Grigorenko V.B., Morozova L.V., Vinogradov S.S. Features of destruction of details of fixture from the constructional steel // Proceedings of VIAM. 2018. No. 4 (64). Ст. 08. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2018-0-4-66-74.

Features of destruction of details of fixture from the constructional steel

Grigorenko V.B., Morozova L.V., Vinogradov S.S.
Abstract

Features of destruction of samples from steel 30ХГСА with galvanotermic coatings on the basis of zinc are analyzed. At formation of a break of the samples tested for grain-boundary brittle destruction, three areas differing on a structure are created. In a near surface zone under a sheeting the area of the maleficiated relief with destruction on the mechanism of a viscous cut is formed. Further the area with a rough relief in which it is possible to allocate a zone of the slowed-down destruction with brittle facets and a zone viscous dimple rupture is created. It is established that when testing for low-cycle fatigue samples from steel 30ХГСА with galvanotermic coatings the centers of destruction are risks or other defects on a steel surface under a covering. In an focal zone the fan-shaped relief is most often observed. In process of removal from the center of destruction fatigue plateaus and grooves are created. In break viscous poles are formed. Research of the destroyed axis made

Keywords
constructional steel, fractography, scanning electronic microscopy, fatigue failure and intercrystalline brittleness.
Reference list
  1. Nesterova E.V., Zolotorevskij N.Yu., Titovec Yu.F., Hlusova E.I. Nasledovanie razorientacij i model formirovaniya struktury bejnita v nizkouglerodistyh stalyah pod vliyaniem deformacii austenite [Inheritance of disordering and model of forming of structure of bainite in low-carbon steels under the influence of austenite deformation] // Voprosy materialovedeniya. 2011. №4 (68). S. 17–26.
  2. Kobayashi J., Ina D., Yoshikawa N., Sugimoto K. Effects of the addition of Cr, Mo and Ni on the microstructure and retained austenite characteristics of 0,2% C–Si–Mn–Nb ultra-highstrength TRIP-aided bainitic ferrite steels // ISIJ International. 2012. Vol. 52. No. 10. P. 1894–1901.
  3. Samojlovich Yu.A. Povyshenie prochnosti zheleznodorozhnyh relsov putem izotermicheskoj zakalki na nizhnij bejnit [Increase of durability of railway rails by isothermal hardening on the lower bainite] // Metallurg. 2012. №10. S. 70–76.
  4. Stali i splavy. Marochnik / pod red. V.G. Sorokina, M.A. Gervaseva i dr. [Steels and alloys. Grade guide / ed. by V.G. Sorokin, M.A. Gervasev et al.]. M.: Intermet Inzhiniring, 2001. 608 s.
  5. Karimova S.A., Chesnokov D.V. Metallicheskie i nemetallicheskie neorganicheskie pokrytiya dlya zashhity izdelij, ekspluatiruyushhihsya vo vseklimaticheskih usloviyah [Metallic and nonmetallic inorganic coatings for protection of the products which are maintaining in all climatic conditions] // Vse materialy. Enciklopedicheskij spravochnik. 2014. №11. S. 36–41.
  6. Kablov E.N. Materialy novogo pokoleniya – osnova innovacij, tehnologicheskogo liderstva i nacionalnoj bezopasnosti Rossii [Materials of new generation – basis of innovations, technological leadership and national security of Russia] // Intellekt i tehnologii. 2016. №2 (14). S. 16–21.
  7. Kablov E.N. Materialy i tehnologii VIAM dlya «Aviadvigatelya» // Permskie aviacionnye dvigateli: inform. byul. 2014. №S. S. 43–47.
  8. Kablov E.N., Nikiforov A.A., Demin S.A., Chesnokov D.V., Vinogradov S.S. Perspektivnye pokrytiya dlya zashhity ot korrozii uglerodistyh stalej [Perspective coverings for corrosion protection of carbon steels] // Stal. 2016. №6. S. 70–81.
  9. Nikiforov A.A., Zakirova L.I., Vinogradov S.S. Termoimmersionnoe pokrytie cink + olovo kontaktnoe [Thermoimmersion covering zinc + tin contact ] // Korroziya: materialy, zashhita. 2016. №8. S. 34–41.
