Efimochkin I.Yu., Schetanov B. V., Paegle S.V., Dvoretskov R.M. Research of peculiarities of mechanical decomposition in synthesis of in-situ composites based on refractory metals // Proceedings of VIAM. 2018. No. 4 (64). Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2018-0-4-38-50.

Research of peculiarities of mechanical decomposition in synthesis of in-situ composites based on refractory metals

Efimochkin I.Yu., Schetanov B. V., Paegle S.V., Dvoretskov R.M.
Abstract

The article describes the method of mechanical alloying as an alternative for obtaining high-temperature materials based on niobium, the obtaining of which by traditional methods (casting technologies) entails great difficulties. Particular attention was paid to the control of intermediate operations related to the process of mechanical alloying. The evolution of the microstructure, phase and granulometric compositions of composite powders (CP) of the Nb–Si–Ti system at various stages of mechanical doping is considered. It is established that the process of mechanical doping consists of two processes: the actual alloying process, which is controlled by the time of powder formation with the X-ray amorphous structure and the process of creating a fractional composition controlled by a histogram of powder distribution in size. The choice of the most effective method of quality control of alloying KP was made. This method is XRF, the criterion of which is the amorphization of the structu

Keywords
high-temperature composite materials, mechanical alloying, powder metallurgy, heat resisting alloys.
Reference list
  1. Kablov E.N., Svetlov I.L., Efimochkin I.Yu. Vysokotemperaturnye Nb–Si-kompozity [High-temperature Nb-Si-composites] // Vestnik Moskovskogo gosudarstvennogo tehnicheskogo universiteta im. N.E. Baumana. Ser.: Mashinostroenie. 2011. №SP2. S. 164–173.
  2. Bewlay B.P., Jackson M.R., Zhao J.-C. et al. Ultrahigh-Teperature Nb-Silicide-Based Composites // MRS Bulletin. 2003. Vol. 28. No. 9. P. 646–653.
  3. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strate-gicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  4. Timofeyeva O.B., Kolodochkina V.G., Shvanova N.F., Neiman A.V. Issledovanie mikrostruktury vysokotemperaturnogo estestvenno kompozicionnogo materiala na osnove niobija, uprochnennogo intermetallidami silicida niobiya [The microstructure analysis of niobium-based high-temperature natural composite material reinforced with niobium silicide intermetallics] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 60–64. DOI: 10.18577/2071-9140-2015-0-1-60-64.
  5. Menon E.S.K., Mendiratta M.G., Dimiduk D.M. Oxidation of complex niobium based alloys // International Symposium Niobium; Science & Technology (Orlando, Florida). December2–5, 2001. P. 121–146.
  6. Muboyadzhyan S.A., Budinovskij S.A., Gayamov A.M., Matveev P.V. Vysokotemperaturnye zharostojkie pokrytiya i zharostojkie sloi dlya teplozashhitnyh pokrytij [High-temperature heat resisting coverings and heat resisting layers for heat-protective coverings] // Aviacionnye materialy i tehnologii. 2013. №1. S. 17–20.
  7. Benjamin J.S. Dispersion Strengthened Superalloys by Mechanical Alloing // Metallurgical Transactions. 1970. Vol. 10. P. 2943–2951.
  8. Jackson M.R., Bewley B.P., Rowe R.G., Skelly D.W., Lipsitt H.A. High Temperature Refractory Metall-Intermetallic Composites // The Journal of The Minerals, Metals & Materials Society. 1996. Vol. 48. No. 1. P. 39–44.
  9. Kablov E.N., Ospennikova O.G., Petrushin N.V., Visik E.M. Monokristallicheskij zharoprochnyj nikelevyj splav novogo pokoleniya s nizkoj plotnostyu [Single-crystal nickel-based superalloy of a new generation with low-density] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 14–25. DOI: 10.18577/2071-9140-2015-0-2-14-25.
  10. Babich B.N., Kolupaeva S.Ya., Kustov Yu.A., Chernyak A.I., Shhetanov B.V. O poluchenii dispersno-uprochnennogo nikel-hromovogo splava metodom mehanicheskogo legirovaniya [About receiving disperse strengthened nickel-chrome alloy method of mechanical alloying] // Poroshkovaya metallurgiya. 1977. №2 (170). S. 53–57.
  11. Babich B.N. Dispersnoe uprochnenie i mehanicheskoe legirovanie – novye puti sozdaniya vysokotemperaturnyh aviacionnyh materialov [Disperse hardening and mechanical alloying – new ways of creation of high-temperature aviation materials] // Aviacionnye materialy na rubezhe XX–XXI vekov: sb. nauch. tr. M.: VIAM, 1994. S. 304–313.
  12. Shhetanov B.V., Efimochkin I.Yu., Murasheva V.V., Shheglova T.M. Issledovanie NbSi-kompozitov, armirovannyh monokristallicheskimi voloknami α-Al2O3, s barernym pokrytiem i bez nego [Research of the NbSi-composites reinforced by single-crystal fibers α-Al2O3, with barrier coating and without it] // Materialovedenie. 2015. №9. S. 48–53.
  13. Zhao J.-C., Jackson M.R., Peluso L.A. Mapping of the Nb–Ti–Si phase diagram using diffusion multiples // Material Science & Engineering: A. 2004. Vol. 372. P. 21–27.
  14. Wang D., Yang S., Yang M. et al. Experimental investigation of phase equilibria in the Fe–Nb–Si ternary system // Journal of Alloys and Compounds. 2014. P. 183–192.
  15. Honghui X., Yong D., Zhaohui Y. et al. Phase equilibria of the Fe–Nb–Ti system at 900°C // Journal of Alloys and Compounds. 2005. P. 151–155.