Grigorenko V.B., Morozova L.V. The usage of fractographic analysis to diagnostic the causes of destruction of products from medium-carbon steel // Proceedings of VIAM. 2018. No. 8 (68). Ст. 10. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2018-0-8-98-111.

The usage of fractographic analysis to diagnostic the causes of destruction of products from medium-carbon steel

Grigorenko V.B., Morozova L.V.
Abstract

The reasons of destruction of products from medium-carbon steels (steel 60, steel 55 and steel 51HFA) are investigated and established. It was established that the main material of the products (cables and springs) met the requirements of the normative documentation on the composition, structure and content of non-metallic inclusions. The destructions were caused by the action of stresses exceeding the permissible (in the first and third cases). Differences in the structure of the breaks, obtained from the action of complex static load and cyclic loads, both at low tension levels and at elevated ones are shown.

Keywords
constructional steel, fractography, scanning electronic microscopy, fatigue failure, intercrystalline brittleness.
Reference list
  1. Kablov E.N. Materialy – osnova lyubogo dela [Materials are the base of any business] // Delovaya slava Rossii. 2013. №2 (40). S. 4–9.
  2. Kablov E.N. Materialy novogo pokoleniya – osnova innovatsij, tekhnologicheskogo liderstva i natsionalnoj bezopasnosti Rossii [Materials of new generation are the base of innovations, technological leadership and national security of Russia ] // Intellekt i tekhnologii. 2016. №2 (14). S. 16–21.
  3. Kablov E.N. Iz chego sdelat budushchee? Materialy novogo pokoleniya, tekhnologii ikh sozdaniya i pererabotki – osnova innovatsij [Of what to make the future? Materials of new generation, technology of their creation and processing are the base of innovations] // Krylya Rodiny. 2016. №5. S. 8–18.
  4. Stali i splavy. Marochnik / pod red. V.G. Sorokina, M.A. Gervaseva [There were also alloys. Grade guide / ed. by V.G. Sorokin, M.A. Gervasev]. M.: Intermet Inzhiniring, 2001. 608 s.
  5. GOST 7372–79. Provoloka stalnaya kanatnaya. Tekhnicheskie usloviya [State Standard 7372–79. Wire the steel rope. Specifications]. M.: Izd-vo standartov, 2003. 17 s.
  6. GOST 1050–2013. Metalloproduktsiya iz nelegirovannykh konstruktsionnykh kachestvennykh i spetsialnykh stalej. Obshchie tekhnicheskie usloviya [State Standard 1050–2013. Steel products from undoped constructional qualitative and special the staly. General specifications]. M.: Standartinform, 2014. 32 s.
  7. GOST 14959–2016. Metalloproduktsiya iz ressorno-pruzhinnoj nelegirovannoj i legirovannoj stali. Tekhnicheskie usloviya [State Standard 14959–2016. Steel products from spring and spring undoped and alloy steel. Specifications]. M.: Standartinform, 2017, 28 s.
  8. Vinogradov S.S., Nikiforov A.A., Demin S.A., Chesnokov D.V. Zashchita ot korrozii uglerodistykh stalej [Protection against corrosion of carbon steel] // Aviacionnye materialy i tehnologii. 2017. №S. S. 242–263. DOI: 10.18577/2071-9140-2017-0-S-242-263.
  9. GOST 2172–80. Kanaty stalnye aviatsionnye. Tekhnicheskie usloviya [State Standard 2172–80. Ropes the steel aviation. Specifications]. M.: Izd-vo standartov, 2003. 8 s.
  10. Badikov K.A., Savkin A.N., Andronik A.V. Ocenka treshhinostojkosti nizkolegirovannoj stali pri neregulyarnom ciklicheskom nagruzhenii [The evaluation of fracture toughness of low-alloy steels by irregular cyclic loading] // Aviacionnye materialy i tehnologii. 2015. №S1 (38). S. 20–26. DOI: 10.18577/2071-9140-2015-0-S1-20-26.
  11. Gromov V.I., Voznesenskaya N.M., Pokrovskaya N.G., Tonysheva O.A. Vysokoprochnye konstrukcionnye i korrozionnostojkie stali FGUP «VIAM» dlya izdelij aviacionnoj tehniki [High-strength constructional and corrosion-resistant steels developed by VIAM for aviation engineering] // Aviacionnye materialy i tehnologii. 2017. №S. S. 159–174. DOI: 10.18577/2071-9140-2017-0-S-159-174.
  12. Kudrya A.V., Sokolovskaya E.A., Nin Khaj Le, Kha Ngok Ngo. Svyaz morfologii vyazkikh izlomov razlichnoj prirody i svojstv konstruktsionnykh stalej [Communication of morphology of ductile fractures of the different nature and properties constructional steels] // Metallovedenie i termicheskaya obrabotka metallov. 2018. №4. S. 36–41.
  13. Kudrya A.V., Sokolovskaya E.A, Trachenko V.A. i dr. Izmerenie neodnorodnosti razrusheniya v konstruktsionnykh stalyakh s raznorodnoj strukturoj [Measurement of heterogenity of destruction in constructional stalyakh with diverse structure] // Metallovedenie i termicheskaya obrabotka metallov. 2015. №4. S. 12–18.
  14. Kudrya A.V., Sokolovskaya E.A., Nin Khaj Le i dr. Otsenka stroeniya izlomov i struktur v konstruktsionnykh stalyakh s ispolzovaniem kompyuterizirovannykh protsedur [Assessment of structure of breaks and structures in constructional stalyakh with use of the computerized procedures] // Vektor nauki TGU. 2015. №4. S. 44–52.
  15. Grigorenko V.B., Morozova L.V. Primenenie rastrovoj elektronnoj mikroskopii dlya izucheniya nachal'nykh stadij razrusheniya [Application of the scanning electron microscopy for studying of initial destruction stages] // Aviacionnye materialy i tehnologii. 2018. №1 (50). S. 77–87. DOI: 10.18577/2071-9140-2018-0-1-77-87.