Gorbovets M.A., Slavin A.V. The coded marking of specimens for high-temperature tests // Proceedings of VIAM. 2019. No. 10 (82). Ст. 12. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2019-0-10-125-132.

The coded marking of specimens for high-temperature tests

Gorbovets M.A., Slavin A.V.
Abstract

The analysis of existing ways of bar code is carried out and opportunity and expediency of their use with reference to test pieces is evaluated. As objects samples for the most demanded tests by determination of physicomechanical properties of metal materials are considered. For identification of metal samples for high-temperature tests by the optimum decision drawing complete (expanded) marking on packaging and the reduced marking on sample end face is. For automation of identification of sample it is reasonable to put shaped coding on sample packaging.

Keywords
normative documentation, quality management system (QMS), aviaengine building, constructional materials, tests.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Ospennikova O.G., Lomberg B.S., Sidorov V.V. Prioritetnyye napravleniya razvitiya tekhnologiy proizvodstva zharoprochnykh materialov dlya aviatsionnogo dvigatelestroyeniya [Priority areas for the development of technologies for the production of heat-resistant materials for aircraft engine building] // Problemy chernoy metallurgii i materialovedeniya. 2013. №3. S. 47–54.
  3. Kablov E.N. Materialy novogo pokoleniya – osnova innovatsiy, tekhnologicheskogo liderstva i natsionalnoy bezopasnosti Rossii [Materials of a new generation – the basis of innovation, technological leadership and national security of Russia] // Intellekt i tekhnologii. 2016. №2 (14). S. 16–21.
  4. Kablov E.N. Materialy i tekhnologii VIAM dlya «Aviadvigatelya» [VIAM materials and technologies for Aviadvigatel] // Permskiye aviatsionnyye dvigateli. 2014. №31. S. 43–47.
  5. GOST ISO/MEK 17025–2009. Obshchiye trebovaniya k kompetentnosti ispytatelnykh i kalibrovochnykh laboratoriy [ISO/IEC 17025:2005. General requirements for the competence of testing and calibration laboratories]. M.: Standartinform, 2018. 31 s.
  6. Gorbovets M.A., Belyayev M.S., Ryzhkov P.V. Soprotivleniye ustalosti zharoprochnykh nikelevykh splavov, poluchennykh metodom SLS [Fatigue strength of heat-resistant nickel alloys produced by selec-tive laser melting] // Aviacionnye materialy i tehnologii. 2018. №3. S. 50–55. DOI: 10.18577/2071-9140-2018-0-3-50-55.
  7. Gorbovets M.A., Kochetkov D.A., Khodinev I.A. Analiz i sravnenie rossijskogo i zarubezhnogo standartov, ustanavlivayushchikh metody ispytanij na termomekhanicheskuyu ustalost [The analysis and comparison of the RF and foreign standards for method of thermomechanical fatigue tests] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №4. St. 11. Available at: http://www.viam-works.ru (accessed: April 03, 2019). DOI: 10.18577/2307-6046-2017-0-4-11-11.
  8. Solovyev A.E., Golynets S.A., Khvatsky K.K., Aslanyan I.R. Provedenie staticheskih ispytanij pri rastyazhenii na mashinah firmy Zwick/Roell [Performing of static tensile tests on Zwick/Roell machines] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №8. St. 12. Available at: http://viam-works.ru (accessed: April 03, 2019). DOI: 10.18577/2307-6046-2015-0-8-12-12.
  9. Letnikov M.N., Lomberg B.S., Ospennikova O.G., Bakradze M.M. Vliyaniye skorosti okhlazhdeniya pri zakalke na mikrostrukturu i svoystva zharoprochnogo deformiruyemogo nikelevogo splava VZH175-ID [influence of quench rate on microstructure and mechanical properties of nickel-based wrought superalloy VZh175-ID] // Aviacionnye materialy i tehnologii. 2019. №2 (55). S. 21–30. DOI: 10.18577/2071-9140-2019-0-2-21-30.
  10. Dzunovich D.A., Lukina E.A., Yakovlev A.L. Vliyaniye rezhimov termicheskoy obrabotki na tekhnologichnost i mekhanicheskiye svoystva listov iz vysokoprochnogo titanovogo splava VT23 [Influence of heat treatment parameters on producibility and mechani-cal properties of sheets made from high-strength titanium alloy VT23] // Aviacionnye materialy i tehnologii. 2018. №3. S. 3–10. DOI: 10.18577/2071-9140-2018-0-3-3-10.
  11. Solonina O.P., Glazunov S.G. Zharoprochnyye titanovyye splavy [Heat resistant titanium alloys]. M.: Metallurgiya, 1976. 448 s.
  12. Bazyleva O.A., Bondarenko Yu.A., Timofeyeva O.B., Khvatskiy K.K. Vliyaniye kristallograficheskoy oriyentatsii na strukturu i svoystva splava VKNA-1V [The influence of crystallographic orientation on the structure and properties of VKNA-1V alloy] // Metallurgiya mashinostroyeniya. 2012. №4. S. 3–7.
  13. Povarova K.B., Bazyleva O.A., Kazanskaya N.K., Drozdov A.A. i dr. Konstruktsionnyye zharoprochnyye splavy na osnove Ni3Al: polucheniye, struktura i svoystva [Structural heat-resistant alloys based on Ni3Al: production, structure, and properties] // Materialovedeniye. 2011. №4. S. 39–48.
  14. Nagesha A., Goyal Sunil, Nandagopal M. yet al. Dynamic strain ageing in Inconel Alloy 783 under tension and low cycle fatigue // Materials Science and Engineering: A. 2012. Vol. 546. P. 34–39.
  15. Dong C., Yu H., Li Y. et al. Life modeling of anisotropic fatigue behaviour for a single crystal nickel-base superalloy // International Journal of Fatigue. 2014. Vol. 61. P. 21–27. DOI: 10.1016/j.ijfatigue.2013.11.026.