Antipov V.V., Konovalov A.N., Serebrennikova N.Yu., Somov A.V., Nefedova Yu.N. Influence of structure on fire resistance and fireproof FMLs SIAL-type and possibility of application of data of materials in aircraft industry // Proceedings of VIAM. 2019. No. 1 (73). Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2019-0-1-40-46.

Influence of structure on fire resistance and fireproof FMLs SIAL-type and possibility of application of data of materials in aircraft industry

Antipov V.V., Konovalov A.N., Serebrennikova N.Yu., Somov A.V., Nefedova Yu.N.
Abstract

A method of fire resistance testing subject to foreign and national regulations of materials made for fire dangerous areas in aircraft engineering was developed. Different compositions of aluminum fiber-glass materials based on 1441 Al–Li alloy sheets were tested to determine a fire-resistance value. Recommendations of forming an aluminum fiber-glass material to enhance a fire resistance level are stated. Technological process of manufacturing of aviation details with requirements of fire resistance is described through the example aircraft engine cowling prototype manufacture.

Keywords
Al–Li alloy, fire resistance, fireproof, burn-through, hybrid material, forming an aluminum fiber-glass material.
Reference list
  1. Fridlyander I.N. Vospominaniya o sozdanii aviakosmicheskoy i atomnoy tekhniki iz alyuminiyevykh splavov [Memories of the creation of aerospace and nuclear technology from aluminum alloys]. M.: Nauka, 2005. 275 s.
  2. Kablov E.N. Materialy novogo pokoleniya – osnova innovatsiy, tekhnologicheskogo liderstva i natsionalnoy bezopasnosti Rossii [Materials of the new generation - the basis of innovation, technological leadership and national security of Russia] // Intellekt & Tekhnologii. 2016. №2. S. 41–46.
  3. Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Yevrazii. 2015. №1. S. 36–39.
  4. Kablov E.N. O nastoyashchem i budushchem VIAM i otechestvennogo materialovedeniya: interv'yu [About the present and the future of the Institute of Scientific and Technical Information and Russian Materials Science: an interview] // Rossiyskaya akademiya nauk. 2015. 19 yanvarya. S. 10–15.
  5. Raskutin A.E. Strategiia razvitiia polimernykh kompozitsionnykh materialov [Development strategy of polymer composite materials] // Aviatsionnye materialy i tekhnologii. 2017. №S. S. 344–348. DOI: 10.18577/2071-9140-2017-0-S-344-348.
  6. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  7. Roebroeks G.H.J.J. GLARE: a structural material for fire resistant fuselages // AGARD Conference Proceedings. October, 1996. R. 26–1; 26–13.
  8. Characterisation of Fibre Metal Laminates under Thermo-mechanical Loadings / ed. M. Hagenbeek. Netherlands, 2005. R. 17–22.
  9. Fridlyander I.N., Senatorova O.G., Anikhovskaya L.I. Struktura i svoystva konstruktsionnykh alyumostekloplastikov marki SIAL [Structure and properties of structural aluminum-glass plastics of the SIAL brand] // Sloistyye kompozitsionnyye materialy – 98: sb. tr. Mezhdunar. konf. Volgograd, 1998. S. 131–133.
  10. Shavnev A.A., Kurbatkina E.I., Kosolapov D.V. Metody sozdaniya alyuminiyevykh kompozitsionnykh materialov [Methods for joining of aluminum composite materials (review)] // Aviacionnye materialy i tehnologii. 2017. №3 (38). S. 35–42. DOI: 10.18577/2071-9140-2017-0-3-35-42.
  11. Fridlyander I.N., Anikhovskaya L.I., Senatorova O.G. Kleyenyye metallicheskiye i sloistyye kompozity. Tsvetnyye metally i splavy. Kompozitsionnyye metallicheskiye materialy [Glued metal and laminated composites. Non-ferrous metals and alloys. Composite metallic materials]. M.: Mashinostrienie, 2001. T.: II–3. S. 814–832.
  12. Podzhivotov N.YU., Kablov E.N., Antipov V.V., Yerasov V.S. Sloistyye metallopolimernyye materialy v elementakh konstruktsii vozdushnykh sudov [Laminated metal-polymer materials in the structural elements of aircraft] // Perspektivnyye materialy. 2016. №10. S. 5–19.
  13. Shestov V.V., Antipov V.V., Senatorova O.G., Sidelnikov V.V. Konstruktsionnyye sloistyye alyumostekloplastiki 1441-SIAL [Structural layered alumino-glass plastics 1441-SIAL] // Metallovedeniye i termicheskaya obrabotka metallov. 2013. №9. S. 28–32.
  14. Leshchiner L.N., Latushkina L.V., Fedorenko T.P. Splav 1441 sistemy Al–Cu–Mg–Li [Alloy 1441 of the Al – Cu – Mg – Li system] // Tez. dokl. Vsesoyuz. nauch. konf. Metallovedeniye splavov alyuminiya s litiyem. M.: VILS, 1991. S. 76–77.
  15. Antipov V.V., Senatorova O.G., Lukina N.F. i dr. Sloistye metallopolimernye kompozicionnye materialy [Layered metalpolymeric composite materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 226–230.
  16. Antipov V.V., Senatorova O.G., Sidelnikov V.V. Issledovanie pozharostojkosti sloistyh gibridnyh alyumostekloplastikov klassa SIAL [Research of fire firmness layered hybrid aluminum fibreglasses of SIAL’s class] // Aviacionnye materialy i tehnologii. 2011. №3. S. 36–41.
  17. Barbotko S.L., Kirillov V.N., Shurkova E.N. Ocenka pozharnoj bezopasnosti polimernyh kompozicionnyh materialov aviacionnogo naznacheniya [Fire safety evolution for polymer composites of aeronautical application] // Aviacionnye materialy i tehnologii. 2012. №3. S. 56–63.
  18. Kutsevich K.E., Tyumeneva T.Yu., Petrova A.P. Vliyaniye napolniteley na svoystva kleyevykh prepregov i PKM na ikh osnove [Influence of fillers on properties of adhesive prepregs and PCM on their basis] // Aviacionnye materialy i tehnologii. 2017. №4 (49). S. 51–55. DOI: 10.18577/2071-9140-2017-0-4-51-55.
  19. Barbotko S.L. Razvitie metodov ocenki pozharobezopasnosti materialov aviacionnogo naznacheniya [Development of the fire safety test methods for aviation materials] // Aviacionnye materialy i tehnologii. 2017. №S. S. 516–526. DOI: 10.18577/2071-9140-2017-0-S-516-526.