  10. Taranceva K.R., Nikolotov A.D. Elektroosazhdenie splava olovo-cink iz stabilizirovannogo pirofosfatnogo elektrolita kak alternativa kadmievomu pokrytiyu [Alloy electrosedimentation tin-zinc from the stabilized pirofosfatny electrolit as alternative to cadmic covering] // Korroziya: materialy, zashhita. 2014. №3. S. 27–30.
  11. Grinevich A.V., Erasov V.S., Yakusheva N.A., Terehin A.L. Ustalostnaya dolgovechnost stali VKS-9 v usloviyah simmetrichnogo nagruzheniya «rastyazhenie–szhatie» i «izgib s vrashheniem» [Fatigue life of steel VKS-9 in conditions of symmetric loading «tension–compression» and «bending with rotation»] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №9. St. 11. Available at: http://www.viam-works.ru (accessed: February 05, 2018.). DOI: 10.18577/2307-6046-2017-0-9-11-11.
  12. Gromov V.I., Krotov V.N., Kurpyakova N.A., Sedov O.V., Doroshenko A.V. Vliyanie ostatochnogo austenita na strukturu i svojstva diffuzionnogo sloya stali martensitnogo klassa posle vakuumnoj cementacii [Influence of residual austenite on the structure and properties of diffusion layer of martensitic grade steel after vacuum carburization] // Aviacionnye materialy i tehnologii 2016. №4 (45) S. 3–8. DOI: 10.18577/2071-9140-2016-0-4-3-8.
  13. Gordeeva T.A., Zhegina I.P. Analiz izlomov pri ocenke nadezhnosti materialov [The analysis of breaks at assessment of reliability of materials]. M.: Mashinostroenie, 1978. 200 s.
  14. Fonshtejn N.M., Bronfin B.M., Shirman A.Z. et al. Kolichestvennoe mikrofrak-tograficheskoe issledovaniya vyazkogo razrusheniya v nizkolegirovannyh stalyah [Quantitative microfractographic researches of viscous destruction in low-alloy steels] // Fizika metallov i metallovedenie. 1982. T. 53. №1. S. 174–179.
  15. Badikov K.A., Savkin A.N., Andronik A.V. Ocenka treshhinostojkosti nizkolegirovannoj stali pri neregulyarnom ciklicheskom nagruzhenii [The evaluation of fracture toughness of low-alloy steels by irregular cyclic loading] // Aviacionnye materialy i tehnologii. 2015. №S1 (38). S. 20–26. DOI: 10.18577/2071-9140-2015-0-S1-20-26.
  16. Erasov V.S., Nuzhnyj G.A., Grinevich A.V. Ob ocenke povrezhdaemosti metallicheskih materialov metodami mehanicheskih ispytanij [About assessment of damageability of metal materials methods of mechanical tests] // Deformaciya i razrushenie materialov. 2015. №3. S. 42–47.
  17. Kudrya A.V., Sokolovskaya E.A., Le Haj Nin, Trachenko V.A., Skorodumov S.V. i dr. Ocenka stroeniya izlomov i struktur v konstrukcionnyh stalyah s ispol'zovaniem kompyuterizirovannyh procedur [Assessment of structure of breaks and structures in constructional stalyakh with use of the computerized procedures] // Vektor nauki TGU. 2015. №4. S. 44–52.
  18. Matvienko Yu.G. Modeli i kriterii mehaniki razrusheniya [Models and criteria of fracture mechanics]. M.: Fizmatlit, 2006. 328 s.
  19. Grinevich A.V., Nuzhnyj G.A., Bakanov A.V., Ulkin M.Yu., Odincev I.N. Ocenka nesushhej sposobnosti elementov krepezha iz polimernyh kompozicionnyh materialov [As-sessment of bearing capacity of elements of fixture from polymeric composite materials ] // Deformaciya i razrushenie materialov. 2015. №12. S. 38–42.
  20. Orlov M.R., Ospennikova O.G., Gromov V.I. Zamedlennoe razrushenie stali 38HN3MA v processe dlitelnoj ekspluatacii [Steel 38ХН3МА delayed fracture in the course of long opera-tion] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroenie. 2011. Specialnyj vypusk: Perspektivnye konstrukcionnye materialy i tehnologii. S. 5–10.
  21. Bytsenko O.A., Grigorenko V.B., Lukina E.A., Morozova L.V. Razvitie metodov metallofizicheskih issledovanij: metodologicheskie voprosy i prakticheskaya znachimost [Development of methods for metal-physical research: methodological issues and practical significance] // Aviacionnye materialy i tehnologii. 2017. №S. S. 498–515. DOI: 10.18577/2071-9140-2017-0-S-498-515.