Rassokhina L.I., Bityutskaya O.N., Gamazina M.V., Echin A.B. Technological process development of casting details «diffuser» for gas turbine engines from VZh159 superalloy in the conditions of the machine-building enterprise // Proceedings of VIAM. 2019. No. 12 (84). Ст. 03. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2019-0-12-20-28.

Technological process development of casting details «diffuser» for gas turbine engines from VZh159 superalloy in the conditions of the machine-building enterprise

Rassokhina L.I., Bityutskaya O.N., Gamazina M.V., Echin A.B.
Abstract

The results of development the technological process of obtaining casting parts «diffuser» for gas turbine engines in the conditions of machine-building enterprise are presented. Nondestructive testing was carried out to identify metallurgical defects on castings, and tensile and long – term strength tests were carried out to determine mechanical properties. The conclusion is made that the fulfilled technological process of casting of shaped parts from VZh159 superalloy allows to recommend it to serial production for production of shaped castings of details of aircraft engines.

Keywords
alloy VZh159, superalloys, casting properties, gate-feeding system, gas turbine engines.
Reference list
  1. Sorokin L.I. Svarivayemost zharoprochnykh splavov, primenyayemykh v aviatsionnykh gazoturbinnykh dvigatelyakh [Weldability of heat-resistant alloys used in aircraft gas turbine engines] // Svarochnoye proizvodstvo. 1997. №4. S. 4–11.
  2. Lomberg B.S., Ovsepyan S.V., Bakradze M.M., Mazalov I.S. Vysokozharoprochnyye deformiruyemyye nikelevyye splavy dlya perspektivnykh gazoturbinnykh dvigateley i gazoturbinnykh ustanovok [High-temperature wrought wrought nickel alloys for promising gas turbine engines and gas turbine units] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroyeniye, 2011. №SP2. S. 98–103.
  3. Moiseev S.A., Latyshev V.B. Zharoprochnyye svarivayemyye splavy dlya uzlov statora sovremennykh i perspektivnykh aviatsionnykh GTD [Heat resisting welded alloys for nodes of stator of modern and perspective aviation GTD] // Aviacionnye materialy i tehnologii. 2003. №1. S. 152–157.
  4. Kablov E.N. Tendentsii i oriyentiry innovatsionnogo razvitiya Rossii: sb. nauch.-inform. materialov. 3-e izd. [Tendencies and guidelines for innovative development of Russia: collection of scientific and information materials. 3rd ed.]. M.: VIAM, 2015. 720 s.
  5. Kablov E.N., Ospennikova O.G., Lomberg B.S., Sidorov V.V. Prioritetnye napravleniya razvitiya tekhnologiy proizvodstva zharoprochnykh materialov dlya aviatsionnogo dvigatelestroyeniya [Priority areas for the development of technologies for the production of heat-resistant materials for aircraft engine manufacturing] // Problemy chernoy metallurgii i materialovedeniya. 2013. №3. S. 47–54.
  6. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Liteynyye zharoprochnyye nikelevyye splavy dlya perspektivnykh aviatsionnykh GTD [Heat-resistant nickel alloys for advanced aviation gas turbine engines] // Tekhnologiya legkikh splavov. 2007. №2. S. 6–16.
  7. Evgenov A.G., Rogalev A.M., Nerush S.V., Mazalov I.S. Issledovanie svojstv splava EP648, poluchennogo metodom selektivnogo lazernogo splavleniya metallicheskih poroshkov [A study of properties of EP648 alloy manufactured by the selective laser sintering of metal powders] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №2. St. 02. Available at: http://www.viam-works.ru (accessed: October 24, 2019). DOI: 10.18577/2307-6046-2015-0-2-2-2.
  8. Evgenov A.G., Gorbovec M.A., Prager S.M. Struktura i mehanicheskie svojstva zharoprochnyh splavov VZh159 i EP648, poluchennyh metodom selektivnogo lazernogo splavleniya [Structure and mechanical properties of heat resistant alloys VZh159 and EP648, prepared by selective laser fusing] // Aviacionnye materialy i tehnologii. 2016. №S1. S. 8–15. DOI: 10.18577/2071-9140-2016-0-S1-8-15.
  9. Kablov E.N., Evgenov A.G., Ospennikova O.G., Semenov B.I., Semenov A.B., Korolev V.A. Metalloporoshkovyye kompozitsii zharoprochnogo splava EP648 proizvodstva FGUP «VIAM» GNTS RF v tekhnologiyakh selektivnogo lazernogo splavleniya, lazernoy gazoporoshkovoy naplavki i vysokotochnogo lit'ya polimerov, napolnennykh metallicheskimi poroshkami [Metal powder compositions of the heat-resistant alloy EP648 manufactured by FSUE «VIAM» SSC RF in technologies of selective laser fusion, laser gas-powder surfacing and high-precision casting of polymers filled with metal powders] // Izvestiya vysshikh uchebnykh zavedeniy. Ser: Mashinostroyeniye. 2016. №9 (678). S. 62–80.
  10. Mazalov I.S., Evgenov A.G., Prager S.M. Perspektivy primeneniya zharoprochnogo strukturnostabilnogo splava VZh159 dlya additivnogo proizvodstva vysokotemperaturnyh detalej GTD [Perspectives of heat resistant structurally stable alloy VZh159 application for additive production of high-temperature parts of GTE] // Aviacionnye materialy i tehnologii. 2016. №S1. S. 3–7. DOI: 10.18577/2071-9140-2016-0-S1-3-7.
  11. Evgenov A.G., Rogalev A.M., Karachevtsev F.N., Mazalov I.S. Vliyaniye goryachego izostaticheskogo pressovaniya i termicheskoy obrabotki na svoystva splava EP648, sintezirovannogo metodom selektivnogo lazernogo splavleniya [The effect of hot isostatic pressing and heat treatment on the properties of the EP648 alloy synthesized by selective laser fusion] // Tekhnologiya mashinostroyeniya. 2015. №9. S. 11–16.
  12. Lomberg B.S., Moiseyev S.A. Zharoprochnyye i deformiruyemyye splavy dlya sovremennykh i perspektivnykh GTD [Heat-resistant and deformable alloys for modern and promising gas-turbine engines] // Vse materialy. Entsiklopedicheskiy spravochnik. 2007. №6. S. 2–5.
  13. Lomberg B.S., Kapitanenko D.V., Mazalov I.S., Bubnov M.V. Tekhnologicheskie parametry polucheniya detaley kholodnoy shtampovkoy iz listovykh zagotovok zharoprochnykh splavov VZH159, VZh171 i vysokoprochnogo splava VZh172 [Technological parameters for producing parts by cold stamping from sheet blanks of heat-resistant alloys VZh159, VZh171 and high-strength alloy VZh172] // Kuznechno-shtampovochnoye proizvodstvo. Obrabotka materialov davleniyem. 2015. №8. S. 14–19.
  14. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  15. Kablov E.N., Petrushin N.V., Svetlov I.L. Sovremennyye litye nikelevye zharoprochnye splavy [Modern Cast Nickel Heat Resistant Alloys] // Tr. Mezhdunar. nauch.-tekhnich. konf. «Nauchnyye idei S.T. Kishkina i sovremennoye materialovedeniye». M.: VIAM, 2006. S. 39–55.