Kolpachkov E.D., Petrova A.P., Kurnosov A.O., Sokolov I.I. Methods of molding aviation products from PCM (review) // Proceedings of VIAM. 2019. No. 11 (83). Ст. 03. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2019-0-11-22-36.

Methods of molding aviation products from PCM (review)

Kolpachkov E.D., Petrova A.P., Kurnosov A.O., Sokolov I.I.
Abstract

This paper presents the basic methods of molding aviation products from polymer composite materials (PCM). For the analysis of the presented methods, a classification is proposed, which is based on the principle of separation into prepreg, non-prepreg, and other methods. The distinctive features of these methods are analyzed, the main technological parameters are considered, the process flow diagrams are presented, as well as the molding equipment circuits, the main advantages and disadvantages are given.

Keywords
PCM, product aviation purpose, methods of processing of polymer PCM, composite materials.
Reference list
  1. Kablov E.N. Iz chego sdelat budushcheye? Materialy novogo pokoleniya, tekhnologii ikh sozdaniya i pererabotki – osnova innovatsiy [What to make the future of? Materials of a new generation, technologies for their creation and processing – the basis of innovation] // Krylya Rodiny. 2016. №5. S. 8–18.
  2. Kablov E.N., Startsev V.O. Sistemnyj analiz vliyaniya klimata na mekhanicheskie svojstva polimernykh kompozitsionnykh materialov po dannym otechestvennykh i zarubezhnykh istochnikov (obzor) [Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review)] // Aviacionnye materialy i tehnologii. 2018. №2 (51). S. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  3. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  4. Raskutin A.E. Strategiia razvitiia polimernykh kompozitsionnykh materialov [Development strategy of polymer composite materials] // Aviaсionnye materialy i tehnologii. 2017. №S. S. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
  5. Bychkov R.A. Fizika i khimiya materialov pokrytiy: ucheb.-metod. posobiye [Physics and chemistry of coating materials: tutorial]. M.: MGAPI, 2004. 268 s.
  6. Dzhogan O.M., Kostenko O.P. Metody propitki pod davleniyem [Pressure impregnation methods] // Voprosy proyektirovaniya i proizvodstva konstruktsiy letatelnykh apparatov. 2011. №4. S. 111–125.
  7. Kogan D.I. Tekhnologiya izgotovleniya polimernykh kompozitsionnykh materialov sposobom propitki plenochnymi svyazuyushchimi: dis. … kand. tekhn. nauk [The manufacturing technology of polymer composite materials by the method of impregnation with film binders: thesis, Cand. Sc. (Tech.)]. M.: VIAM, 2011. 139 s.
  8. Kallister U., Ritvich D. Materialovedeniye: ot tekhnologii k primeneniyu (metally, keramika, polimery) [Material science: from technology to application (metals, ceramics, polymers).]. SPb.: Nauchnyye osnovy i tekhnologii, 2011. 896 s.
  9. Balakirev V.S., Zayev A.V., Bolshakov A.A. i dr. Avtomatizirovannyye proizvodstva izdeliy iz kompozitsionnykh materialov [Automated production of products from composite materials]. M.: Khimiya, 1990. 240 s.
  10. Trostyanskaya E.B., Golovkin G.S., Dmitrenko V.P. i dr. Perspektivnyye PKM i progressivnyye tekhnologii proizvodstva iz nikh elementov konstruktsii LA [Promising PCM and advanced technologies for the production of aircraft structural elements from them] // Aviatsionnaya promyshlennost. 1987. №2. S. 37–42.
  11. Bratukhin A.G., Bogolyubov V.S., Sirotkin O.S. Tekhnologiya proizvodstva izdeliy i integralnykh konstruktsiy iz kompozitsionnykh materialov v mashinostroyenii [Technology for the production of products and integrated structures from composite materials in mechanical engineering]. M.: Gotika, 2003. 516 s.
  12. Dushin M.I., Hrulkov A.V., Muhametov R.R. Vybor tehnologicheskih parametrov avtoklavnogo formovaniya detalej iz polimernyh kompozicionnyh materialov [A choice of technological parameters of autoclave formation of details from polymeric composite materials] // Aviacionnye materialy i tehnologii. 2011. №3. S. 20–26.
  13. Kolosov A.E., Repelis I.A., Khozin V.G., Klyavin V.V. Propitka voloknistykh napolniteley polimernym svyazuyushchim [The impregnation of fibrous fillers with a polymer binder] // Mekhanika kompozitnykh materialov. 1988. №3. S. 490–496.
  14. Fisher K. Autoclave quality outside the autoclave? // High-Performance Composites. 2006. Vol. 21. No. 2. P. 14–23.
  15. MS-21 – layner s «chernym» krylom [MS-21 is a liner with a «black» wing] // Aviatsiya Rossii^ internet-portal. Available at: http://www.aviation21.ru (accessed: October 18, 2019).
  16. Nelyub V.A., Grashchenkov D.V., Kogan D.I., Sokolov I.A. Primeneniye pryamykh metodov formovaniya pri proizvodstve krupnogabaritnykh detaley iz stekloplastikov [The use of direct molding methods in the production of large-sized parts from fiberglass] // Khimicheskaya tekhnologiya. 2012. №12. S. 735–739.
