Pentuykhin S.I., Trapeznikov A.V., Vlasova K.A., Klyukvina T.D. Determination of optimal manufacturing technology of casting alloy AK7ch. with using of ceramic molds // Proceedings of VIAM. 2018. No. 7 (67). Ст. 03. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2018-0-7-25-32.

Determination of optimal manufacturing technology of casting alloy AK7ch. with using of ceramic molds

Pentuykhin S.I., Trapeznikov A.V., Vlasova K.A., Klyukvina T.D.
Abstract

This work is devoted to the determination of the optimal technology for manufacturing castings from the АК7ч. alloy (Al–Si systems) by the method of investment casting. Data on the capabilities of the investment casting method are given. The data on the basic requirements for the ceramic shell, as well as the method of its production and application, are presented. An experiment was conducted to determine the required number of layers of ceramic coating for aluminum castings of various configurations. On the basis of the analysis of the results of the work, the optimal number of applied layers was chosen for the production of model blocks and the method of shell molding.

Keywords
eramic molds, investment casting, strength, shell, binder, suspension, aluminum alloys.
Reference list
  1. Vlasova K.A., Klyukvina T.D., Leonov A.A., Larionov S.A. Vzaimodejstvie modelnykh sostavov s plastikovoj osnastkoj, izgotovlennoj s pomoshchyu tekhnologii 3D-pechati [Interaction of model compositions with plastic equipment made using 3D printing technology] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2018. №2. St. 07. URL: http://www.viam-works.ru (accessed: June 25, 2018). DOI: 10.18577/2307-6046-2018-0-2-7-7.
  2. Shklennik YA.I., Ozerov V.A. Lite po vyplavlyaemym modelyam. Inzhenernaya monografiya [Investment casting. Engineering monograph]. M.: Mashinostroenie, 1984. 408 s.
  3. Spetsialnye sposoby litya: spravochnik / pod obshch. red. V.A. Efimova [Special ways of molding: directory / gen. ed. by V.A. Efimov]. M.: Mashinostroenie, 1991. 436 s.
  4. Klyukvina T.D., Vlasova K.A., Leonov A.A., Yashina S.A. Izuchenie mekhanizma obrazovaniya prochnosti v samotverdeyushchikh smesyakh s fenolnym svyazuyushchim (obzor) [Study of the mechanism of formation of strength in self-hardening mixtures with a phenolic binder (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2018. №3. St. 03. Available at: http://viam-works.ru (accessed: June 25, 2018). DOI: 10.18577/2307-6046-2018-0-3-3.
  5. Garshin A.P., Gropyanov V.M., Zajtsev G.P. Keramika dlya mashinostroeniya [Ceramics for mechanical engineering]. M.: Nauchtekhlitizdat, 2003. 384 s.
  6. Trukhov A.P., Sorokin A.Yu., Ershov M.Yu. i dr. Tekhnologiya litejnogo proizvodstva: lite v peschanye formy: ucheb. [Technology of foundry production: sand casting: textbook]. M.: Akademiya, 2005. 528 s.
  7. Ozerov V.A., Garanin V.F. Lite povyshennoj tochnosti po razovym modelyam: ucheb. posobie [Enhanced accuracy molding on one-time models: manual]. M.: Vysshaya shkola, 1988. 87 s.
  8. Ivanov V.N., Kazennov S.A., Kurchman B.S. i dr. Lite po vyplavlyaemym modelyam. 3-e izd., pererab. i dop. [Investment casting. 3rd ed., rev. and add.]. M.: Mashinostroenie, 1984. 408 s.
  9. Ospennikova O.G. Issledovanie i razrabotka parametrov tehnologicheskogo processa izgotovleniya modelej iz modelnyh kompozicij na osnove sinteticheskih voskov [Research and working out of parametres of technological process of manufacturing of models from modelling compositions on the basis of synthetic waxes] // Aviacionnye materialy i tehnologii. 2014. №3. S. 18–21. DOI: 10.18577/2071-9140-2014-0-3-18-21.
  10. Ivanov V.N. Slovar-spravochnik po litejnomu proizvodstvu [The dictionary reference on foundry production]. M.: Mashinostroenie, 1990. 384 s.
  11. Lakedemonskij A.V., Kvasha F.S., Mendeleev Ya.I. i dr. Litejnye defekty i sposoby ikh ustraneniya [Foundry defects and ways of their elimination]. M.: Mashinostroenie, 1972. 152 s.
  12. Mikheev S.V., Stroganov G.B., Romashin A.G. Keramicheskie i kompozitsionnye materialy v aviatsionnoj tekhnike [Ceramic and composite materials in aviation engineering]. M.: Alteks, 2002. 276 s.
  13. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  14. Kablov E.N. Sovremennye materialy – osnova innovatsionnoj modernizatsii Rossii [Modern materials – basis of innovative modernization of Russia] // Metally Evrazii. 2012. №3. S. 10–15.
  15. Duyunova V.A., Volkova E.F., Uridiya Z.P., Trapeznikov A.V. Dinamika razvitiya magnievyh i litejnyh alyuminievyh splavov [Dynamics of the development of magnesium and cast aluminum alloys] // Aviacionnye materialy i tehnologii. 2017. №S. S. 225–241. DOI: 10.18577/2071-9140-2017-0-S-225-241.
  16. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Entsiklopedicheskij spravochnik. 2008. №3. S. 2–14.
  17. Alyuminievye splavy v aviakosmicheskoj tekhnike / pod obshch. red. E.N. Kablova [Aluminum alloys in aerospace equipment / gen. ed. by E.N. Kablov]. M.: Nauka, 2001. 192 s.