Azarovskiy E.N., Muboyadzhyan S.A. Investigation of the process of modification of steels EP866 and EI961 in titanium plasma VDR with tests on resistance to salt corrosion // Proceedings of VIAM. 2018. No. 2 (62). Ст. 11. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2018-0-2-11-11.

Investigation of the process of modification of steels EP866 and EI961 in titanium plasma VDR with tests on resistance to salt corrosion

Azarovskiy E.N., Muboyadzhyan S.A.
Abstract

The process of surface modification in the ion-plasma installation MAP-3 is considered. It is shown that with the chosen parameters of the modification process, the temperature of the samples does not exceed the tempering temperature of the compressor steels EP866 and EI961. Metallographic and microspectral studies of the surface layer of the samples after modification have been carried out. Modified samples were tested for resistance to salt corrosion by the VIAM method at a temperature of 600°C.

Keywords
steel compressor, vacuum arc, titanium plasma, ion modification, thermally ion diffusion, ion etching, microstructure, electron microscopy.
Reference list
  1. Kablov E.N. Razrabotki VIAM dlya gazoturbinnyh dvigatelej i ustanovok [Development of VIAM for gas turbine engines and installations] // Krylya Rodiny. 2010. №4. S. 31–33.
  2. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] // Metally Evrazii. 2012. №3. S. 10–15.
  3. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
  4. Salahova R.K. Korrozionnaja stojkost stali 30HGSA s «trehvalentnym» hromovym pokrytiem v estestvennyh i iskusstvennyh sredah [Corrosion resistance of steel 30ХГСА with «trivalent» chrome plating in natural and artificial environments] //Aviacionnye materialy i tehnologii. 2012. №2. S. 59–66.
  5. Anfinogenov A.I. Analiz razvitiya himiko-termicheskoj obrabotki metallov i splavov [Analysis of development of chemical and thermal processing of metals and alloys] // Rasplavy. 2005. №3. S. 40–52.
  6. Kashin D.S., Stehov P.A. Razrabotka kompleksnyh zharostojkih pokrytij dlya detalej iz estestvenno-kompozicionnogo materiala na osnove niobiya [Development of combined heat-resistant coatings for parts made of natural-composite material based on niobium] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №6 (54). St. 4. Available at: http://www.viam-works.ru (accessed: December 11, 2017). DOI: 10.18577/2307-6046-2017-0-6-4-4.
  7. Kablov E.N., Muboyadzhyan S.A. Heat-resistant coatings for the high-pressure turbine blades of promising GTES // Russian metallurgy (Metally). 2012. No. 1. P. 1–7.
  8. Sposob obrabotki poverhnosti metallicheskogo izdeliya: pat. 2368701 Ros. Federaciya [Way of surface treatment of metal product: pat. 2368701 Rus. Federation]; opubl. 27.09.2009.
  9. Sposob naneseniya kombinirovannogo zharostojkogo pokrytiya: pat. 2402633 Ros. Federaciya [Way of drawing the combined heat resisting covering: pat. 2402633 Rus. Federation]; opubl. 27.10.2010.
  10. Aleksandrov D.A., Artemenko N.I. Iznosostojkie pokrytiya dlya zashhity detalej treniya sovremennyh GTD [Wear-resistant coatings to protect friction parts of modern gas turbine engines] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №10. St. 06. Available at: http://www.viam-works.ru (accessed: November 02, 2017). DOI: 10.18577/2307-6046-2016-0-10-6-6.
  11. Artemenko N.I., Simonov V.N. Matematicheskoe modelirovanie processa osazhdeniya titana na ustanovke ionno-plazmennogo napyleniya MAP-3 [Mathematical modeling of the titanium deposition process at the MAP-3 ion-plasma deposition unit] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №6. St. 03. URL: http://www.viam-works.ru (accessed: December 08, 2017). DOI: 10.18577/2307-6046-2017-0-6-3-3.
  12. Muboyadzhyan S.A. Modificirovanie metallicheskoj poverhnosti v plazme vakuumno-dugovogo razryada metodom termostimulirovannoj ionnoj diffuzii [Modifying of metallic surface in vacuum arc discharge plasma method thermo stimulation of ionic diffusion] // Metally. 2008. №6. S. 1–13.
  13. Kablov E.N., Muboyadzhyan S.A. Ionnoe travlenie i modificirovanie poverhnosti otvetstvennyh detalej mashin v vakuumno-dugovoj plazme [Ion etching and modifying of surface of responsible details of machines in vacuum and arc plasma] // Vestnik MGTU im. N.E. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 149–163.
  14. Muboyadzhyan S.A., Azarovskij E.N. Issledovanie novogo processa ionnogo modificirovaniya poverhnosti obrazcov kompressornyh stalej v vakuumno-dugovoj plazme titana [Research of new process of ionic modifying of surface of samples compressor steels in vacuum and arc plasma of titanium] // Metally. 2013. №6. S. 63–73.
  15. Muboyadzhyan S.A., Azarovskij E.N. Modificirovanie poverhnosti obrazcov iz kompressornyh stalej metodom termostimulirovannoj ionnoj diffuzii v titanovoj plazme vakuumno-dugovogo razryada [Modifying of surface of samples from compressor steels method of thermo stimulation ionic diffusion in titanic plasma of the vacuum arc discharge] // Metally. 2015. №6. S. 11–19.
  16. Lygdenov B.D. Intensifikaciya processov himiko-termicheskoj obrabotki pri diffuzionnom titanirovanii [Intensification of processes of chemical and thermal processing at diffusion titanizing]. Barnaul: Izd-vo AltGTU, 2006. 135 s.
  17. Modificirovanie i legirovanie poverhnosti lazernymi, ionnymi i elektronnymi puchkami / pod red. D.M. Pouta i dr. [Modifying and surface alloying laser, ionic and electronic bunches / ed. by D.M. Pout et al.]. M.: Mashinostroenie, 1987. 424 s.
  18. Shulaev V.M., Taran V.S., Timoshenko A.I., Gasilin V.V. Issledovanie effektov modifikacii poverhnosti metallicheskih podlozhek, podvergnutyh ionno-plazmennoj obrabotke [Research of effects of updating of surface of the metal substrates subjected to ion-plasma processing] // Voprosy atomnoj nauki i tehniki. 2011. №6 (76). Ser.: Vakuum, chistye materialy, sverhprovodniki. (19). S. 184–192.
  19. Andreev A.A. Vakuumno-dugovoe modificirovanie poverhnosti stalnyh izdelij [Vacuum and arc modifying of surface of steel products] // FIP. 2007. T. 5. №3–4. S. 140–148.
  20. Kablov E.N. Materialy novogo pokoleniya – osnova innovacij, tehnologicheskogo liderstva i nacionalnoj bezopasnosti Rossii [Materials of new generation – basis of innovations, technological leadership and national security of Russia] // Intellekt i tehnologii. 2016. №2 (14). S. 16–21.