 10.1021/ma302054q.
  39. Nagai A., Kamei Y., Wang S. et al. Synthesis and crosslinking behavior of a novel linear polymer bearing 1,2,3-triazol the main chain by and benzoxazine groups in a step-growth click-coupling reaction // Journal Polymer Science. Part A: Polymer Chemistry. 2008. Vol. 46. P. 2316–2325.
  40. Chernykh A., Agag T., Ishida H. Synthesis of linear polymers containing benzoxazine moieties in the main chain with high molecular design versatility via click reaction // Polymer. 2009. Vol. 50. P. 382–390.
  41. Ye Y.S., Huang Y.J., Chang F.C., Xuea Z.G. Synthesis and characterization of thermally cured polytriazole polymers incorporating main or side chain benzoxazine crosslinking moieties // Polymer Chemistry. 2014. Vol. 5. P. 2863–2871. DOI: 10.1039/C3PY01432K.
  42. Chou C.I., Liu Y.L. High performance thermosets from a curable Diels–Alder polymer possessing benzoxazine groups in the main chain // Polymer Science. Part A: Polymer Chemistry. 2008. Vol. 46. P. 6509–6517. DOI: https://doi.org/10.1002/pola.22960.
  43. Kiskan B., Yagci Y., Ishida H. Synthesis, characterization, and properties of new thermally curable polyetheresters containing benzoxazine moieties in the main chain // Polymer Science. Part A: Polymer Chemistry. 2007. Vol. 46. P. 414–420. DOI: /10.1002/pola.22392.
  44. Kiskan B., Colak D., Cianga I., Yagci Y. Synthesis and Characterization of Thermally Curable Benzoxazine‐Functionalized Polystyrene Macromonomers // Macromolecules Rapid Communication. 2005. Vol. 26. P. 819–824. DOI: /10.1002/marc.200500079.
  45. Kiskan B., Yagci Y. Synthesis and characterization of naphthoxazine functional poly(ε-caprolactone) // Polymer. 2005. Vol. 46. P. 11690–11697. DOI: /10.1016/j.polymer.2005.09.061.
  46. Tasdelen M.A., Kiskan B., Yagci Y. Photoinitiated Free Radical Polymerization Using Benzoxazines as Hydrogen Donors // Macromolcules Rapid Communication. 2006. Vol. 27. P. 1539–1544. DOI: 10.1002/marc.200600424.
  47. Agag T., Vietmeier K., Chernykh A., Ishida H. Side-chain type benzoxazine-functional cellulose via click chemistry // Journal Application Polymer Science. 2012. Vol. 125. P. 1346–1351.
  48. Takeichi T., Thongpradith S., Kawauchi T. Copolymers of Vinyl-Containing Benzoxazine with Vinyl Monomers as Precursors for High Performance Thermosets // Molecules. 2015. Vol. 20. P. 6488–6503. DOI: 10.3390/molecules20046488.
  49. He-Ming M., Yun L., Ying-Xuan L., Jin-Jun Q. Vinyl benzoxazine: a novel heterobifunctional monomer that can undergo both free radical polymerization and cationic ring-opening polymerization // RSC Advances. 2015. Vol. 5. P. 102441–102447. DOI: 10.1039/C5RA18058A.
  50. Brunovska Z., Lyon R., Ishida H. Thermal properties of phthalonitrile functional polybenzoxazines // Thermochim Acta. 2000. Vol. 357–358. P. 195–203. DOI: /10.1016/S0040-6031(00)00388-9.
  51. Zou X., Yang X., Xu M. et al. Curing behaviors and properties of allyland benzoxazine-functional phthalonitrile with improved processability // Journal Polymer Research. 2016. Vol. 23. No. 2. P. 1–9. DOI: 10.1007/s10965-015-0891-3.
  52. Koz B., Kiskan B., Yagci Y. A novel benzoxazine monomer with methacrylate functionality and its thermally curable (co)polymers // Polymer Bulletin. 2011. Vol. 66. P. 165–174.
  53. Liu Y.X., Ma H.M., Liu Y. et al. A well-defined poly (vinyl benzoxazine) obtained by selective free radical polymerization of vinyl group in bifunctional benzoxazine monomer // Polymer. 2016. Vol. 82. P. 32–39.
  54. Kiskan B., Demiray G.N., Yagci Y. Thermally Curable Polyvinylchloride via Click Chemistry // Journal of Polymer Science. Part A: Polymer Chemistry. 2008. Vol. 46. P. 3512–3518. DOI: 10.1002/pola.22685.
  55. Thongpradith T., Hirai S., Takiguchi S., Kawauchi T., Takeichi T. Syntheses of novel benzoxazines having vinyl groups and thermal properties of the thermosets // High Performance Polymers. 2012. Vol. 24. No. 8. P. 765–774. DOI: 10.1177/0954008312451479.
  56. Shilin L., Jianying Y. Synthesis and Characterization of New Benzoxazine-Based Phenolic Resins from Renewable Resources and the Properties of Their Polymers Shengfang // Journal of Applied Polymer Science. 2011. Vol. 122. P. 2843–2848.
  57. Tsukahara Y., Adachi K. Encyclopedia of Polymeric Nanomaterials, Telechelic Polymer: Preparation and Application. Springer. Berlin/Heidelberg, 2015. P. 2491–2498.
  58. Nakamura M., Ishida H. Synthesis and properties of new crosslinkable telechelics with benzoxazine moiety at the chain end // Polymer. 2009. Vol. 50. P. 2688–2695.
  59. Li Y., Zhang C.Y., Zheng S.X. Microphase separation in polybenzoxazine thermosets containing benzoxazine-terminated poly(ethylene oxide) telechelics // European Polymer Journal. 2011. Vol. 47. P. 1550–1562.
  60. Ates S., Dizman C., Aydogan B. et al. Synthesis, characterization and thermally activated curing of polysulfones with benzoxazine end groups // Polymer. 2011. Vol. 52. P. 1504–1509.
  61. Orhana T., Atesb S., Hacaloglua J., Yagci Y. Thermal degradation characteristics of polysulfones with benzoxazine end groups // Journal Anallytical Applied Pyrolysis. 2012. Vol. 94. P. 146–152.
  62. Liu J., Agag T., Ishida H. Main-chain benzoxazine oligomers: a new approach for resin transfer moldable neat benzoxazines for high performance applications // Polymer. 2010. Vol. 51. P. 5688–5694. DOI: /10.1016/j.polymer.2010.08.059.
  63. Zhang K., Qiu J., Li S. et al. Remarkable improvement of thermal stability of main-chain benzoxazine oligomer by incorporating o-norborneneas terminal functionality // Journal Application Polymer Science. 2017. Vol. 134. P. 45408–45415. DOI: /10.1002/app.45408.
  64. Qingyu X., Ming Z., Jiangbing C. et al. Synthesis, polymerization kinetics, and high-frequency dielectric properties of novel main-chain benzoxazine copolymers // Reactive and functional polymers. 2018. Vol. 122. P. 158–166.