  17. Gusev Yu.A., Borshhev A.V., Khrulkov A.V. Osobennosti prepregov dlya avtomatizirovannoj vykladki metodami ATL i AFP [Features of prepregs intended for automated laying by ATL and AFP technologies] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №3. St. 06. Available at: http://www.viam-works.ru (accessed: September 19, 2019). DOI: 10.18577/2307-6046-2015-0-3-6-6.
  18. Sloan J. ATL and AFP: defining the megatrends in composite aerostructures // High Performance Composites. 2008. Vol. 22. No. 6. P. 20–25.
  19. Komarov V.A., Kurkin E.I., Kuznetsov A.S. Issledovaniye i modifikatsiya osnastki i formoobrazuyushchey poverkhnosti s tselyu povysheniya tochnosti izgotovleniya detaley metodom vakuumnoy infuzii [Research and modification of tooling and shaping surface in order to increase the accuracy of manufacturing parts by vacuum infusion] // Izvestiya Samarskogo nauchnogo tsentra RAN. 2013. T. 15. №6 (3). Available at: https://cyberleninka.ru (accessed: November 05, 2019).
  20. Dushin M. I., Hrulkov A.V., Muhametov R.R., Chursova L.V. Osobennosti izgotovleniya izdelij iz PKM metodom propitki pod davleniem [Features of manufacturing of products from PCM impregnation method under pressure] // Aviacionnye materialy i tehnologii. 2012. №1. S. 18–26.
  21. Metod vakuumnoy infuzii i oblasti yeye primeneniya. Ustanovki vakuumnoy infuzii // Oborudovanie dlya sozdaniya i podderzhaniya vakuuma. Laboratornye i promyshlennye vakuumnye sistemy I termicheskoe oborudovanie. Available at: http://www.uksim-oz.ru (accessed: October 18, 2019).
  22. Vacuum injection process for manufacturing fiber reinforced composite products involves evacuating second chamber causing resin to flow into preform in adjacent evacuated first chamber: pat. 10013409 DE; filed 17.03.00; publ. 23.11.00.
  23. Ivanov M.S., Nesterova T.A., Platonov M.M. Polupronitsayemyye membrany dlya protsessa vakuumnoy infuzii PKM (obzor) [Semipermeable membranes for vacuum infusion molding of polymer composite materials (review)] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2017. №2 (50). St. 07. Available at: http://www.viam-works.ru (accessed: October 21, 2019). DOI: 10.18577/2307-6046-2017-0-2-7-7.
  24. Chursova L.V., Dushin M.I., Khrulkov A.V., Mukhametov R.R., Kogan D.I., Popov Yu.O. Osobennosti tekhnologii izgotovleniya detaley iz kompozitsionnykh materialov metodom propitki pod davleniyem [Features of the technology for manufacturing parts from composite materials by pressure impregnation] // Tez. dokl. Mezhotrasl. nauch.-tekhn. konf. «Kompozitsionnyye materialy v aviakosmicheskom materialovedenii». M., 2009. S. 22–25.
  25. Tekhnologii [Technologies] // Kompaniya «Sovremennyye polimernyye tekhnologii»: ofits. sayt. Available at: http://www.apotech.ru (accessed: October 18, 2019).
  26. Gurevich Ya.M., Platonov A.A. Plenochnyye svyazuyushchiye dlya RFI-tekhnologii [Film binders for RFI technology] // Rossiyskiy khimicheskiy zhurnal. 2010. T. LIV: Materialy dlya aviakosmicheskoy tekhniki. S. 63–67.
  27. Timoshkov P.N., Platonov A.A., Hrulkov A.V. Propitka plenochnym svyazuyushhim (RFI) kak perspektivnaya bezavtoklavnaya tehnologiya polucheniya izdelij iz PKM [Film resin infusion as an advanced method for out-of-autoclave processing of polymer composites] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №5. St. 09. Available at: http://www.viam-works.ru (accessed: November 05, 2019). DOI: 10.18577/2307-6046-2015-0-5-9-9.
  28. Rudd C.D., Long A.C., Kendall K.N., Mangin C.G.E. Liquid Moulding Technologies. Woodhead Publishing and SAE International, 1997. P. 42–57.
  29. Ispolzovaniye kompozitov v vetroenergetike // Eksperimentalnyj zavod kompozitnykh materialov: ofits. sayt. Available at: http://www.ezkm.ru (accessed: October 18, 2019).
  30. Vlasov S.V., Kandyrin L.B., Kuleznev A.V. i dr. Osnovy tekhnologii pererabotki plastmass [Fundamentals of plastics processing technology]. M.: Khimiya, 2004. 600 s.
  31. Kholodnikov Yu.V. Sposoby izgotovleniya izdeliy iz kompozitov [Methods of manufacturing products from composites] // Mezhdunarodnyy zhurnal prikladnykh i fundamentalnykh issledovaniy. 2016. №6. S. 214–221.
  32. Zuyev A.S., Emashev A.Yu., Shaydurova G.I. Analiz osobennostey izgotovleniya izdeliy iz polimernykh kompozitsionnykh materialov metodom namotki. Formoobrazuyushchiye opravki [Analysis of the features of manufacturing products from polymer composite materials by winding. Forming mandrels] // Vestnik Moskovskogo gosudarstvennogo tekhnicheskogo universiteta im. N.E. Baumana. Ser.: Mashinostroyeniye. 2018. №3. S. 4–11.
  33. Kryzhanovskiy V.K., Kerber M.L., Burlov V.V. Proizvodstvo izdeliy iz polimernykh materialov [Production of products from polymeric materials]. SPb.: Professiya, 2004. 464 s.
  34. Metod ruchnoy vykladki (kontaktnoye formovaniye) [Manual calculation method (contact molding)] // Naucho-proizvodstvennoe predpriyatie «Polet»: ofits. sayt. Available at: http://www.npppolet.ru (accessed: October 18, 2019).
  35. Tekhnologii [Technologyies] // Kompaniya «Empire-boats»: ofits. sayt. Available at: http:// www.empire-boats.ru (accessed: October 18, 2019).